University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, Effects of Gas Nitriding on Fatigue and Crack Initiation of Ti6Al4V produced by Selective Laser Melting2019, Universidade Federal de São Carlos, Departamento de Engenharia de MateriaisSelective laser melting (SLM) is an additive manufacturing technique which permits fabrication of three dimensional parts by selectively melting consecutive layers of metallic powder. This allows the production of parts with high geometrical complexity. Titanium alloy Ti-6Al-4V (Ti64) is widely used in industry due to its high strength-to-mass ratio, corrosion resistance and biocompatibility. SLM increases the application range of Ti64 because of its flexibility for prototyping any part and its low material waste. Nitriding is a diffusion-based thermo-chemical treatment for interstitial hardening of the surface of Ti64 alloy products. This study characterized the fatigue behaviour of SLM-produced Ti64 nitrided and annealed bars in as-built and machined surface conditions. The surface of the SLM-produced Ti64 parts after gas nitriding showed high values of micro-hardness up to 550 HV just below the surface. Fatigue testing was performed to assess the materials fatigue strength and fractographic imaging was used to examine fracture surface and nitride layer characteristics. Nitriding was found to reduce the fatigue strength of the samples to a similar level irrespective of being in the as-built or machined condition. The effect of nitriding on crack initiation and growth at various stress levels under fatigue loading was investigated.Item type:Publication, Additive manufacturing of Ti-6Al-4V with added boron: Microstructure and hardness modification2018, Trans Tech PublicationsTitanium alloy composites with titanium boride (TiB) discontinuous reinforcement have shown improved performance in terms of strength, stiffness, and hardness. Producing this composite through selective laser melting (SLM) can combine the advantages of freeform design with the ability to produce TiB reinforcement in-situ. In this study, SLM was used to consolidate a pre-alloyed Ti-6Al-4V (Ti64) and amorphous boron (B) powder mixture with the intent of producing 1.5wt% TiB reinforcement in a Ti64 matrix. The processing parameters of laser power and scanning speed were investigated for their effect on the density, microstructures, and hardness of the composite material. The results showed that the boron and Ti64 composite could achieve a density greater than 99.4%. Furthermore, it was found that processing parameters changed the microstructural features of the material. The higher the energy density employed the more homogenous the distribution of boron modified material. Macro features were also observed with laser paths being clearly evident in the subsurface microstructure. Micro-hardness testing and density measurement also showed a corresponding increase with increasing energy density. Maximum hardness of 392.4HV was achieved in the composite compared to 354.2HV in SLM fabricated Ti64.Item type:Publication, Effect of processing condition and composition on the microhardness of Cu-(2.5-10)vol.%Al₂O₃ nanocomposite powder particles produced by high energy mechanical milling2010, World ScientificNanostructured Cu-(2.5-10vol.%)Al₂O₃ nanocomposites were produced using high energy mechanical milling. For the as-milled Cu- Al₂O₃ composite powder particles having Al₂O₃ volume fractions of 2.5% and 5%, the increase in average microhardness is significant with the increase of milling time from 12 hours to 24 hours. With the increase of the content of Al₂O₃ nanoparticles the microhardness increases and in the range of 255HV-270HV. The milled nanocomposite powders were heat treated at 150, 300, 400 and 500°C for 1 hour, respectively, to determine the thermal stability of the powder particles as a function of annealing temperature. The average microhardness increased/decreased for the Cu- Al₂O₃ composites after annealing at 150°C due to the dislocation density, while increasing the annealing temperature to 300°C and 400°C the average microhardness almost remained mostly unchanged. Further increasing the annealing temperature to 500°C causes significant decrease in average microhardness due to reduction in dislocation density and coarsening of Cu grains of the Cu- Al₂O₃ composite powders produced after 24 hours of milling. This paper is to report and discuss the changes of the microhardness of the material, caused by the compositions and processing conditions, used to fabricate the Cu-(2.5-10)vol.% Al₂O₃ nanocomposite powders.