University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
5 results
Search Results
Item type:Publication, Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites2019, SpringerIn this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.Item type:Publication, Hemp fibre reinforced poly(lactic acid) composites2007, Trans Tech PublicationsThe potential of hemp fibre as a reinforcing material for Poly(lactic acid) (PLA) was investigated. Good interaction between hemp fibre and PLA resulted in increases of 100% for Young’s modulus and 30% for tensile strength of composites containing 30 wt% fibre. Different predictive ‘rule of mixtures’ models (e.g. Parallel, Series and Hirsch) were assessed regarding the dependence of tensile properties on fibre loading. Limited agreement with models was observed. Differential scanning calorimetry (DSC) and x-ray diffraction (XRD) studies showed that hemp fibre increased the degree of crystallinity in PLA composites.Item type:Publication, Effect of fibre treatments on interfacial shear strength of hemp fibre reinforced polylactide and unsaturated polyester composites2011, ElsevierSurface treatment of hemp fibres was investigated as a means of improving interfacial shear strength (IFSS) of hemp fibre reinforced polylactide (PLA) and unsaturated polyester (UPE) composites. Fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane. A combined treatment using sodium hydroxide and silane was also carried out. IFSS of PLA/hemp fibre samples increased after treatment, except in the case of maleic anhydride treatment. Increased IFSS could be explained by better bonding of PLA with treated fibres and increased PLA transcrystallinity. The highest IFSS was 11.4 MPa which was obtained for the PLA/alkali treated fibre samples. IFSS of UPE/hemp fibre samples increased for all treated fibres. This is believed to be due to the improvement of chemical bonding between the treated fibres and the UPE as supported by FT-IR results. The highest IFSS (20.3 MPa) was found for the combined sodium hydroxide and silane treatment fibre/UPE samples.Item type:Publication, Influence of loading rate, alkali fibre treatment and crystallinity on fracture toughness of random short hemp fibre reinforced polylactide bio-composites2011, ElsevierPlane-strain fracture toughness (KIc) of random short hemp fibre reinforced polylactide (PLA) bio-composites was investigated along with the effect of loading rate, fibre treatment and PLA crystallinity. Fracture toughness testing was carried out at loading rates varying from 0.5 to 20 mm/min using single-edge-notched bending specimens with 0 to 30 wt% fibre. KQ (trial KIc) of composites decreased as loading rate increased, until stabilising to give KIc values at a loading rate of 10 mm/min and higher. The reduction of crazing and stress whitening, as well as a more direct crack path observed in PLA samples combined with reduced plastic deformation observed in composites provided explanation for this reduction. KIc of composites was found to decrease with increased fibre content and fibre treatment with sodium hydroxide. Studies controlling the degree of PLA crystallinity by heat treatment or “annealing” showed that reduction of KIc can be attributed to increased crystallinity.Item type:Publication, Effect of various chemical treatments on the fibre structure and tensile properties of industrial hemp fibres2011, ELSEVIER SCI LTDIndustrial hemp fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane to investigate the influence of treatment on the fibre structure and tensile properties. It was observed that the average tensile strength of sodium hydroxide treated fibres slightly increased compared with that of untreated fibres, which was believed to be as a result of increased cellulose crystallinity. The average tensile strength of acetic anhydride, maleic anhydride, silane and combined sodium hydroxide and silane treated fibres slightly decreased compared with that of untreated fibres, which was believed to be as a result of decreased cellulose crystallinity. However, the average Young’s modulus of all treated fibres increased compared with untreated fibres. This was considered to be as a result of densification of fibre cell walls due to the removal of non-cellulosic components during treatment.