    Optimising industrial hemp fibre for composites
    2007, Pergamon
    The optimisation of New Zealand grown hemp fibre for inclusion in composites has been investigated. The optimum growing period was found to be 114 days, producing fibres with an average tensile strength of 857 MPa and a Young’s modulus of 58 GPa. An alkali treatment with 10wt% NaOH solution at a maximum processing temperature of 160o C with a hold time of 45 minutes was found to produce strong fibres with a low lignin content and good fibre separation. Although a good fit with the Weibull distribution function was obtained for single fibre strength, this did not allow for accurate scaling to strengths at different lengths. Alkali treated fibres, polypropylene and a maleated polypropylene (MAPP) coupling agent were compounded in a twin-screw extruder, and injection moulded into composite tensile test specimens. The strongest composite consisted of polypropylene with 40wt% fibre and 3wt% MAPP, and had a tensile strength of 47.2 MPa, and a Young’s modulus of 4.88 GPa.
  • Item type:Publication,
    Influence of hygrothermal ageing on the physico-mechanical properties of alkali treated industrial hemp fibre reinforced polylactic acid composites
    2010, SpringerLink
    30 wt% aligned untreated long hemp fibre/polylactic acid (AUL) and aligned alkali treated long hemp fibre/polylactic acid (AAL) composites were produced by film stacking and subjected to hygrothermal ageing environment along with neat polylactic acid (PLA). Hygrothermal ageing was carried out by immersing samples in distilled water at 25 and 50 ºC over a period of 3 months. It was found that both neat PLA and composites followed Fickian diffusion. Higher temperature generally increased the Diffusion coefficient, D of neat PLA and composites, as well as shortening the saturation time. Neat PLA had the lowest D value followed by AAL composites and then AUL composites. After hygrothermal ageing, tensile and flexural strength, Young’s and flexural modulus and KIc were found to decrease and impact strength was found to increase for both AUL and AAL composites. AUL composites had greater overall reduction in mechanical properties than that for AAL composites after hygrothermal ageing. Crystallinity contents of the hygrothermal aged composites support the results of the deterioration of mechanical properties upon exposure to hygrothermal ageing environment.
  • Item type:Publication,
    Influence of alkali fiber treatment and fiber processing on the mechanical properties of hemp/epoxy composites
    2010-10, Wiley
    Industrial hemp fibers were treated with a 5 wt % NaOH, 2 wt % Na₂SO₃ solution at 120°C for 60 min to remove noncellulosic fiber components. Analysis of fibers by lignin analysis, scanning electron microscopy (SEM), zeta potential, Fourier transform infrared (FTIR) spectroscopy, wide angle X-ray diffraction (WAXRD) and differential thermal/thermogravimetric analysis (DTA/TGA), supported that alkali treatment had (i) removed lignin, (ii) separated fibers from their fiber bundles, (iii) exposed cellulose hydroxyl groups, (iv) made the fiber surface cleaner, and (v) enhanced thermal stability of the fibers by increasing cellulose crystallinity through better packing of cellulose chains. Untreated and alkali treated short (random and aligned) and long (aligned) hemp fiber/epoxy composites were produced with fiber contents between 40 and 65 wt %. Although alkali treatment generally improved composite strength, better strength at high fiber contents for long fiber composites was achieved with untreated fiber, which appeared to be due to less fiber/fiber contact between alkali treated fibers. Composites with 65 wt % untreated, long aligned fiber were the strongest with a tensile strength (TS) of 165 MPa, Young's modulus (YM) of 17 GPa, flexural strength of 180 MPa, flexural modulus of 9 GPa, impact energy (IE) of 14.5 kJ/m², and fracture toughness (KIc) of 5 MPa m1/2
  • Item type:Publication,
    Curing kinetics and effects of fibre surface treatment and curing parameters on the interfacial and tensile properties of hemp/epoxy composites
    2009, Brill
    The curing kinetics of neat epoxy (NE) and hemp fibre/epoxy composites was studied and assessed using two dynamic models (the Kissinger and Flynn-Wall-Ozawa Models) and an isothermal model (the Autocatalytic Model) which was generally supported by the experimental data obtained from dynamic and isothermal differential scanning calorimetry (DSC) scans. The activation energies for the curing of composites exhibited lower values compared to curing of NE which is believed to be due to higher nucleophilic activity of the amine groups of the curing agent in the presence of fibres. The highest tensile strength, σ was obtained with composites produced with an epoxy to curing agent ratio of 1:1 and the highest Young's modulus, E was obtained with an epoxy to curing agent ratio of 1:1.2. Alkali treated hemp fibre/epoxy (ATFE) composites were found to have higher σ and E values compared to those for untreated hemp fibre/epoxy (UTFE) composites which was consistent with the trend for interfacial shear strength (IFSS) values. Composites σ and E were found to be higher for a processing temperature of 70°C than for 25°C for both UTFE and ATFE composites, but were found to decrease as the curing temperature was increased further to 120°C.
  • Item type:Publication,
    Influence of accelerated ageing on the physico-mechanical properties of alkali-treated industrial hemp fibre reinforced poly(lactic acid) (PLA) composites
    2010, Elsevier
    30 wt% aligned untreated long hemp fibre/PLA (AUL) and aligned alkali treated long hemp fibre/PLA (AAL) composites were produced by film stacking and subjected to accelerated ageing. Accelerated ageing was carried out using UV irradiation and water spray at 50 °C for four different time intervals (250, 500, 750 and 1000 h). After accelerated ageing, tensile strength (TS), flexural strength, Young's modulus (YM), flexural modulus and mode I fracture toughness (KIc) were found to decrease and impact strength (IS) was found to increase for both AUL and AAL composites. AUL composites had greatest overall reduction in mechanical properties than that for AAL composites upon exposure to accelerated ageing environment. FTIR analysis and crystallinity contents of the accelerated aged composites support the results of the deterioration of mechanical properties upon exposure to accelerated ageing environment.