    Microstructure and mechanical properties of large size as-cast Ti-43Al-9V-0.2Y (at.%) alloy ingot from brim to centre
    2011, Elsevier
    A Ti-43Al-9V-0.2Y (at.%) alloy ingot with the size of Ф160×400mm was prepared by vacuum arc remelting (VAR). The microstructure of the as-cast Ti-43Al-9V-0.2Y alloy was composed of B2/α₂/γ lamellar colonies and massive B2 and γ phases which were distributed along the boundaries of these lamellar colonies in the form of equiaxed grains. Based on the grain size variation along the radius direction of the ingot, the ingot could be divided into four ring regions from brim to centre. It has been understood that the grain size variation between these four regions was due to the interplay of the effects of the cooling rate and the yttrium content on solidified microstructures in these regions. Mechanical testing of the samples cut from these four regions showed that there existed a clear correlation between the yield strength and the average grain sizes of the four ring regions, which approximately conformed to a Hall-Petch relationship.
  • Item type:Publication,
    Interfacial microstructure and shear strength of Ti-6Al-4V/TiAl laminate composite sheet fabricated by hot packed rolling
    2011, Elsevier
    A two layer Ti-6Al-4V(wt%)/Ti-43Al-9V-Y(at%) laminate composite sheet with a uniform interfacial microstructure and no discernible defects at the interfaces has been prepared by hot-pack rolling, and its interfacial microstructure and shear strength were characterized. Characterization of the interfacial microstructure shows that there was an interfacial region of uniform thickness of about 250 μm which consisted of two layers: Layer I on the TiAl side which was 80 μm thick and Layer II on the Ti-6Al-4V side which was 170 μm thick. The microstructure of Layer I consisted of massive γ phases, needlelike γ phases and B2 phase matrix, while the microstructure of Layer II consisted of α₂ phase. The microstructure of the interfacial region is the result of the interdiffusion of Ti element from Ti-6Al-4V alloy layer into the TiAl alloy layer and Al element from the TiAl alloy layer into the Ti-6Al-4V alloy layer. The shear strength measurement demonstrated that the bonding strength between the TiAl alloy and Ti-6Al-4V alloy layers in the laminate composite sheet was very high. This means that the quality of the interfacial bonding between the two layers achieved by the multi-path rolling is high, and the interface between the layers is very effective in transferring loading, causing significantly improved toughness and plasticity of the TiAl/Ti-6Al-4V laminate composite sheet.