University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts2013, ElsevierTi-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.Item type:Publication, High temperature deformation behavior of Ti–46Al–2Cr–4Nb–0.2Y alloy2012, ElsevierThe hot deformation characteristics of cast and hot isostatically pressed Ti-46Al-2Cr-4Nb-0.2Y (at%) alloy in the temperature range of 1100-1250°C and strain rate range of 0.01-1.0s -1 using hot compression tests were studied. The processing map of the alloy at true strain of 0.5 was also developed on the basis of the dynamic materials model (DMM). The experimental results show that the flow stress decreases significantly with increasing deformation temperature and decreasing strain rate. Using the kinetic rate equation the stress exponent n and the apparent activation energy of deformation Q were determined as 4.47 and 400.4kJmol -1, respectively. The efficiency values of power dissipation of the domain at strain rate below 0.4s -1 show that the dynamic recrystallization occurring of γ phase in the alloy is easier in the wide deformation temperature range (1100-1250°C) due to low stacking fault energy. The fraction of new recrystallized grains increased with increasing the hot deformation temperature at a given strain rate. With the increasing of strain rate, the uniformity of microstructure was decreased. The domain defined by the temperature range of 1200-1230°C and the strain rate range of 0.01-0.05s -1 which corresponds to a peak efficiency of about 60% is the optimal deformation condition of the alloy. Based on the optimal deformation conditions, a cylindrical sample was near isothermally forged. The microstructure and shape of pancake by forging was in good agreement with the prediction of processing map.Item type:Publication, Microstructure and mechanical properties of large size Ti-43Al-9V-0.2Y alloy pancake produced by pack-forging2013, ElsevierA pancake of Ti-43Al-9V-0.2Y (at.%) alloy with dimensions of ϕ480 mm × 46 mm was fabricated by pack-forging with a thick reduction of 80%. The as-forged Ti-43Al-9V-0.2Y alloy pancake has a duplex (DP) microstructure, which is composed of B2/α₂/γ lamellar colonies and massive B2 and γ phase regions distributed along the boundaries between the lamellar colonies. Different microstructures were obtained by heat treatment of samples cut from the as-forged Ti-43Al-9V-0.2Y alloy pancake. A fully lamellar (FL) structure consisting of B2/α₂/γ lamellar colonies was obtained after the heat treatment of 1350 °C/8 h. Tensile test results exhibited that the yield strength (YS) and ultimate tensile strength (UTS) of the alloy with DP microstructure were decreased from 680.7 MPa to 834.3 MPa at room temperature to 589.5 MPa and 693.1 MPa at 700 °C, respectively, and the elongation (δ) of the alloy with DP microstructure was increased from 1.99% at room temperature to 12.12% at 700 °C; the elongation (δ) of the alloy with FL microstructure was increased from 1.52% at room temperature to 85.84% at 800 °C.