University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
41 results
Search Results
Item type:Publication, Microstructure development and properties of alumina–Ti aluminide interpenetrating composites2006, ElsevierInterpenetrating phase Al₂O₃–Ti₃Al composites have been fabricated by reaction sintering of 2 and 4-h discus milled composite powders containing Al and TiO₂ using controlled heat-treatment in non-oxidizing atmospheres. Pressureless sintering and hot pressing of the powders has been carried out under vacuum and argon at temperatures between 1278 °C and 1500 °C and a heating rate of 5 °C/min. Densification of the composites was investigated as a function of temperature. It was shown that lower porosity was obtained by hot pressing compared to pressureless sintering. The microstructure development and mechanical properties of dense Al₂O₃–Ti₃Al composites fabricated by hot pressing of Al–TiO₂ powder blends were examined. Fully dense microstructures could be achieved by hot pressing at 1387 °C under vacuum. An increase of Vickers hardness was observed with increasing temperature, which can be attributed to the increase of density and the decrease in the level of porosity of the composites. The mechanical behaviour exhibited by the composites can be related to properties such as Al₂O₃ particle size and porosity level. Fracture toughness of 6.3 ± 0.8 MPa m1/2 and Vickers hardness of 13.6 ± 0.4 GPa were achieved for the fully dense composite produced by hot pressing discus milled powder.Item type:Publication, Sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites2006, ElsevierThe sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites produced using Al/TiO₂ composite powders have been studied. Ti(Al,O), Ti₃Al(O) and TiAl(O) represent α-Ti phase with dissolved Al and O, and Ti3Al and TiAl phases with dissolved O, respectively. The Al/TiO₂ composite powders were produced by high energy mechanical milling using Al and TiO₂ powders as the starting materials. It was found that the matrices of the composites became fully dense after sintering at 1550 °C, and the Al₂O₃ particles became fully sintered when the sintering temperature was increased to 1650 °C. The reactions between Al and TiO₂ which occur during heating the powder compacts to 1400 °C have little effect on the sintering of the composite powders. The Al₂O₃ particles in the composites become significantly coarsened during sintering at 1550 °C or above, and the coarsening rate of the Al₂O₃ particles increases in the order of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl/Al₂O₃ composites. This can be attributed to the decrease of the solidus temperature or melting points of the corresponding matrices. It is evident that in the initial stage of sintering, coarsening of the Al2O₃ particles occurs through coalescence. Hipping of the pre-sintered composites at 1300 °C with a pressure of 200 MPa without canning causes significant increase of the density and substantial further coarsening of the Al₂O₃ particles.Item type:Publication, Investigation of a discus-milling process using a powder mixture of Al and TiO₂2006, SpringerIn this study, a powder mixture of Al and TiO₂ was employed to investigate the milling process in a discus mill. In this first report on this novel mechanical mill, several variables, including the milling time and powder charge and their effects on the microstructural evolution of powder particles, are monitored and studied. The study reveals that the dominant parameters of the milling process are the milling time and the starting powder charge, similar to the other high-energy ball-milling processes. The longer the milling time and the smaller the starting powder charge, the more homogeneous the mixing and the finer the microstructure of the powder particles. The reaction between Al and TiO₂ was not observed with a milling period as long as 6 hours, for the present materials. However, the reaction between Al and TiO₂, during the subsequent heat treatment, is influenced by the milling condition. The powders with the longer milling times and finer mixing microstructures also form a finer microstructure, after the reaction between Al and TiO₂ during heat treatment. The methods for achieving an optimal milling efficiency for the Al- TiO₂ system are discussed.Item type:Publication, Factors controlling the tensile properties of ultrafine structured Cu–5vol%Al₂O₃ nanocomposite prepared by high energy mechanical milling and powder compact extrusion2013, ElsevierThe microstructures and tensile properties of two ultrafine structured Cu–5vol%Al₂O₃ nanocomposite samples made by a combination of high energy mechanical milling of a mixture of Cu powder and gamma Al₂O₃ nanopowder and powder compact extrusion were studied. The sample extruded at 750 °C exhibited a microstructure consisting of Cu grains with sizes in the range of 100–500 nm and a dispersion of Al₂O₃ nanoparticles with sizes in the range of 20–345 nm. With the extrusion temperature increasing to 900 °C, the Cu grain sizes remained almost unchanged, but a large fraction of the Al₂O₃ nanoparticles were dissolved, leading to possible formation of nanometer sized Al³⁺/O²⁻ clusters. This microstructural difference of the two samples causes an interesting difference in tensile properties, with the sample extruded at 900 °C showing approximately 150 MPa higher yield strength and ultimate tensile strength and also better ductility than the sample extruded at 750 °C. It appears that this significant beneficial effect of dissolution of Al₂O₃ nanoparticles is mainly caused by the significant strengthening effect of the nanometer sized Al³⁺/O²⁻ clusters through Orowan mechanism.Item type:Publication, The development of porous titanium products using slip casting2013, ElsevierAn optimized titanium slurry was developed from 43 vol.% of titanium powder, 0.3 dw.% of dispersant, 0.8 dw.% of plasticizer and 0.8 dw.% of binder, mixed with a balance of distilled water, which produced a viscosity of 40 cP. It was then poured into a plaster mold to form compacts with a green density of 45%. Thermal debinding was carried out at 320 ℃ with an argon flow for 2 h, followed by vacuum sintering different samples at 1000 ℃ and 1200 ℃ for 0.5 h, respectively. The porous sintered compacts had satisfactory tensile strength with some plastic deformation. The increase in oxygen and carbon content during processing was minor. An X-ray diffraction pattern showed pure alpha titanium peaks without any indication of contamination from organic additives. The results from this investigation suggested that slip casting is a potentially low-cost, simple production route for manufacturing porous titanium products.Item type:Publication, Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts2013, ElsevierTi-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.Item type:Publication, High temperature deformation behavior of Ti–46Al–2Cr–4Nb–0.2Y alloy2012, ElsevierThe hot deformation characteristics of cast and hot isostatically pressed Ti-46Al-2Cr-4Nb-0.2Y (at%) alloy in the temperature range of 1100-1250°C and strain rate range of 0.01-1.0s -1 using hot compression tests were studied. The processing map of the alloy at true strain of 0.5 was also developed on the basis of the dynamic materials model (DMM). The experimental results show that the flow stress decreases significantly with increasing deformation temperature and decreasing strain rate. Using the kinetic rate equation the stress exponent n and the apparent activation energy of deformation Q were determined as 4.47 and 400.4kJmol -1, respectively. The efficiency values of power dissipation of the domain at strain rate below 0.4s -1 show that the dynamic recrystallization occurring of γ phase in the alloy is easier in the wide deformation temperature range (1100-1250°C) due to low stacking fault energy. The fraction of new recrystallized grains increased with increasing the hot deformation temperature at a given strain rate. With the increasing of strain rate, the uniformity of microstructure was decreased. The domain defined by the temperature range of 1200-1230°C and the strain rate range of 0.01-0.05s -1 which corresponds to a peak efficiency of about 60% is the optimal deformation condition of the alloy. Based on the optimal deformation conditions, a cylindrical sample was near isothermally forged. The microstructure and shape of pancake by forging was in good agreement with the prediction of processing map.Item type:Publication, Microstructure and mechanical properties of large size Ti-43Al-9V-0.2Y alloy pancake produced by pack-forging2013, ElsevierA pancake of Ti-43Al-9V-0.2Y (at.%) alloy with dimensions of ϕ480 mm × 46 mm was fabricated by pack-forging with a thick reduction of 80%. The as-forged Ti-43Al-9V-0.2Y alloy pancake has a duplex (DP) microstructure, which is composed of B2/α₂/γ lamellar colonies and massive B2 and γ phase regions distributed along the boundaries between the lamellar colonies. Different microstructures were obtained by heat treatment of samples cut from the as-forged Ti-43Al-9V-0.2Y alloy pancake. A fully lamellar (FL) structure consisting of B2/α₂/γ lamellar colonies was obtained after the heat treatment of 1350 °C/8 h. Tensile test results exhibited that the yield strength (YS) and ultimate tensile strength (UTS) of the alloy with DP microstructure were decreased from 680.7 MPa to 834.3 MPa at room temperature to 589.5 MPa and 693.1 MPa at 700 °C, respectively, and the elongation (δ) of the alloy with DP microstructure was increased from 1.99% at room temperature to 12.12% at 700 °C; the elongation (δ) of the alloy with FL microstructure was increased from 1.52% at room temperature to 85.84% at 800 °C.Item type:Publication, Optimisation of performance of dispersants in aqueous titanium slips2012, Trans Tech PublicationsSlip casting is a well-established ceramic casting technique used for large scale fabrication of ceramic products with complex shapes. A homogenous slip with a desired level of stability is required, which is controlled using a dispersant. This paper describes the selection and optimisation of various dispersants used to produce Ti powder slips. A consideration of the effect of concentration and pH of the solvent on the dispersion of anionic polyelectrolyte dispersants (Dispex N-40, Synthecol SD375 & Dolapix CE64) was examined by measuring the sedimentation height and rate, the streaming potential and the slip viscosity. It was found that Dolapix CE64 showed the best deflocculating effect at 0.3dw.% with pH of 7. In particular, the measurements on Dolapix CE64 gave consistent results. This indicated that Dolapix CE64 is an effective dispersant in the preparation of a titanium slip.Item type:Publication, Modification of sintered titanium alloys by hot isostatic pressing2012, Trans Tech PublicationsPowder metallurgy (PM) permits to obtain titanium alloys with properties and microstructures close to ingot metallurgy products. However, residual porosity is normally present in the products produced by the PM route of powder pressing and sintering (P&S)\, and this needs to be reduced by using post-sintering process step such as hot isostatic pressing (HIP) and forging. In this study, the microstructural and mechanical property changes caused by HIP of samples of two alloys, near-α Ti-3Al-2.5V alloy and α+β Ti-6Al-4V, produced by P&S route were investigated. Two types of powders were utilised: prealloyed powders and blend of elemental titanium powder and master alloy powder. Four conditions defined by HIP temperature, pressure and time were used to HIP the sintered samples with two geometries. The results show that, independent of the HIP conditions used, HIP increased the relative density of the samples to approximately 97.5% and their hardness by 30-50 HV depending on the HIP condition. However, HIP at 1000°C changes the fracture mode of the sintered samples from ductile to brittle.