University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
4 results
Search Results
Item type:Publication, Strengthening mechanisms of Ti via Al addition2020, ElsevierPure Ti is characterised by an interesting combination of performance from an engineering point of view. The addition of Al to Ti can be used to reduce the intrinsic cost of the material, decrease the density of the alloy, and increase the mechanical performance. This study is focused on evaluating the physical properties, microstructural evolution and mechanical behaviour of Ti-xAl alloys (where x = 1–6 wt%) in order to scientifically understand the strengthening mechanisms of the addition of Al to pure Ti manufactured via the conventional powder metallurgy route of cold uniaxial pressing plus solid state sintering. The addition of Al to Ti does not affect the compressibility of the alloy but changes the consolidation and densification of the alloy. The incremental addition of Al results in the progressive strengthening of Ti via the simultaneous contribution from substitutional solid solution and grain refinement strengthening which outdo the negative effect of the residual porosity.Item type:Publication, Effect of Mn on the Properties of Powder Metallurgy Ti-2.5Al-xMn Alloys.2023-07-10, MDPITitanium alloys are the ideal material for a wide range of structural applications, but their high cost compared to other metals hinders their adoption. Powder metallurgy and cheap alloying elements can be used to create new Ti alloys. In this study, the simultaneous addition of Al and Mn is considered to manufacture and characterise ternary Ti-2.5Al-Mn alloys obtained via pressing and sintering by varying the Mn content (1-10 wt.%). It is found that the addition of the alloying elements reduces compressibility. Consequently, the amount of porosity increases (8.5 → 10.8%) with the amount of Mn as the alloys were processed under the same conditions. The progressive addition of Mn refines the classical lamellar microstructure and, eventually, transforms it into an equiaxed β-grain structure with acicular α grains. The microstructural changes lead to continuous increases in strength (ultimate tensile strength: 694 → 851 MPa) and hardness (225 → 325 HV30) with an associated loss of ductility (elongation to failure: 13.9 → 1.0%). However, the obtained ternary Ti-2.5Al-Mn alloys have similar or better overall mechanical behaviour than most of the binary Ti-Mn alloys obtained through a variety of manufacturing methods.Item type:Publication, Antibacterial Ti-Mn-Cu alloys for biomedical applications2020, Oxford University Press (OUP)Titanium alloys are common biomedical materials due to their biocompatibility and mechanical performance. However, titanium alloys are expensive and, unless surface treated, generally cannot prevent surgical infections related to bacteria which can damage the integrity of the implant. In this study, new titanium alloys were developed via powder metallurgy and the addition of manganese and copper, respectively, aiming to limit the manufacturing costs and induce new functionality on the materials including antibacterial response. The addition of manganese and copper to titanium significantly changes the behaviour of the Ti-Mn-Cu alloys leading to the successful stabilization of the beta titanium phase, great refinement of the typical lamellar structure, and achievement of materials with low level of porosity. Consequently, it is found that the mechanical performance and the antibacterial efficacy are enhanced by the addition of a higher amount of alloying elements. The manufactured Ti-Mn-Cu alloys fulfil the requirements for structural biomedical implants and have antibacterial response making them potential candidates for permanent medical implants.Item type:Publication, Biomedical Ti-Cu-Mn alloys with antibacterial capability2021, ElsevierThis study aims to develop Ti–Cu–Mn alloys with antibacterial capability for reducing the possibility of bacterial infection during biomedical implant surgeries. Ternary alloys were designed to be manufactured via powder metallurgy, which has intrinsic manufacturing, economic, and environmental benefits. The amount of each of the alloying elements was limited to prevent the formation of brittle phases. It is found that the selected compositions of Cu (0.5-5 wt.%) plus Mn (0.25-2.5 Mn wt.%) can successfully be manufactured achieving microstructures, tensile properties and antibacterial capability performance comparable to those of other biomedical Ti alloys. Specifically, homogeneous compositions are achieved with the selected sintering parameters (1300 °C/120 min). The strength and hardness of the material increase proportionally with the addition rate of Cu and Mn, and antibacterial capability values were found to be above the 90% threshold required for antibacterial certification.