<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 10 of 16
  • Item type:Publication,
    Analysis of mechanical properties of hemp fibre reinforced unsaturated polyester composites
    2013, Sage
    Different chemically treated hemp fibre reinforced unsaturated polyester composites were investigated over a range of fibre content (0–60 wt%). Although Young’s modulus of all the short fibre reinforced unsaturated polyester composites was found to be higher than that of unreinforced unsaturated polyester; however, tensile strength of the composites exceeded that of the unsaturated polyester matrix only for the combined alkali- and silane-treated fibre composites at 40 wt% fibre content. The decrease in tensile strength of the composites could be attributed to stress concentrations caused by the fibres in conjunction with the brittle matrix. Impact strength of all the treated fibre composites was higher than that of the untreated fibre composites at all fibre contents. KIc and GIc of the composites decreased initially and thenincreased as the fibre content increased because more and more fibres being available to pull-out. The mechanical properties of the composites were increased further due to the alignment of long fibres.
  • Item type:Publication,
    A study of polyvinyl butyryl based binder system in titanium based metal injection moulding
    2012, Trans Tech Publications
    Metal injection moulding (MIM) is an innovative injection moulding technique widely used to produce complex shaped components from feedstock composed of metal powders and thermosetting or thermoplastic binders. In MIM, binder selection and formulation are considered as critical processes since binder characteristics dictate the success of MIM. The purpose of this study is to determine the feasibility of polyvinyl butyryl (PVB) based binder system in Ti-6Al-4V(wt.%)/binder feedstock, as well as to understand the effects of key parameters, such as powder loading and mixing conditions on the rheological properties of a feedstock. In this study, PVB, polyethylene glycol (PEG), and stearic acid (SA) were chosen to formulate a multi-component binder system to prepare Ti-6Al-4V based feedstock with the aid of three types of mixers: a compounder, a modified mechanical mixer and a twin screw extruder. Further, morphological analysis was performed using optical microscopy and scanning electron microscopy. Thermal analysis was performed using simultaneous differential thermal analysis and thermogravimetric analysis. Results showed that binder formulation was reasonably successful with the aid of both mechanical mixer and a twin screw extruder under certain mixing conditions, and the critical powder loading was 68 vol.%, resulting in an optimum powder loading of 63 vol.%.
  • Item type:Publication,
    The Effect of Aqueous Urea on the Processing, Structure and Properties of CGM
    2012-06, Springer
    Corn gluten meal (CGM) is potentially a cost-effective raw material for producing a bioderivable thermoplastic. However, CGM disintegrates to a powder subsequent to processing with polar plasticisers, such as water. The hypothesis of this study was that aqueous urea could be used to denature protein within CGM and therefore encourage protein–protein interactions leading to consolidated bioplastics when using water as a plasticiser. To assess this, the effects of aqueous urea on structure and properties of CGM with particular focus on storage were assessed. Processing of CGM with aqueous urea produced consolidated materials. FTIR analysis showed secondary structure was modified during processing, leading to increased amounts of α-helices and random coils and reduction of the amount of intermolecular β-sheets and turns. Above 6 wt% free water, the plasticising efficiency of water in processed CGM increased as the amount of denatured proteins increased. Below 6 wt% free water, protein secondary structure did not have a significant influence on thermal and flexural properties. It was found that storage environment and urea concentration influenced the rate of drying, however, the final water content was constant relative to CGM, and not urea. The materials were resistant to cracking at urea concentrations above 8 M, provided the mass loss during storage did not exceed 15 wt%.
  • Item type:Publication,
    Flexural properties of hemp fibre reinforced polylactide and unsaturated polyester composites
    2011, Elsevier
    In this work, flexural strength and flexural modulus of chemically treated random short and aligned long hemp fibre reinforced polylactide and unsaturated polyester composites were investigated over a range of fibre content (0–50 wt%). Flexural strength of the composites was found to decrease with increased fibre content; however, flexural modulus increased with increased fibre content. The reason for this decrease in flexural strength was found to be due to fibre defects (i.e. kinks) which could induce stress concentration points in the composites during flexural test, accordingly flexural strength decreased. Alkali and silane fibre treatments were found to improve flexural strength and flexural modulus which could be due to enhanced fibre/matrix adhesion.
  • Item type:Publication,
    Microstructure and mechanical behaviour of ultrafine grained Al-4wt%Cu-(2.5-10) Vol.% SiC metal matrix composites produced by powder compact forging
    2011, Trans Tech Publications
    Ultrafine grained Al-4wt%Cu-(2.5-10) vol.% SiC metal matrix composite powders were produced from a mixture of Al, Cu and SiC powders using high energy mechanical milling (HEMM). The composite powders produced were first hot pressed at 300°C with a pressure of 240 MPa to produce cylindrical powder compacts with a relative density in the range of 80-94% which decreased with increasing the SiC volume fraction. Powder compact forging was utilized to consolidate the powder compacts into nearly fully dense forged disks. With increasing the volume fraction of SiC from 2.5% to 10%, the average microhardness of the forged disks increased from 73HV to 162HV. The fracture strength of the forged disks increased from 225 to 412 MPa with increasing the volume fraction of SiC particles from 2.5 to 10%. The Al-4wt%Cu-2.5vol.%SiC forged disk did not show any macroscopic plastic yielding, while the Al-4wt%Cu-(7.5 and 10)vol.% SiC forged disk showed macroscopic plastic yielding with a small plastic strain to fracture (~1%).
  • Item type:Publication,
    Influence of hygrothermal ageing on the physico-mechanical properties of alkali treated industrial hemp fibre reinforced polylactic acid composites
    2010, SpringerLink
    30 wt% aligned untreated long hemp fibre/polylactic acid (AUL) and aligned alkali treated long hemp fibre/polylactic acid (AAL) composites were produced by film stacking and subjected to hygrothermal ageing environment along with neat polylactic acid (PLA). Hygrothermal ageing was carried out by immersing samples in distilled water at 25 and 50 ºC over a period of 3 months. It was found that both neat PLA and composites followed Fickian diffusion. Higher temperature generally increased the Diffusion coefficient, D of neat PLA and composites, as well as shortening the saturation time. Neat PLA had the lowest D value followed by AAL composites and then AUL composites. After hygrothermal ageing, tensile and flexural strength, Young’s and flexural modulus and KIc were found to decrease and impact strength was found to increase for both AUL and AAL composites. AUL composites had greater overall reduction in mechanical properties than that for AAL composites after hygrothermal ageing. Crystallinity contents of the hygrothermal aged composites support the results of the deterioration of mechanical properties upon exposure to hygrothermal ageing environment.
  • Item type:Publication,
    Influence of alkali fiber treatment and fiber processing on the mechanical properties of hemp/epoxy composites
    2010-10, Wiley
    Industrial hemp fibers were treated with a 5 wt % NaOH, 2 wt % Na₂SO₃ solution at 120°C for 60 min to remove noncellulosic fiber components. Analysis of fibers by lignin analysis, scanning electron microscopy (SEM), zeta potential, Fourier transform infrared (FTIR) spectroscopy, wide angle X-ray diffraction (WAXRD) and differential thermal/thermogravimetric analysis (DTA/TGA), supported that alkali treatment had (i) removed lignin, (ii) separated fibers from their fiber bundles, (iii) exposed cellulose hydroxyl groups, (iv) made the fiber surface cleaner, and (v) enhanced thermal stability of the fibers by increasing cellulose crystallinity through better packing of cellulose chains. Untreated and alkali treated short (random and aligned) and long (aligned) hemp fiber/epoxy composites were produced with fiber contents between 40 and 65 wt %. Although alkali treatment generally improved composite strength, better strength at high fiber contents for long fiber composites was achieved with untreated fiber, which appeared to be due to less fiber/fiber contact between alkali treated fibers. Composites with 65 wt % untreated, long aligned fiber were the strongest with a tensile strength (TS) of 165 MPa, Young's modulus (YM) of 17 GPa, flexural strength of 180 MPa, flexural modulus of 9 GPa, impact energy (IE) of 14.5 kJ/m², and fracture toughness (KIc) of 5 MPa m1/2
  • Item type:Publication,
    Improvement of mechanical performance of industrial hemp fibre reinforced polylactide biocomposites
    2011-03, Elsevier
    In this work, mechanical properties of chemically treated random short fibre and aligned long hemp fibre reinforced PLA composites were investigated over a range of fibre content (0–40 wt.%). It was found that tensile strength, Young’s modulus and impact strength of short hemp fibre reinforced PLA composites increased with increased fibre content. Alkali and silane fibre treatments were found to improve tensile and impact properties which appears to be due to good fibre/matrix adhesion and increased matrix crystallinity. A 30 wt.% alkali treated fibre reinforced PLA composite (PLA/ALK) with a tensile strength of 75.5 MPa, Young’s modulus of 8.18 GPa and impact strength of 2.64 kJ/m2 was found to be the best. However, plane-strain fracture toughness and strain energy release rate decreased with increased fibre content. The mechanical properties of the PLA/ALK composites were increased further due to alignment of long fibres.
  • Item type:Publication,
    Characterisation of hemp fibre reinforced Poly(Lactic Acid) composites
    2009, Inderscience Enterprises
    In this work, the mechanical properties including tensile strength, flexural strength, impact strength and fracture toughness of the PLA/hemp composites were investigated over a range of fibre content (0-30 wt.%). It was observed that, the tensile strength and Young's modulus of the composites increased with increased fibre content. The flexural strength did not increase with fibre reinforcement, however, the flexural modulus of the composites increased significantly. Impact strength of the composites increased up to 20 wt. % fibre loading, however, further increased fibre loading caused a reduction of impact strength. KIc and GIc values decreased with increased fibre content.
  • Item type:Publication,
    Hemp fibre reinforced composites using chelator and enzyme treatments
    2010, Elsevier
    The main objective of the current work was to investigate using chelator treatment, and combined chelator and enzyme treatments, to separate hemp fibre from its bundles, as well as remove non-cellulosic compounds, and thus therefore improve the interfacial bonding in the composite. Wet chemical analysis, FTIR, X-ray diffraction (XRD), thermal analysis and single fibre tensile testing were used to characterise the effect of treatment on hemp fibres. The higher chelator concentration treated hemp fibre composites had the highest tensile strength of 42 MPa, an increase of 19% compared to composites with untreated hemp fibre.