<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 10 of 20
  • Item type:Publication,
    Analysis of rheological behaviour of titanium feedstocks formulated with a water-soluble binder system for powder injection moulding
    2014-09, Elsevier
    Binder selection and formulation are critical in powder injection moulding. Binders play a key role in controlling the rheological properties of a feedstock and influence whether the resulting feedstock can be successfully injection moulded, debound and sintered without defects. A four-step process was used to mix hydride-dehydride titanium alloy (processed) powder (Ti-6Al-4 V) with a polyethylene glycol (PEG) based water soluble binder system. The rheological properties, including flow behaviour index, flow activation energy, fluidity and melt flow index of the homogeneous feedstock, were determined with a capillary rheometer. All feedstock formulations exhibited shear thinning flow behaviour. The optimum feedstock consisting of 60 vol.% powder content, 32 vol.% PEG, 6 vol.% polyvinyl butyryl and 2 vol.% stearic acid was suitable for titanium injection moulding.
  • Item type:Publication,
    Development and design of binder systems for titanium metal injection molding: An overview
    2013, ASM International
    Titanium metal injection molding (Ti-MIM) has been practiced since the late 1980s. Logically, the Ti-MIM practice follows the similar processes developed for the antecedent materials such as stainless steel and ceramics. Although Ti-MIM is a favorite research topic today, the issue of convincing the designers to use Ti injection-molded parts still exists. This is mainly because of the concern about contamination which seems unavoidable during the Ti-MIM process. Much information about the binder formulation, powder requirements, debinding, and sintering is available in the literature. There are several powder vendors and feedstock suppliers. However, most of the binders in the feedstock are proprietarily protected. The disclosed information on the binders used for formulating powder feedstock is very limited, which in turn discourages their adoption by engineering designers. This overview intends to discuss some of major binder systems for Ti-MIM available in the literature. It serves to provide a guideline for the Ti-MIM practitioners to choose a suitable powder feedstock.
  • Item type:Publication,
    Microstructural evolution during mechanical milling of Ti/Al powder mixture and production of intermetallic TiAl cathode target
    2011, Springer
    Titanium aluminides are of great technological interest because of their attractive mechanical properties. Mechanical milling/alloying is a promising powder metallurgical technique, which can achieve ultrafine, uniform and manipulable microstructures. In this study, we employed a recently revisited discus mill to produce a composite Ti– (50–57) at.%Al powder feedstock, which is suitable for hot consolidation to produce bulk cathode targets for physical vapour deposition (PVD) coatings. The effects of milling time, quantity of process control agent (PCA) and discus-topowder weight ratio (DPR) on the microstructure evolution of the attendant Ti/Al composite powder were investigated in detail. It was found that to produce Ti/Al composite powders with a fine particle size and a uniform microstructure, the practicable processing parameters should be 2 or 3% isopropanol addition as PCA, 12 h of milling time and at least 13:1 DPR weight ratio. Cathode targets were produced by hot isostatic pressing (HIPing) the as-milled powders. The targets were then used to produce a PVD TiAlN coating which had an average microhardness of 2400 HV.
  • Item type:Publication,
    Mechanical behaviour of Titanium, Ti-6Al-4V (wt %) alloy and Ti-47Al-2Cr (at %) alloy produced using powder compact forging
    2011, Trans Tech Publications
    Powder compact forging was used to produce bulk consolidated titanium and Ti-6Al-4V (wt %) and Ti-47Al-2Cr (at%) alloy disks from hydrogenated and dehydrogenated (HDH) and gas atomised powders (GA) powders (in the case of titanium and Ti-6Al-4V) and a mechanically milled powder (in the case of Ti-47Al-2Cr alloy). The bulk titanium and Ti-6Al-4V (wt %) alloy have been produced by forging of the powder compacts. The Ti-47Al-2Cr (at %) alloy was produced using canned powder compact forging of a Ti/Al/Cr composite powder. The purpose of the present study is to investigate the deformation and fracture behaviour of the bulk consolidated as-forged materials, by conducting tensile testing at room temperature (RT) and examination of the fractured specimens which had near-α, α + β and γ phase structures, respectively. It was found that as-forged bulk titanium disk produced using HDH powder showed a yield point with a yield strength of ~700 MPa and with a considerable amount of ductility. While the as-forged Ti-6Al-4V (wt %) alloy produced using HDH powder, fractured prematurely without any yielding. On the other hand yielding was observed in the as-forged Ti-6Al-4V (wt %) alloy produced using GA powder, showing a yield strength of ~970 MPa and a considerable amount of plastic strain to fracture. The bulk consolidated Ti-47Al-2Cr (at %) alloy also fractured prematurely with fracture strength of ~125 MPa. The mechanical behaviour of the as-forged bulk materials was found to be dependent on several factors such as initial powders used, green density of the powder compact, forging parameters used during forging. It was expected that the entrapped gas in green compacts, absorbed oxygen, porosity and inter-particle bonding play an important role on the quality of the as-forged material, which in turn affected the mechanical behaviour of the bulk material.
  • Item type:Publication,
    The performance of thermally sprayed titanium based composite coatings in molten aluminium
    2011, Elsevier
    The service life of die and tool steels in contact with molten aluminium is important in the aluminium processing industry. This article describes an investigation of the efficiency of thermally sprayed Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite coatings in resisting aluminium soldering on H13 tool steel. The powder feedstocks for making the composite coatings were produced by high energy mechanical milling of a mixture of Al and TiO₂ powders using different molar ratios followed by a thermal reaction process. The feedstocks were then thermally sprayed using a high velocity oxygen fuel (HVOF) technique onto an H13 steel substrate to produce composite coatings. The performance of the coatings was assessed in terms of Al soldering and liquid metal corrosion resistance after immersing in molten aluminium at a temperature of 700 ± 10 °C. The results of this study showed that composite coatings have a potential to act as a physical barrier to prevent aluminium attack on H13 tool steel. The nature of Al attack on H13 tool steel changed from generalised to more localised attack with the thermally sprayed coating. A Ti(Al,O)/Al₂O₃ composite coating was not attacked by molten aluminium, however localised attack on a H13 tool steel substrate was found to be caused by molten metal penetration through defects in the coating. Composite coating TiAl(O)/Al₂O₃ was attacked by molten aluminium resulting in dissolution of the coating. Composite coatings showed significantly lower dissolution in molten aluminium compared with the uncoated H13 steel. A Ti(Al,O)/Al₂O₃ composite coating was found to be a more effective protective coating than a TiAl(O)/Al₂O₃ composite coating due its greater resistance to molten aluminium attack.
  • Item type:Publication,
    The mechanical behaviour of an ultrafine grained Ti-47Al-2Cr (at%) alloy in tension and compression and at different temperatures
    2011, Elsevier
    A bulk ultrafine grained (UFG) Ti-47Al-2Cr (at%) alloy has been produced using a powder metallurgy process that combines high energy mechanical milling (HEMM) of a mixture of Ti, Al and Cr powders to produce a Ti/Al/Cr composite powder and hot isostatic pressing (HIP) of the composite powder compact. The purpose of the present study is to determine the mechanical behaviour of the alloy in tension and compression at room temperature (RT) and elevated temperatures, and also to compare the compression behaviour of the material with its tensile behaviour. It has been found that due to the residual pores, lack of full level interparticle bonding and high oxygen content (0.87wt%) in the consolidated samples, the UFG TiAl based alloy has a very low room temperature tensile fracture strength of 100 MPa and shows no tensile ductility. However these microstructural defects and high oxygen content have much less significant effect on the room temperature compressive mechanical properties, and the alloy shows a high compressive yield strength of 1410 MPa, and some ductility (plastic strain to fracture 4%). At elevated temperatures of 800oC and above, the alloy shows high tensile and compressive ductility as demonstrated by 75% tensile elongation to fracture and no cracking in upset forging with a height reduction of 50% at 900oC. The yield strength of the alloy at 900oC is 55 MPa in tension and 33 MPa in compression, both of which are lower than those of coarse grained TiAl based alloys with similar compositions at 900oC. This is due to a higher creep rate of the UFG alloy caused by the small grains. The good formability of the UFG TiAl based alloy as reflected by the lower critical temperature above which the alloy becomes highly formable indicates that the material can be used as a suitable precursor for secondary thermomechanical processing and super-plastic forming.
  • Item type:Publication,
    High temperature mechanical properties of Ti-47Al-2Cr (at %) alloy produced using powder compact forging of a mechanically milled powder
    2009, IOP Publishing
    Ultrafine grained (UFG) Ti-47Al-2Cr (at %) alloy was prepared using a combination of high energy ball milling of a mixture of elemental powders to produce a Ti/Al/Cr composite powder and forging of compacts of this composite powder. The microstucture of the powder forged alloy was found to be dependent on the initial condition of the powder. The alloy produced by this method has demonstrated good formability, both in tensile and compression testings at elevated temperatures. A ductility of 80–165% in tension has been observed, while in a compression plastic strain of ~ 50% was found to be easily achievable, without causing cracking. The deformation behaviour of the particular alloy in tension and compression at elevated temperature has been discussed in detail. The results from the present investigation indicate that UFG Ti-47Al-2Cr (at %) alloy produced using powder compact forging has good formability, and is suitable precursor for near-net shaping using thermomechanical processes such as forging and superplastic forming.
  • Item type:Publication,
    Effect of milling parameters on microstructure of Ti/Al composite powder produced by discus milling
    2006, World Scientific Publishing Co
    The motivation of this research is to develop a process for producing Ti/Al composite powders that enable synthesis of a single-phase TiAl intermetallic bulk material, which is then used as a target for physical vapour deposition (PVD) coating. This study reports the effects of milling time, amount of process control agent (PCA) added as well as the powder-to-medium ratio on the microstructure of the Ti/Al composite powder. Optical microscopy and scanning electron microscopy (SEM) were used to evaluate the level of mixing and the resulting powder particle size. X-ray diffraction analysis and differential thermal analysis were used for determining the phase constituents and the solid state reaction temperature of the as-milled powders.
  • Item type:Publication,
    Thermal stability of nanocrystalline copper films
    2006, World Scientific Publishing Co
    The grain growth kinetics of nanocrystalline copper thin film samples was investigated. The grain size of nanocrystalline copper samples was determined from the broadening of X-ray spectra. It was found that the grain size increased linearly with isothermal annealing time within the first 10 minutes, beyond which power-law growth kinetics is applied. The activation energy for grain growth was determined by constructing an Arrhenius plot, which shows an activation energy of about 21 – 30 kJ/mol. The low activation energy is attributed to the second phase particle drag and the porosity drag, which act as the pinning force for grain growth in nanocrystalline copper.
  • Item type:Publication,
    Fabrication of TiAl target by mechanical alloying and applications in physical vapour deposition coating
    2007, Trans Tech Publications Ltd
    The research involves the development of a powder metallurgical route for producing good quality TiAl targets for making physical vapour deposition (PVD) coatings. Mixtures of elemental titanium and aluminium powders were mechanically milled using a novel discus milling technique under various conditions. Hot isostatic pressing (HIP) was then employed for consolidation of the mechanically alloyed powders. A cathodic arc vapour deposition process was applied to produce a TiAIN coating. A microstructural examination was conducted on the target material and PVD coatings, using X-ray diffractometry (XRD), X-ray photoelectron spectrometry (XPS) and scanning electron microscopy (SEM). It has been found that combining mechanical alloying and HIP enable us to produce a fairly good quality of TiAl based target. The PVD coatings obtained from the TiAl target showed very high microhardness values.