University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
5 results
Search Results
Item type:Publication, Evaluation of reactive induction sintering as a manufacturing route for blended elemental Ti-5Al-2.5Fe alloy2018, ElsevierThis work focuses on gaining a better understanding of the feasibility of using reactive induction sintering to obtain the alloy Ti-5Al-2.5Fe using Ti, Al and Fe powders (i.e. via a blended elemental approach). For this, powder compacts were induction sintered under various temperature/time combinations like 700–1250 °C and isothermal holding of 0–15 min. Compositional homogeneity, microstructure evolution and mechanical properties of the sintered Ti-5Al-2.5Fe alloy were investigated. It was found that by increasing the sintering temperature and isothermal holding time, sintered Ti-5Al-2.5Fe components with a homogeneous chemical composition and a Widmanstätten microstructure can be produced. The tensile strength increases with the sintering temperature/time reaching comparable values to the wrought alloy; however the residual porosity has a significant impact on the ductility of the alloy. This study demonstrates that reactive induction sintering is suitable to shorten the production route of blended elemental Ti alloys to be used in non-critical applications where ductility is not the main requirement.Item type:Publication, Low-Cost α+β PM Ti Alloys by Fe/Ni Addition to Pure Ti2016Ti and its alloys can deliver a very interesting combination of properties such as low density, high strength, corrosion resistance and biocompatibility and, therefore, are very flexible materials which can be adapted to various applications. Nonetheless, Ti and Ti alloys are only employed in critical applications (i.e. aeronautical and aerospace, nautical, medical, etc.) or in products for leisure. In both of these cases the higher fabrication costs of Ti in comparison to its competitors (i.e. steel and aluminium) is not the limiting factor as it is for many structural applications, especially for mass production (i.e. automotive sector). The use of creative techniques and the decrement of the starting price of Ti have been identified as the two main routes to follow to decrease the fabrication costs. In this study, the production of low-cost α+β Ti alloys has been assessed by combining the addition of cheap alloying elements (in particular a Fe/Ni powder) with the classical powder metallurgy route (pressing and sintering). Physical and mechanical properties as well as microstructural analysis of these low-cost alloys were measured and correlated to the processing parameters used to sinter them. It is found that the low-cost Ti alloys show similar behaviour to conventional α+β Ti alloys and, thus, have the potential to be used for non-critical applications.Item type:Publication, Quantifying the properties of low-cost powder metallurgy titanium alloys2017-02The extensive industrial employment of titanium is hindered by its high production costs where reduction of these costs can be achieved using cheap alloying elements and appropriate alternative processing techniques. In this work the feasibility of the production of low-cost titanium alloys is addressed by adding steel to pure titanium and processing the alloys by powder metallurgy. In particular, a spherical 4140 LCH steel powder commonly used in metal injection moulding is blended with irregular hydride-dehydride Ti. The new low-cost alloys are cold uniaxially pressed and sintered under high vacuum and show comparable properties to other wrought-equivalent and powder metallurgy titanium alloys. Differential thermal analysis and X-ray diffraction analyses confirm that Ti can tolerate the employment of iron as primary alloying element without forming detrimental TiFe-based intermetallic phases. Thus, the newly designed α+β alloys could be used for cheaper non-critical components.Item type:Publication, Evaluation of the mechanical properties of powder metallurgy Ti-6Al-7Nb alloy2017-03Titanium and its alloys are common biomedical materials owing to their combination of mechanical properties, corrosion resistance and biocompatibility. Powder metallurgy (PM) techniques can be used to fabricate biomaterials with tailored properties because changing the processing parameters, such as the sintering temperature, products with different level of porosity and mechanical performances can be obtained. This study addresses the production of the biomedical Ti-6Al-7Nb alloy by means of the master alloy addition variant of the PM blending elemental approach. The sintering parameters investigated guarantee that the complete diffusion of the alloying elements and the homogenization of the microstructure is achieved. The sintering of the Ti-6Al-7Nb alloy induces a total shrinkage between 7.4% and 10.7% and the level of porosity decreases from 6.2% to 4.7% with the increment of the sintering temperature. Vickers hardness (280–300 HV30) and tensile properties (different combination of strength and elongation around 900 MPa and 3%) are achieved.Item type:Publication, Modification of sintered titanium alloys by hot isostatic pressing2012, Trans Tech PublicationsPowder metallurgy (PM) permits to obtain titanium alloys with properties and microstructures close to ingot metallurgy products. However, residual porosity is normally present in the products produced by the PM route of powder pressing and sintering (P&S)\, and this needs to be reduced by using post-sintering process step such as hot isostatic pressing (HIP) and forging. In this study, the microstructural and mechanical property changes caused by HIP of samples of two alloys, near-α Ti-3Al-2.5V alloy and α+β Ti-6Al-4V, produced by P&S route were investigated. Two types of powders were utilised: prealloyed powders and blend of elemental titanium powder and master alloy powder. Four conditions defined by HIP temperature, pressure and time were used to HIP the sintered samples with two geometries. The results show that, independent of the HIP conditions used, HIP increased the relative density of the samples to approximately 97.5% and their hardness by 30-50 HV depending on the HIP condition. However, HIP at 1000°C changes the fracture mode of the sintered samples from ductile to brittle.