University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
16 results
Search Results
Item type:Publication, Microstructural evolution during mechanical milling of Ti/Al powder mixture and production of intermetallic TiAl cathode target2011, SpringerTitanium aluminides are of great technological interest because of their attractive mechanical properties. Mechanical milling/alloying is a promising powder metallurgical technique, which can achieve ultrafine, uniform and manipulable microstructures. In this study, we employed a recently revisited discus mill to produce a composite Ti– (50–57) at.%Al powder feedstock, which is suitable for hot consolidation to produce bulk cathode targets for physical vapour deposition (PVD) coatings. The effects of milling time, quantity of process control agent (PCA) and discus-topowder weight ratio (DPR) on the microstructure evolution of the attendant Ti/Al composite powder were investigated in detail. It was found that to produce Ti/Al composite powders with a fine particle size and a uniform microstructure, the practicable processing parameters should be 2 or 3% isopropanol addition as PCA, 12 h of milling time and at least 13:1 DPR weight ratio. Cathode targets were produced by hot isostatic pressing (HIPing) the as-milled powders. The targets were then used to produce a PVD TiAlN coating which had an average microhardness of 2400 HV.Item type:Publication, Mechanical behaviour of Titanium, Ti-6Al-4V (wt %) alloy and Ti-47Al-2Cr (at %) alloy produced using powder compact forging2011, Trans Tech PublicationsPowder compact forging was used to produce bulk consolidated titanium and Ti-6Al-4V (wt %) and Ti-47Al-2Cr (at%) alloy disks from hydrogenated and dehydrogenated (HDH) and gas atomised powders (GA) powders (in the case of titanium and Ti-6Al-4V) and a mechanically milled powder (in the case of Ti-47Al-2Cr alloy). The bulk titanium and Ti-6Al-4V (wt %) alloy have been produced by forging of the powder compacts. The Ti-47Al-2Cr (at %) alloy was produced using canned powder compact forging of a Ti/Al/Cr composite powder. The purpose of the present study is to investigate the deformation and fracture behaviour of the bulk consolidated as-forged materials, by conducting tensile testing at room temperature (RT) and examination of the fractured specimens which had near-α, α + β and γ phase structures, respectively. It was found that as-forged bulk titanium disk produced using HDH powder showed a yield point with a yield strength of ~700 MPa and with a considerable amount of ductility. While the as-forged Ti-6Al-4V (wt %) alloy produced using HDH powder, fractured prematurely without any yielding. On the other hand yielding was observed in the as-forged Ti-6Al-4V (wt %) alloy produced using GA powder, showing a yield strength of ~970 MPa and a considerable amount of plastic strain to fracture. The bulk consolidated Ti-47Al-2Cr (at %) alloy also fractured prematurely with fracture strength of ~125 MPa. The mechanical behaviour of the as-forged bulk materials was found to be dependent on several factors such as initial powders used, green density of the powder compact, forging parameters used during forging. It was expected that the entrapped gas in green compacts, absorbed oxygen, porosity and inter-particle bonding play an important role on the quality of the as-forged material, which in turn affected the mechanical behaviour of the bulk material.Item type:Publication, The performance of thermally sprayed titanium based composite coatings in molten aluminium2011, ElsevierThe service life of die and tool steels in contact with molten aluminium is important in the aluminium processing industry. This article describes an investigation of the efficiency of thermally sprayed Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite coatings in resisting aluminium soldering on H13 tool steel. The powder feedstocks for making the composite coatings were produced by high energy mechanical milling of a mixture of Al and TiO₂ powders using different molar ratios followed by a thermal reaction process. The feedstocks were then thermally sprayed using a high velocity oxygen fuel (HVOF) technique onto an H13 steel substrate to produce composite coatings. The performance of the coatings was assessed in terms of Al soldering and liquid metal corrosion resistance after immersing in molten aluminium at a temperature of 700 ± 10 °C. The results of this study showed that composite coatings have a potential to act as a physical barrier to prevent aluminium attack on H13 tool steel. The nature of Al attack on H13 tool steel changed from generalised to more localised attack with the thermally sprayed coating. A Ti(Al,O)/Al₂O₃ composite coating was not attacked by molten aluminium, however localised attack on a H13 tool steel substrate was found to be caused by molten metal penetration through defects in the coating. Composite coating TiAl(O)/Al₂O₃ was attacked by molten aluminium resulting in dissolution of the coating. Composite coatings showed significantly lower dissolution in molten aluminium compared with the uncoated H13 steel. A Ti(Al,O)/Al₂O₃ composite coating was found to be a more effective protective coating than a TiAl(O)/Al₂O₃ composite coating due its greater resistance to molten aluminium attack.Item type:Publication, High temperature mechanical properties of Ti-47Al-2Cr (at %) alloy produced using powder compact forging of a mechanically milled powder2009, IOP PublishingUltrafine grained (UFG) Ti-47Al-2Cr (at %) alloy was prepared using a combination of high energy ball milling of a mixture of elemental powders to produce a Ti/Al/Cr composite powder and forging of compacts of this composite powder. The microstucture of the powder forged alloy was found to be dependent on the initial condition of the powder. The alloy produced by this method has demonstrated good formability, both in tensile and compression testings at elevated temperatures. A ductility of 80–165% in tension has been observed, while in a compression plastic strain of ~ 50% was found to be easily achievable, without causing cracking. The deformation behaviour of the particular alloy in tension and compression at elevated temperature has been discussed in detail. The results from the present investigation indicate that UFG Ti-47Al-2Cr (at %) alloy produced using powder compact forging has good formability, and is suitable precursor for near-net shaping using thermomechanical processes such as forging and superplastic forming.Item type:Publication, Effect of milling parameters on microstructure of Ti/Al composite powder produced by discus milling2006, World Scientific Publishing CoThe motivation of this research is to develop a process for producing Ti/Al composite powders that enable synthesis of a single-phase TiAl intermetallic bulk material, which is then used as a target for physical vapour deposition (PVD) coating. This study reports the effects of milling time, amount of process control agent (PCA) added as well as the powder-to-medium ratio on the microstructure of the Ti/Al composite powder. Optical microscopy and scanning electron microscopy (SEM) were used to evaluate the level of mixing and the resulting powder particle size. X-ray diffraction analysis and differential thermal analysis were used for determining the phase constituents and the solid state reaction temperature of the as-milled powders.Item type:Publication, Thermal stability of nanocrystalline copper films2006, World Scientific Publishing CoThe grain growth kinetics of nanocrystalline copper thin film samples was investigated. The grain size of nanocrystalline copper samples was determined from the broadening of X-ray spectra. It was found that the grain size increased linearly with isothermal annealing time within the first 10 minutes, beyond which power-law growth kinetics is applied. The activation energy for grain growth was determined by constructing an Arrhenius plot, which shows an activation energy of about 21 – 30 kJ/mol. The low activation energy is attributed to the second phase particle drag and the porosity drag, which act as the pinning force for grain growth in nanocrystalline copper.Item type:Publication, Fabrication of TiAl target by mechanical alloying and applications in physical vapour deposition coating2007, Trans Tech Publications LtdThe research involves the development of a powder metallurgical route for producing good quality TiAl targets for making physical vapour deposition (PVD) coatings. Mixtures of elemental titanium and aluminium powders were mechanically milled using a novel discus milling technique under various conditions. Hot isostatic pressing (HIP) was then employed for consolidation of the mechanically alloyed powders. A cathodic arc vapour deposition process was applied to produce a TiAIN coating. A microstructural examination was conducted on the target material and PVD coatings, using X-ray diffractometry (XRD), X-ray photoelectron spectrometry (XPS) and scanning electron microscopy (SEM). It has been found that combining mechanical alloying and HIP enable us to produce a fairly good quality of TiAl based target. The PVD coatings obtained from the TiAl target showed very high microhardness values.Item type:Publication, Discussions on grain refinement of magnesium alloys by carbon inoculation2005-03, ElsevierCarbon inoculation has no effect on magnesium alloys that do not contain aluminium. The hypothesis proposed in a recent article [Scripta Materialia 49 (2003) 1129] that segregation of carbon plays a major role in the grain refinement of magnesium alloys by carbon inoculation is inconsistent with many of the observed facts. The Al4C3 or Al–C–O hypothesis, which is supported by experimental observations, is still the most reasonable mechanism proposed to date for the grain refinement of magnesium alloys by carbon inoculation.Item type:Publication, Effect of manganese on grain refinement of Mg–Al based alloys2006-06, ElsevierManganese is a grain refiner for high purity Mg–3%Al, Mg–6%Al, Mg–9%Al, and commercial AZ31 (Mg–3%Al–1%Zn) alloys when introduced in the form of an Al–60%Mn master alloy splatter but the use of pure Mn flakes and ALTAB™ Mn75 tablets shows no grain refinement. Long time holding of the melt at 730 °C leads to an increase in grain size. The mechanism is attributed to the presence of an ε-AlMn phase (hexagonal close-packed) in the master alloy splatter.Item type:Publication, Effect of iron on grain refinement of high-purity Mg–Al alloys2004-07, Elsevier LtdThe effect of iron on the grain refinement of high-purity Mg–3%Al and Mg–9%Al alloys has been investigated using anhydrous FeCl3 as an iron additive at 750 °C in carbon-free aluminium titanite crucibles. It was shown that grain refinement was readily achievable for both alloys. Fe- and Al-rich intermetallic particles were observed in many magnesium grains.