University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
10 results
Search Results
Item type:Publication, Heat treatment, impact properties, and fracture behaviour of Ti-6Al-4V alloy produced by powder compact extrusion.2019, MDPIThe mechanical properties of titanium and titanium alloys are very sensitive to processing, microstructure, and impurity levels. In this paper, a blended powder mixture of Ti-6Al-4V alloy was consolidated by powder compact extrusion that involved warm compaction, vacuum sintering, and hot extrusion. The as-processed material with an oxygen content of 0.34 wt.% was subjected to various annealing treatments. The impact toughness of heat-treated material was determined using Charpy V-notch impact testing at room temperature. An emphasis was placed on establishing a relationship among fracture behaviour, microstructure, and the resulting properties of tested material. From the results, it is apparent that the highest impact toughness value of 19.3 J was achieved after α/β annealing and is comparable with typical values given in the literature for wrought Ti-6Al-4V. In terms of fracture behaviour, it is quite apparent that the crack propagation behaviour of powder-produced material is rather complex compared with the limited amount of data reported for ingot counterparts.Item type:Publication, On microstructural evolution and mechanical properties of Ti-5Al-5V-5Mo-3Cr alloy synthesised from elemental powder mixtures2018, ElsevierIn this paper, we explored to prepare a multi-compositional titanium alloy, Ti-5Al-5V-5Mo-3Cr (Ti-5553), by powder compact extrusion from elemental powder mixtures, and investigate the microstructure variation during the synthesising process and after post heat treatments and the changes of mechanical properties. XRD, OM and SEM were used to analyse the phase constitutions and microstructures of the Ti-5553 alloy at different processing conditions, and tensile tests were conducted to examine their mechanical properties. The results showed that a homogeneous Ti-5553 alloy was successfully produced by powder compact extrusion from the powder mixtures, β phase was mainly contained in the hot-pressed and 1200°C-extruded Ti-5553 alloy and had an equiaxed microstructure. Different types of α phase precipitated from the β matrix after heat treatment, and this significantly changed the microstructures and improved the mechanical properties of the extruded Ti-5553 alloy, with yield strength of 1250 MPa and ultimate strength of 1300 MPa for the alloy treated at 675 °C for 2 h, and the ductility of about 6.1% for the alloy treated at 780 °C for 2 h.Item type:Publication, Evaluation of reactive induction sintering as a manufacturing route for blended elemental Ti-5Al-2.5Fe alloy2018, ElsevierThis work focuses on gaining a better understanding of the feasibility of using reactive induction sintering to obtain the alloy Ti-5Al-2.5Fe using Ti, Al and Fe powders (i.e. via a blended elemental approach). For this, powder compacts were induction sintered under various temperature/time combinations like 700–1250 °C and isothermal holding of 0–15 min. Compositional homogeneity, microstructure evolution and mechanical properties of the sintered Ti-5Al-2.5Fe alloy were investigated. It was found that by increasing the sintering temperature and isothermal holding time, sintered Ti-5Al-2.5Fe components with a homogeneous chemical composition and a Widmanstätten microstructure can be produced. The tensile strength increases with the sintering temperature/time reaching comparable values to the wrought alloy; however the residual porosity has a significant impact on the ductility of the alloy. This study demonstrates that reactive induction sintering is suitable to shorten the production route of blended elemental Ti alloys to be used in non-critical applications where ductility is not the main requirement.Item type:Publication, Processing, microstructure and high strain rate behaviour of Ti-6Al-4V Alloy produced from a blended mixture using powder compact extrusion2016, Trans Tech PublicationsPowder compact extrusion (PCE) is an innovative way of processing titanium and titanium alloys to produce good-quality material with a wide range of compositions, microstructures and mechanical properties. This paper explores PCE processing of Ti-6Al-4V alloy prepared from a blended powder mixture, containing elemental hydride-dehydride (HDH) titanium powder and master alloy (60Al-40V) powder. The warm pressed compacts of blended powders were sintered using a vacuum sintering furnace prior to β extrusion. The resulting material was used to measure the performance under high strain rate and tri-axial stress state using Charpy v-notch testing. A comparison was made of the microstructure after vacuum sintering and hot extrusion in addition to oxygen measurements to determine the degree of oxygen pickup during each processing stage. A comprehensive study of fracture surfaces in selected samples was carried out using optical microscopy and scanning electron microscopy. Based on the results, it is clear that certain samples picked up varying amounts of interstitial impurities during processing and as a consequence a significant number of micro-cracks were observed in lamellar type microstructures. The oxygen content of all as-extruded samples was between 0.34-0.44 wt.% with resultant impact toughness in the range of 10-14 J. The best impact toughness attained for the lowest oxygen as-extruded rods was 20% lower than the literature values for wrought material. In terms of fracture behaviour, ductile dimples, cleavage facets and cracks passing through lamellar structures were observed in all samples. However, the quantity of these fracture features varied significantly in each sample.Item type:Publication, Development of low cost PM Ti alloys by thermomechanical processing of powder blends2016, Trans Tech PublicationsThis research focuses on the development of low cost powder metallurgy (PM) Ti alloys suitable for application in PM thermomechanical processing with mechanical properties comparable to those of wrought Ti6Al4V alloy. The alloy systems studied are Ti3Al2V, Ti5Fe and Ti3.2Fe1Cr0.6Ni0.1Mo (Ti5SS). The alloy mixtures were produced by blending Ti HDH powders with Al40V, 316SS master alloy powders or elemental Fe powder. The blended powders were further consolidated using various methods: high vacuum sintering (HVS), induction sintering (IS), powder compact forging (PCF) and powder compact extrusion (PCE). It is found that, PM Ti3Al2V and Ti5Fe alloy processed by PCE or PCF followed by recrystallization annealing (RA) achieved tensile properties comparable with wrought Ti6Al4V alloy. Tensile properties such as yield strength (YS) of 910MPa, UTS of 1010MPa and 15% elongation to fracture for Ti3Al2V alloy are reported. Ti5Fe alloy gives YS and UTS of 870MPa and 968MPa respectively, combined with 20.3% elongation to fracture. The tensile results are related to the microstructure developed during the consolidation processes. The oxygen contamination as a result of the high temperature processing is also reported.Item type:Publication, Development and design of binder systems for titanium metal injection molding: An overview2013, ASM InternationalTitanium metal injection molding (Ti-MIM) has been practiced since the late 1980s. Logically, the Ti-MIM practice follows the similar processes developed for the antecedent materials such as stainless steel and ceramics. Although Ti-MIM is a favorite research topic today, the issue of convincing the designers to use Ti injection-molded parts still exists. This is mainly because of the concern about contamination which seems unavoidable during the Ti-MIM process. Much information about the binder formulation, powder requirements, debinding, and sintering is available in the literature. There are several powder vendors and feedstock suppliers. However, most of the binders in the feedstock are proprietarily protected. The disclosed information on the binders used for formulating powder feedstock is very limited, which in turn discourages their adoption by engineering designers. This overview intends to discuss some of major binder systems for Ti-MIM available in the literature. It serves to provide a guideline for the Ti-MIM practitioners to choose a suitable powder feedstock.Item type:Publication, The mechanical behaviour of an ultrafine grained Ti-47Al-2Cr (at%) alloy in tension and compression and at different temperatures2011, ElsevierA bulk ultrafine grained (UFG) Ti-47Al-2Cr (at%) alloy has been produced using a powder metallurgy process that combines high energy mechanical milling (HEMM) of a mixture of Ti, Al and Cr powders to produce a Ti/Al/Cr composite powder and hot isostatic pressing (HIP) of the composite powder compact. The purpose of the present study is to determine the mechanical behaviour of the alloy in tension and compression at room temperature (RT) and elevated temperatures, and also to compare the compression behaviour of the material with its tensile behaviour. It has been found that due to the residual pores, lack of full level interparticle bonding and high oxygen content (0.87wt%) in the consolidated samples, the UFG TiAl based alloy has a very low room temperature tensile fracture strength of 100 MPa and shows no tensile ductility. However these microstructural defects and high oxygen content have much less significant effect on the room temperature compressive mechanical properties, and the alloy shows a high compressive yield strength of 1410 MPa, and some ductility (plastic strain to fracture 4%). At elevated temperatures of 800oC and above, the alloy shows high tensile and compressive ductility as demonstrated by 75% tensile elongation to fracture and no cracking in upset forging with a height reduction of 50% at 900oC. The yield strength of the alloy at 900oC is 55 MPa in tension and 33 MPa in compression, both of which are lower than those of coarse grained TiAl based alloys with similar compositions at 900oC. This is due to a higher creep rate of the UFG alloy caused by the small grains. The good formability of the UFG TiAl based alloy as reflected by the lower critical temperature above which the alloy becomes highly formable indicates that the material can be used as a suitable precursor for secondary thermomechanical processing and super-plastic forming.Item type:Publication, Tribological properties of thermally sprayed TiAl-Al₂O₃ composite coating2009, IOP PublishingThe use of thermal spray coatings provides protection to the surfaces operating in severe environments. The main goal of the current work is to investigate the possibility of using a high velocity oxy fuel (HVOF) thermally sprayed wear resistant TiAl/Al2O3 coating on tool steel (H13) which is used for making dies for aluminium high pressure die casting. A feedstock of TiAl/Al2O3 composite powder was produced from a mixture of Al and TiO2 powders by high energy mechanical milling, followed by a thermal reaction process. The feedstock was then thermally sprayed using a high velocity oxy-fuel (HVOF) technique onto H13 steel substrates to produce a composite coating. The present study describes and compares the tribological properties such as friction and sliding wear rate of the coating both at room and high temperature (700°C). The results showed that the composite coating has lower wear rate at high temperature (700°C) than the uncoated H13 sample. At Room temperature without using lubricant there is no much significant difference between the wear rate of the coated and uncoated samples. The experimental results showed that the composite coating has great potential for high temperature application due to its lower wear rate at high temperature in comparison with the uncoated sample at the same temperature. The composite coating was characterized using scanning electron microscopy (SEM), optical microscopy and X-ray diffractometry (XRD). This paper reports the experimental observations and discusses the wear resistance performance of the coatings at room and high temperatures.Item type:Publication, Shape and deformation measurement using heterodyne range imaging technology2006-11, NZNDTARange imaging is emerging as a promising alternative technology for applications that require non-contact visual inspection of object deformation and shape. Previously, we presented a solid-state full-field heterodyne range imaging device capable of capturing three-dimensional images with sub-millimetre range resolution. Using a heterodyne indirect time-of-flight configuration, this system simultaneously measures distance (and intensity), for each pixel in a cameras field of view. In this paper we briefly describe our range imaging system, and its principle of operation. By performing measurements on several metal objects, we demonstrate the potential capabilities of this technology for surface profiling and deformation measurement. In addition to verifying system performance, the reported examples highlight some important system limitations. With these in mind we subsequently discuss the further developments required to enable the use of this device as a robust and practical tool in non-destructive testing and measurement applications.Item type:Publication, Transient liquid phase sintering of high density Transient liquid phase sintering of high density Fe₃Al using Fe and Fe₂Al₅/FeAl₂ powders Part 1: Experimentation and results2003-03, Maney PublishingHigh density Fe[sub 3]Al was produced through transient liquid phase sintering, using rapid heating rates of greater than 150 K min[sup -1] and a mixture of prealloyed and elemental powders. Prealloyed Fe[sub 2]Al[sub 5]/FeAl[sub 2] (50Fe/50Al, wt-%) powder was added to elemental iron powder in a ratio appropriate for producing an overall Fe[sub 3]Al (13•87 wt-%) ratio. The heating rate, sintering time, sintering temperature, green density and powder particle size were controlled during the study. Heating rate, sintering time and powder particle size had the most significant influence upon the sintered density of the compacts. The highest sintered density of 6•12 Mg m[sup -3] (92% of the theoretical density for Fe3Al) was achieved after 15 minutes of sintering at 1350°C, using a 250 K min[sup - 1] heating rate, 1-6 μm Fe powders and 5•66 μm alloy powders. SEM microscopy suggests that agglomerated Fe[sub 2]Al[sub 5]/ FeAl[sub 2] particles, which form a liquid during sintering, are responsible for a significant portion of the remaining porosity in high sintered density compacts, creating stable pores, larger than 100 μm diameter, after melting. High density was achieved by minimising the Kirkendall porosity formed during heating by unbalanced diffusion and solubility between the iron and Fe[sub 2]Al[sub 5]/FeAl[sub 2] components. The lower diffusion rate of aluminium in the prealloyed powder into the iron compared with elemental aluminium in iron, coupled with a fast heating rate, is expected to permit minimal iron-aluminium interdiffusion during heating so that when a liquid forms the aluminium dissolves in the iron to promote solidification at a lower aluminium content. This leads to a further reduction in porosity.