University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
5 results
Search Results
Item type:Publication, Preparation and characterisation of decoloured Novatein and modified PLA blends2017Modified Poly (lactic acid) (PLA) was blended with Decoloured Novatein® (DNTP), a thermoplastic protein material using reactive extrusion to produce a degradable material with improved properties compared to neat Decoloured Novatein®. PLA was modified through free radical grafting of itaconic anhydride to create reactive side-chain groups. Varying ratios of DNTP/ PLA-g-IA or PLA were prepared. Blending DNTP with PLA was found to increase tensile strength between 22% to 538% and modulus between 201 GPa to 3193 GPa, whereas the strain at break decreased between 80% to 94% depending on the blend ratio. The glass transition temperature of the blends which was measured as the tan δ peak, also revealed an increase when compared to neat DNTP. Scanning electron microscope revealed an enhanced interfacial adhesion between the two phases in the blends with PLA-g-IA suggesting a more homogenous microstructure. WAXS result revealed an insignificant decrease in the crystallinity of the blends compared to neat DNTP, indicating that blending with PLA had no structural effect on DNTP. The results show the possibility and feasibility of blending DNTP with PLA for use in agricultural and packaging applications.Item type:Publication, Effect of oxidative treatment on the secondary structure of decoloured bloodmeal2014Bloodmeal can be decoloured using peracetic acid resulting in a material with a pale-yellow colour which only needs sodium dodecyl sulphate, water and triethylene glycol to extrude into a semi-transparent bioplastic. Fourier-transform infrared (FTIR) spectroscopy using Synchrotron light was used to investigate the effect of peracetic acid treatment at various concentrations on the spatial distribution of secondary structures within particles of bloodmeal. Oxidation caused aggregation of helical structures into sheets and acetic acid suppressed sheet formation. Decolouring with peracetic acid led to particles with a higher degree of disorder at the outer edges and higher proportions of ordered structures at the core, consistent with the expected diffusion controlled heterogeneous phase decolouring reaction. The degradation of stabilizing intra- and intermolecular interactions and the presence of acetate ions results in increased chain mobility and greater amorphous content in the material, as evidenced by reduction in Tg and greater enthalpy of relaxation with increasing PAA concentration.Item type:Publication, Plasticization of Bloodmeal-based Thermoplastics2013, CHEMECA 2013Water is the most common plasticizer for proteinbased thermoplastics, lowering the softening point to a allow processing without excessive degradation. The biggest drawback of using water a plasticizer is that water easily evaporates from the material during use or storage. This leads to embrittlement and loss of functionality over time. In this study a series of high molecular mass plasticizers were evaluated for their efficiency in plasticizing bloodmeal-based thermoplastics. It was found that propylene glycol, di and tri-ethylene glycol were most efficient in increasing the material’s ductility, as measured by elongation at break. Using 10 parts plasticizer per hundred bloodmeal (pphBM) in combination with 10 pphBM urea gave optimal results in terms of Young’s modulus, tensile strength and processability. The mechanical properties of plasticized samples showed a stronger dependency on moisture content, compared to unplasticized samples and reached higher equilibrium moisture content in a shorter time. Using 10 pphBM TEG as plasticizer in resulted in a plastic material with a Young’s modulus of 869 MPa, tensile strength of 14.7 MPa and an elongation at break of 46%.Item type:Publication, Time dependent properties of thermoplastic protein produced from bloodmeal with sodium sulphite as an anti-crosslinking agent2012, Engineers AustraliaThe aim of this research was to investigate how the time dependent mechanical behaviour of bloodmeal-based thermoplastic was affected by varying sodium sulphite content at two injection moulding temperatures (120°C at exit or 140°C at exit). Thermoplastic protein was prepared by extrusion with 2, 3 or 4g sodium sulphite (SS), 3g sodium dodecyl sulphate, 10 g urea, 20 g triethylene glycol and 40 g water per 100 g bloodmeal, then injection moulded into test specimens. Pull to break, creep and stress relaxation tests were performed on conditioned samples and glass transition temperature (Tg) was determined by dynamic mechanical analysis. Ultimate tensile strength was 7.9, 7.6 and 5.6 MPa for samples moulded at 120°C and 7.6, 6.3 and 5.7 MPa when moulded at 140°C with 2, 3 and 4 g SS respectively. Experimental creep data was modelled with a 4 element model, consisting of a spring and dashpot in parallel, in series with an additional spring and dashpot. Plotting creep compliance versus time showed increasing chain mobility as SS content increased. Relaxation was modelled with the Struik equation for short-time experiments. Relaxation times were 530, 360 and 250 s with 2, 3 and 4 g SS respectively when moulded at the lower temperature. At 140°C, relaxation times were 440, 430 and 190 s for these SS contents. Tg was in the range 57-65°C (1 Hz peak in tanδ) for all samples, but was lowest for samples with 4 g SS. These results show that both increased sodium sulphite and the higher moulding temperature increased chain mobility in the processed plastic.Item type:Publication, Structural characterisation of pre-processed thermoplastic protein derived from bloodmeal2012, Engineers AustraliaAdditives are required to convert bloodmeal powder into an extrudable thermoplastic protein-based bioplastic. These include a protein denaturant, a surfactant, a reducing agent and plasticisers. The objective of this work was to assess the structural changes induced in bloodmeal by these additives prior to extrusion. Structure was investigated using Fourier transform infrared (FT-IR) spectroscopy, wide angle X-ray scattering (WAXS) and synchrotron light based FT-IR microspectroscopy. FT-IR results suggested the additives reduced α-helical content. The shape of the amide I region (1600 – 1700 cm⁻¹, representing carbonyl group stretching in the protein backbone) is known to depend on protein secondary structures. Bloodmeal showed a broad, convoluted peak in this region, with a maximum in the range 1648 – 1658 cm⁻¹, associated with α-helices. With processing additives, a dip was seen in the α-helix region, with twin peaks emerging either side of it. Urea, one of the additives, also absorbs in the amide I region and may also contribute to a change in its shape. Analysis of the amide 3 region supported a reduction in the ratio of α helices to β sheets. Further support of structural changes was shown by WAXS. The additives decreased the sharpness of peaks corresponding to 4.8 Å and 10 Å, thought to represent intra-helix spacing and inter-helix packing respectively. FT-IR microspectroscopy at the Australian Synchrotron enabled spatial variations in secondary structure to be explored using peaks in the amide 3 region. Spatial distribution of secondary structure was detected in bloodmeal and thermoplastically modified bloodmeal prior to extrusion (PPM-TEG). Bloodmeal showed domain separation on the approximate order of 10 μm, whilst PPM-TEG appeared to have larger phases and overall reduced α-helical content, relative to beta sheets.