<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 6 of 6
  • Item type:Publication,
    Mechanical behaviour of ultrafine grained Cu and Cu-(2.5 and 5) vol.%Al₂O₃ composites produced by powder compact forging
    2011, Trans Tech Publications
    Nanostructured Cu-(2.5 and 5) vol.%Al₂O₃ composite powders were produced from a mixture of Cu powder and Al₂O₃ nanopowder using high energy mechanical milling, and then compacted by hot pressing. The Cu and Cu- Al₂O₃ composite powder compacts were then forged into disks at temperatures in the range of 500-800°C to consolidate the Cu and Cu- Al₂O₃ composite powders. Tensile testing of the specimens cut from the forged disks showed that the Cu forged disk had a good ductility (plastic strain to fracture: ~15%) and high yield strength of 320 MPa, and the Cu-(2.5 and 5)vol.%Al₂O₃ composite forged disks had a high fracture strength in range of 530-600 MPa, but low ductility.
  • Item type:Publication,
    Microstructure and mechanical behaviour of ultrafine grained Al-4wt%Cu-(2.5-10) Vol.% SiC metal matrix composites produced by powder compact forging
    2011, Trans Tech Publications
    Ultrafine grained Al-4wt%Cu-(2.5-10) vol.% SiC metal matrix composite powders were produced from a mixture of Al, Cu and SiC powders using high energy mechanical milling (HEMM). The composite powders produced were first hot pressed at 300°C with a pressure of 240 MPa to produce cylindrical powder compacts with a relative density in the range of 80-94% which decreased with increasing the SiC volume fraction. Powder compact forging was utilized to consolidate the powder compacts into nearly fully dense forged disks. With increasing the volume fraction of SiC from 2.5% to 10%, the average microhardness of the forged disks increased from 73HV to 162HV. The fracture strength of the forged disks increased from 225 to 412 MPa with increasing the volume fraction of SiC particles from 2.5 to 10%. The Al-4wt%Cu-2.5vol.%SiC forged disk did not show any macroscopic plastic yielding, while the Al-4wt%Cu-(7.5 and 10)vol.% SiC forged disk showed macroscopic plastic yielding with a small plastic strain to fracture (~1%).
  • Item type:Publication,
    Microstructure and thermal stability of nanostructured Cu-7.5vol.%Al₂O₃ composite powders produced by high energy mechanical milling
    2009, IOP Science
    Nanostructured Cu-7.5vol.%Al₂O₃ composite powders were produced from a mixture of Cu powder and Al₂O₃ nanopowder using two routes of high energy mechanical milling. The milled composite powders were heat treated at 150, 300, 400 and 500°C for 1 hour, respectively, to determine the thermal stability of the microstructure and corresponding micohardness change of the powder particles as a function of the annealing temperature. For the nanocomposite powder produced with 12 hours of milling (Route 1), heat treatment at 150°C did not change the microstructure, increasing the annealing temperature from 150 to 500°C caused the Cu grain sizes to increase due to grain coarsening. For the composite powder produced with 24 hours milling (Route 2), the grain sizes of the Cu matrix also increased due to grain coarsening with increasing the annealing temperature from 150 to 500°C. Average microhardness decreased significantly for both the nanocomposite powders but the degree of grain size increase was smaller with increasing the annealing temperature from 400 to 500°C.
  • Item type:Publication,
    Consolidation of ultrafine-grained Cu powder and nanostructured Cu–(2.5–10) vol%Al₂O₃composite powders by powder compact forging.
    2010, Springer
    An as-received ultrafine-grained Cu powder and four nanostructured Cu–(2.5–10) vol%Al2O3 composite powders produced by high-energy mechanical milling of mixtures of the Cu powder and an Al₂O₃ nanopowder were consolidated using warm powder compaction followed by open die powder compact forging. The circular discs produced in the experiments achieved full densification. Tensile testing of the specimens cut from the forged discs showed that the Cu-forged disc had a fairly high yield strength of 330 MPa, UTS of 340 MPa and a plastic strain to fracture of 15%, but the Cu– Al₂O₃ composite-forged discs did not show any macroscopic plastic yielding. The fracture strength of the composite-forged discs decreased almost linearly with the increase of the volume fraction of Al₂O₃ nanoparticles. This study shows that a high level of consolidation of the ultrafine-grained Cu powder and the nanostructured Cu–2.5 vol% Al₂O₃ composite powder has been achieved by warm powder compacting at 350 °C and powder compact forging at 500 and 700 °C. However, this is not true for the nanostructured Cu–(5, 7.5 and 10) vol% Al₂O₃ composite powders, possibly due to their higher powder particle hardness at elevated temperatures in the range of 350–800 °C.
  • Item type:Publication,
    Thermal stability and microhardness of Cu-10vol.%Al2O3nanocomposite produced by high energy mechanical milling
    2010, IOPScience
    Cu-10vol.%Al₂O₃ nanocomposite powders were produced using two high energy milling routes and heat treated at 150, 300, 400 and 500°C for 1 hour, respectively, to determine the thermal stability of the microstructure and the micohardness change of the materials as a function of the annealing temperature. Annealing of the as-milled powders at 150°C caused recovery and recrystallisation that leads to significant decrease in dislocation density and slight decrease of microhardness. Increasing the annealing temperature to 400°C causes slight coarsening of the Cu grains and corresponding slight decrease of microhardness. Further increasing the annealing temperature to 500°C causes significant coarsening of the Cu grains and cause significant decrease in microhardness. The effects of different factors on the thermal stability and micohardness change of the Cu- Al₂O₃ are discussed.
  • Item type:Publication,
    Synthesis and thermal stability of Cu-(2.5-10)vol.%Al₂O₃ nanocomposite powders by high energy mechanical milling
    2009, IOPscience
    High energy mechanical milling (HEMM) of a mixture of Cu powder and Al₂O₃ nanopowder has been used to produce Cu-(2.5-10)vol.%Al₂O₃ nanocomposite powders with a ultrafine grained or nanocrystalline Cu matrix. The microstructure and microhardness of the as-milled powder particles and the thermal stability and microhardness change of the nanocomposite powder particles caused by annealing at temperatures up to 500oC have been studied. It is shown that HEMM can be effectively used to disperse (2.5-10)vol.% Al₂O₃ nanoparticles into a ultrafine grained or nanocrystalline Cu matrix. Using larger diameter balls or increasing the volume fraction of Al₂O₃ nanoparticles to 7.5% or higher allows synthesis of Cu-Al₂O₃ nanocomposite powders with nanocrystalline Cu matrix. Refining the microstructure of the Cu matrix and increasing the volume fraction of Al₂O₃ nanoparticles in the nanocomposite both increase the thermal stability of the nanocomposite structure.