<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 6 of 6
  • Item type:Publication,
    Comparison of strength and Young modulus of aligned discontinuous fibre PLA composites obtained experimentally and from theoretical prediction models
    2019, Elsevier
    The present paper describes work carried out to compare the strength performance of PLA reinforced aligned discontinuous harakeke and hemp fibre mat composites evaluated experimentally and using various simple elastic mathematical prediction models. Fibre mats were produced by means of Dynamic Sheet Former (DSF), and stacked alternately with PLA sheets to produce composites with up to 40 wt% fibre content. The fibre content was increased from 5 wt% to 40 wt% using 5 wt% interval. In this work, both harakeke and hemp composites were manufactured using hot-press. It was found that, better agreement to the experiment was obtained for Young’s modulus compared to those composite strengths. The Modified Rule of Mixtures is found to give accuracy within 41% for strength, while the Cox model showing the best agreement (<10%) for Young’s modulus for fibre contents up to 25 wt%. Better agreement obtained for Young’s modulus is believed to due to less mechanism involved at where Young’s modulus is measured.
  • Item type:Publication,
    Fibre orientation of novel dynamically sheet formed discontinuous natural fibre PLA composites
    2016, Elsevier
    This paper describes work carried out to fabricate and to assess the fibre orientation in PLA reinforced by aligned discontinuous harakeke and hemp fibre mats produced using a dynamic sheet former (DSF). These mats were combined with PLA sheets to make composites with fibre contents of 5–40 wt% using a hot press. It was found that the fibre orientation factors (Kθ) for both harakeke and hemp fibre composites were higher than those values seen in the literature for composites prepared using injection moulding and hot pressed using randomly oriented fibre mats, but slightly lower than the highest values obtained with aligned fibre nonwoven preform composites utilising more processing stages. The highest Kθ values for harakeke and hemp fibres in this work were found to be 0.58 and 0.44 respectively. Kθ decreased, reflecting increased fibre misalignment as fibre content increased, believed to be due to fibre agglomeration and the higher pressure required during processing.
  • Item type:Publication,
    The effect of silane coupling agent on iron sand for use in magnetorheological elastomers Part 1: Surface chemical modification and characterization
    2015-01-01, Elsevier
    Bis-(3-triethoxysilylpropyl) tetrasulphane (TESPT) was employed for surface modification of iron sand for use in magnetorheological elastomers (MREs). The amount of TESPT was varied at five levels (2, 4, 6, 8 and 10 wt%) relative to iron sand content to assess the optimum amount of coupling agent for interfacial bonding and damping performance. Evidence that coupling had occurred between iron sand and TESPT was identified by Raman Spectroscopy and the grafting percentage was determined by thermogravimetric analysis. Subsequently, isotropic MREs containing unmodified and modified iron sand particles and natural rubber were prepared. Crosslink density assessment by swelling testing provided evidence that the tetrasulphane group of TESPT formed crosslinks with the rubber chains. The results exhibited the advantages of TESPT as a coupling agent between iron sand particles and rubber and also revealed that 6% TESPT content produced the highest crosslink density. The effects of the amount of TESPT on dynamic mechanical properties the morphological characteristics of the MREs were also investigated.
  • Item type:Publication,
    Comparison of dynamic properties of magnetorheological elastomers with existing antivibration rubbers
    2015-12-15, Elsevier
    Tan δ and energy dissipated during hysteresis testing of isotropic and anisotropic MREs containing silane modified iron sand particles in a natural rubber matrix were compared with existing antivibration rubbers. Tan δ was measured using dynamic mechanical analysis (DMA) over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100–50 °C). Energy dissipated was measured using a universal tester under cyclic tensile loading. The chosen antivibration rubbers for comparison contained different contents of carbon black filler (30, 50 and 70 phr) in a natural rubber matrix. It was found that energy absorption for comparative samples was generally higher than isotropic and anisotropic MREs over the range of frequency and strain amplitude explored, as well as in hysteresis testing and this was believed to be largely due the presence of carbon black in the formulation. Further assessment was carried out on materials that were the same as anisotropic MREs except they had additions of carbon black. The energy absorption was found higher than comparative samples with the same carbon black contents, supporting the use of iron sand to improve damping. However, trends for energy absorption at around Tg were found to reverse which is considered to be due to the segmental motion of rubber chains being by far the most significant influence on energy absorption in the glass transition zone.
  • Item type:Publication,
    Mode I and Mode II interlaminar fracture toughness of composite laminates interleaved with electrospun nanofibre veils
    2015-05-01, Elsevier
    In this study, the effects of interleaved nanofibre veils on the Mode I and Mode II interlaminar fracture toughness (ILFT) of autoclave cured unidirectional carbon/epoxy composite laminates were investigated. Various electrospun nanofibre veils consisting of a range of different polymer types, fibre diameters and veil architectures were placed in the laminate mid-planes, which were subsequently subjected to double cantilever beam and end-notch flexure tests. It was found that the polymer type and veil areal weight were the most important factors contributing to laminate performance. A 4.5 g/m2 PA66 veil provided the best all-round performance with fracture toughness improvements of 156% and 69% for Mode I and Mode II, respectively.
  • Item type:Publication,
    Comparison of harakeke with hemp fibre as a potential reinforcement in composites
    2014-12-01, Elsevier
    The objective of this study was to characterize the performance of untreated and chemically treated harakeke fibre (a leaf fibre from a plant native to New Zealand) and compare with hemp fibre to assess its use as potential reinforcement in composites. Alkali treatment is among the most popular treatments used to remove unwanted fibre constituents such as pectin, hemicellulose and waxes; it can enhance fibre properties, fibre separation, interfacial bonding and fibre dispersion within a composite. Physical and mechanical properties of untreated and alkali treated fibres were assessed using single fibre tensile testing, X-ray diffraction (XRD), scanning electron microscopy (SEM) and thermal analysis using thermogravimetric analysis (TGA). Untreated harakeke fibre was found to be lower in tensile strength compared to untreated hemp fibre. It was also found that the tensile strength of harakeke and hemp fibres treated with 5wt% NaOH/2wt% Na2SO3 and 5wt% NaOH was not significantly affected and these fibres had good fibre separation. However, alkali treatment was found to lead to higher crystallinity index (Ic) and better thermal stability for harakeke as well as hemp fibres.