<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 2 of 2
  • Item type:Publication,
    Sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites
    2006, Elsevier
    The sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites produced using Al/TiO₂ composite powders have been studied. Ti(Al,O), Ti₃Al(O) and TiAl(O) represent α-Ti phase with dissolved Al and O, and Ti3Al and TiAl phases with dissolved O, respectively. The Al/TiO₂ composite powders were produced by high energy mechanical milling using Al and TiO₂ powders as the starting materials. It was found that the matrices of the composites became fully dense after sintering at 1550 °C, and the Al₂O₃ particles became fully sintered when the sintering temperature was increased to 1650 °C. The reactions between Al and TiO₂ which occur during heating the powder compacts to 1400 °C have little effect on the sintering of the composite powders. The Al₂O₃ particles in the composites become significantly coarsened during sintering at 1550 °C or above, and the coarsening rate of the Al₂O₃ particles increases in the order of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl/Al₂O₃ composites. This can be attributed to the decrease of the solidus temperature or melting points of the corresponding matrices. It is evident that in the initial stage of sintering, coarsening of the Al2O₃ particles occurs through coalescence. Hipping of the pre-sintered composites at 1300 °C with a pressure of 200 MPa without canning causes significant increase of the density and substantial further coarsening of the Al₂O₃ particles.
  • Item type:Publication,
    Synthesis, Microstructure, and Mechanical Properties of a Novel Ti₂AlC/TiC/Al₂O₃In Situ Composite
    2006, Wiley-Blackwell Publishing, Inc.
    This paper describes a novel process for synthesizing a Ti₂AlC/TiC/Al₂O₃in situ composite. This route utilizes TiO₂, carbon, and Al powders as raw materials, and involves high-energy mechanical milling and powder sintering. The Ti₂AlC/TiC/Al₂O₃ bulk in situ composite produced has a phase composition of Ti₂AlC–20 vol% TiC–35 vol% Al₂O₃ with fine Al₂O₃ particles (size: 0.5–15 μm) embedded in a Ti₂AlC/TiC matrix. The Ti₂AlC grains exhibit a nanometer scale lamellar structure, and most of the Al₂O₃ grains contain fine cubic TiOmC1−m precipitates (size: 10–200 nm). The average hardness and bending strength of the composite are in the ranges of 11–12.5 GPa and 380–440 MPa, respectively. Here we have demonstrated that the mechanical performance (mainly hardness and bending strength) of the composite is directly correlated with the size of the Al2O3 particles present in the as-fabricated in situ composite.