  • Item type:Publication,
    A symmetric and interconnected skeleton structural (SISS) model for predicting thermal and electrical conductivity and Young’s modulus of porous foams
    2008, Elsevier
    A symmetric and interconnected skeleton structural (SISS) model is proposed for predicting the thermal and electrical conductivities and Young’s modulus of open-cell foams with hollow and solid struts. The model predicted the effective thermal and electrical conductivities of solid-strut aluminium foams and other open-cell foams for the entire porosity range. The SISS model provided upper and lower bounds for the effective thermal conductivity and Young’s modulus of hollow-strut open-cell nickel foams. The SISS model was also found to predict the effective thermal conductivity of closed-cell graphite foams, and the effective electrical conductivity and Young’s modulus of closed-cell aluminium foams with reasonable accuracy. By analogy, the SISS model might also be applied to other physical properties.
  • Item type:Publication,
    Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts
    2013, Elsevier
    Ti-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.
  • Item type:Publication,
    Analysis of mechanical properties of hemp fibre reinforced unsaturated polyester composites
    2013, Sage
    Different chemically treated hemp fibre reinforced unsaturated polyester composites were investigated over a range of fibre content (0–60 wt%). Although Young’s modulus of all the short fibre reinforced unsaturated polyester composites was found to be higher than that of unreinforced unsaturated polyester; however, tensile strength of the composites exceeded that of the unsaturated polyester matrix only for the combined alkali- and silane-treated fibre composites at 40 wt% fibre content. The decrease in tensile strength of the composites could be attributed to stress concentrations caused by the fibres in conjunction with the brittle matrix. Impact strength of all the treated fibre composites was higher than that of the untreated fibre composites at all fibre contents. KIc and GIc of the composites decreased initially and thenincreased as the fibre content increased because more and more fibres being available to pull-out. The mechanical properties of the composites were increased further due to the alignment of long fibres.
  • Item type:Publication,
    Flexural properties of hemp fibre reinforced polylactide and unsaturated polyester composites
    2011, Elsevier
    In this work, flexural strength and flexural modulus of chemically treated random short and aligned long hemp fibre reinforced polylactide and unsaturated polyester composites were investigated over a range of fibre content (0–50 wt%). Flexural strength of the composites was found to decrease with increased fibre content; however, flexural modulus increased with increased fibre content. The reason for this decrease in flexural strength was found to be due to fibre defects (i.e. kinks) which could induce stress concentration points in the composites during flexural test, accordingly flexural strength decreased. Alkali and silane fibre treatments were found to improve flexural strength and flexural modulus which could be due to enhanced fibre/matrix adhesion.
  • Item type:Publication,
    Mechanical properties and fracture behaviour of nanostructured and ultrafine structured TiAl Alloys synthesised by mechanical milling of powders and hot isostatic pressing
    2011, Trans Tech Publications
    Bulk nanostructured (grain sizes in the range of 50-200nm) and ultrafine structured (grain sizes in the range of 100-500nm) γ-TiAl based alloys with compositions Ti-47Al (in at%) and Ti–45Al–2Cr–2Nb–1B–0.5Ta (in at%), respectively, have been produced using a combination of high energy mechanical milling of mixtures of elemental powders and hot isostatic pressing at 800 and 1000oC respectively, and the microstructures of the samples have been characterised. At room temperature, the HIPed samples fractured prematurely at tensile stresses in the range of 200-300MPa and showed no ductility, very likely due to the relative high oxygen content (0.6wt%) in the samples and very low tolerance of TiAl based alloys on dissolved oxygen. At 800oC, the HIPed samples showed a yield strength in the range of 55-70MPa, a tensile strength in the range of 60-80MPa, a large amount of elongation to fracturing around 100% and clear strain softening. Examination of the fractured tensile test specimens at room temperature and 800oC showed that the level of the consolidation was fairly high, but the HIPed samples do contain a small fraction of interparticle boundaries with weak atomic bonding. The fracture of the HIPed samples in tensile testing at room temperature and 800oC, respectively, is predominately intergranular, and the large amount of plastic deformation prior to fracture at 800oC is achieved mainly through grain boundary sliding in conjunction with dislocation gliding, in agreement with the deformation mechanisms of nanostructured and ultrafine structured alloys generally agreed by researchers.
  • Item type:Publication,
    Mechanical properties and water absorption of thermoplastic bloodmeal
    2011, Wiley Online Library
    Bloodmeal mixtures containing SS, water, SDS and urea were extruded and injection-molded. Increased chain mobility with sufficient plasticization during processing increased the amount of available amino acids for strong water/protein interactions. Materials containing low water and increased SS had reduced tensile strength and elongation, compared to higher water at the same SS content. Materials containing three parts SS per hundred parts bloodmeal (pphbm), 60 pphbm water and 20 pphbm urea, were the only ductile materials after conditioning. Changing any one of these factors to a lower level will result in a brittle material. This mixture in combination with 3 pphbm SDS resulted in optimal mechanical properties (tensile strength of 9.6 MPa and Young's modulus of 534.9 MPa).
  • Item type:Publication,
    Degradation as a result of UV radiation of bloodmeal-based thermoplastics
    2011, Elsevier
    Polymers are known for their susceptibility to degradation as a result of ultra-violet (UV) radiation. In this study, the UV stability of bloodmeal-based thermoplastics (BMT) was evaluated over a period of 12 weeks. Formulations with and without plasticiser were tested and moisture was excluded during accelerated weathering to isolate the effect of UV because of the material’s known sensitivity to moisture. It was found that embrittlement due to loss of water overshadowed the effect of UV degradation. Embrittlement caused the material’s toughness to be reduced by an order of magnitude after only two weeks of exposure, for either plasticised or unplasticised samples. An initial increase in tensile strength was observed after two weeks followed by a steady decline in strength. The elastic modulus reached a plateau after about two weeks of exposure. FTIR did not confirm any chemical changes after 12 weeks exposure and TGA suggested that low molecular mass species were quickly lost during the course of the test. The absence of chemical changes does not suggest resistance to environmental degradation, although the dark pigmentation of bloodmeal may have contributed to the lack of UV degradation. Embrittlement remains a greater concern and requires further attention.
  • Item type:Publication,
    Influence of alkali fiber treatment and fiber processing on the mechanical properties of hemp/epoxy composites
    2010-10, Wiley
    Industrial hemp fibers were treated with a 5 wt % NaOH, 2 wt % Na₂SO₃ solution at 120°C for 60 min to remove noncellulosic fiber components. Analysis of fibers by lignin analysis, scanning electron microscopy (SEM), zeta potential, Fourier transform infrared (FTIR) spectroscopy, wide angle X-ray diffraction (WAXRD) and differential thermal/thermogravimetric analysis (DTA/TGA), supported that alkali treatment had (i) removed lignin, (ii) separated fibers from their fiber bundles, (iii) exposed cellulose hydroxyl groups, (iv) made the fiber surface cleaner, and (v) enhanced thermal stability of the fibers by increasing cellulose crystallinity through better packing of cellulose chains. Untreated and alkali treated short (random and aligned) and long (aligned) hemp fiber/epoxy composites were produced with fiber contents between 40 and 65 wt %. Although alkali treatment generally improved composite strength, better strength at high fiber contents for long fiber composites was achieved with untreated fiber, which appeared to be due to less fiber/fiber contact between alkali treated fibers. Composites with 65 wt % untreated, long aligned fiber were the strongest with a tensile strength (TS) of 165 MPa, Young's modulus (YM) of 17 GPa, flexural strength of 180 MPa, flexural modulus of 9 GPa, impact energy (IE) of 14.5 kJ/m², and fracture toughness (KIc) of 5 MPa m1/2
  • Item type:Publication,
    Improvement of mechanical performance of industrial hemp fibre reinforced polylactide biocomposites
    2011-03, Elsevier
    In this work, mechanical properties of chemically treated random short fibre and aligned long hemp fibre reinforced PLA composites were investigated over a range of fibre content (0–40 wt.%). It was found that tensile strength, Young’s modulus and impact strength of short hemp fibre reinforced PLA composites increased with increased fibre content. Alkali and silane fibre treatments were found to improve tensile and impact properties which appears to be due to good fibre/matrix adhesion and increased matrix crystallinity. A 30 wt.% alkali treated fibre reinforced PLA composite (PLA/ALK) with a tensile strength of 75.5 MPa, Young’s modulus of 8.18 GPa and impact strength of 2.64 kJ/m2 was found to be the best. However, plane-strain fracture toughness and strain energy release rate decreased with increased fibre content. The mechanical properties of the PLA/ALK composites were increased further due to alignment of long fibres.
  • Item type:Publication,
    Effect of spark plasma sintering temperature on microstructure and mechanical properties of an ultrafine grained TiAl intermetallic alloy
    2009, Elsevier
    The effect of spark plasma sintering (SPS) temperature on the microstructure and mechanical properties of a bulk solid ultrafine grained gamma TiAl alloy produced by SPS of an ultrafine structured Ti/Al composite powder with a nominal composition of Ti–47 at.%Al has been investigated. The Ti/Al composite powder was produced using high energy mechanical milling. It was found that an SPS temperature of 800 °C led to the completion of the reactions needed for reaching the phase equilibrium and formation of a nanostructure with grain sizes in the range of 50–100 nm. However, this SPS temperature was not sufficient to achieve a nearly full density of the compact or a high level of interparticle bonding. Increasing the SPS temperature from 800 to 900 °C caused a significant increase of the density and the level of interparticle bonding while still maintaining grain sizes of <500 nm. The bulk TiAl alloy produced under this condition had a good compression yield strength, fracture strength, bending strength and plastic strain to fracture of 1722, 1963, 610 MPa and 4%, respectively. Increasing the SPS temperature from 900 to 1100 °C caused significant coarsening of the TiAl grains which led to a clear decrease in yield strength and hardness and a slight increase in ductility.