<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 5 of 5
  • Item type:Publication,
    Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts
    2013, Elsevier
    Ti-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.
  • Item type:Publication,
    Modification of sintered titanium alloys by hot isostatic pressing
    2012, Trans Tech Publications
    Powder metallurgy (PM) permits to obtain titanium alloys with properties and microstructures close to ingot metallurgy products. However, residual porosity is normally present in the products produced by the PM route of powder pressing and sintering (P&S)\, and this needs to be reduced by using post-sintering process step such as hot isostatic pressing (HIP) and forging. In this study, the microstructural and mechanical property changes caused by HIP of samples of two alloys, near-α Ti-3Al-2.5V alloy and α+β Ti-6Al-4V, produced by P&S route were investigated. Two types of powders were utilised: prealloyed powders and blend of elemental titanium powder and master alloy powder. Four conditions defined by HIP temperature, pressure and time were used to HIP the sintered samples with two geometries. The results show that, independent of the HIP conditions used, HIP increased the relative density of the samples to approximately 97.5% and their hardness by 30-50 HV depending on the HIP condition. However, HIP at 1000°C changes the fracture mode of the sintered samples from ductile to brittle.
  • Item type:Publication,
    Comparison of blended elemental (BE) and mechanical alloyed (MA) powder compact forging into Ti-6Al-4V rocker arms
    2012, Trans Tech Publications
    Ti-6Al-4V rocker arms for internal combustion engines were produced by forging of compacts of blended powder consisting of elemental hydride-dehydride (HDH) titanium powder and Al60V40 (wt%) master alloy powder or mechanical alloyed (MA) powder synthesized by high energy mechanical milling of a mixture of HDH titanium and Al60V40 master alloy powders. The powder compacts were made by warm compaction, and their relative density was 90%. The mechanical properties and microstructures of as-forged parts made using blended powder were improved significantly with increasing holding time at forging temperature, and close to those of as-forged parts produced by powder compact forging of HDH Ti-6Al-4V pre-alloyed powder. However, the as-forged part produced by powder compact forging of MA powder was brittle, and fractured prematurely during tensile testing.
  • Item type:Publication,
    Tensile properties of Ti-6Al-4V discs produced by open die powder compact forging of pre-alloyed HDH powders
    2012, Trans Tech Publications
    Open die powder compact forging was employed for consolidation of Ti-6Al-4V(wt.%) powders which were produced by a hydride-dehydride (HDH) process. The powders were initially warm-compacted into cylindrical shapes. Induction heating was used for preheating the compacts prior to forging into plates. The effect of the forging parameters such as temperature and pre-sintering time on the microstructure and tensile properties of the forged plates were studied. Porosity and the alpha-beta phase distribution were investigated to enable a better understanding of their effect on the fracture behaviour of the tensile tested specimens. The fracture surfaces of the broken tensile specimens were analysed using Scanning Electron Microscopy (SEM) to find the correlation between microstructure, residual porosity and fracture behaviour. A combination of high ultimate tensile strength of over 1200MPa and a good ductility reflected by an elongation to fracture of around 10% was achieved in some of the forged discs.
  • Item type:Publication,
    Effects of lubrication on the powder metallurgy processing of titanium
    2012, Trans Tech Publications
    The role of lubrication on the consolidation behaviour of titanium powder, density increase and change in microstructure on subsequent sintering was investigated. HDH titanium powder mixed with 0-2wt% stearic acid or magnesium stearate was cold compacted. It was found that 0.3-0.6wt% of internal lubricant significantly improves the compressibility. However, more than 0.6wt% of lubricant aids the densification in the low-pressure region but limits the maximum density at high pressure. Moreover, 0.3-0.6wt% of lubricant offers a more uniform density distribution to the powder compact, while greater than 0.6wt% of lubricant leads to a segregation of lubricant in the surface region. The shape retention, ejection behaviour, de-lubrication behaviour and sintered properties were also studied in this work.