University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
4 results
Search Results
Item type:Publication, Evaluation of reactive induction sintering as a manufacturing route for blended elemental Ti-5Al-2.5Fe alloy2018, ElsevierThis work focuses on gaining a better understanding of the feasibility of using reactive induction sintering to obtain the alloy Ti-5Al-2.5Fe using Ti, Al and Fe powders (i.e. via a blended elemental approach). For this, powder compacts were induction sintered under various temperature/time combinations like 700–1250 °C and isothermal holding of 0–15 min. Compositional homogeneity, microstructure evolution and mechanical properties of the sintered Ti-5Al-2.5Fe alloy were investigated. It was found that by increasing the sintering temperature and isothermal holding time, sintered Ti-5Al-2.5Fe components with a homogeneous chemical composition and a Widmanstätten microstructure can be produced. The tensile strength increases with the sintering temperature/time reaching comparable values to the wrought alloy; however the residual porosity has a significant impact on the ductility of the alloy. This study demonstrates that reactive induction sintering is suitable to shorten the production route of blended elemental Ti alloys to be used in non-critical applications where ductility is not the main requirement.Item type:Publication, Comparison of blended elemental (BE) and mechanical alloyed (MA) powder compact forging into Ti-6Al-4V rocker arms2012, Trans Tech PublicationsTi-6Al-4V rocker arms for internal combustion engines were produced by forging of compacts of blended powder consisting of elemental hydride-dehydride (HDH) titanium powder and Al60V40 (wt%) master alloy powder or mechanical alloyed (MA) powder synthesized by high energy mechanical milling of a mixture of HDH titanium and Al60V40 master alloy powders. The powder compacts were made by warm compaction, and their relative density was 90%. The mechanical properties and microstructures of as-forged parts made using blended powder were improved significantly with increasing holding time at forging temperature, and close to those of as-forged parts produced by powder compact forging of HDH Ti-6Al-4V pre-alloyed powder. However, the as-forged part produced by powder compact forging of MA powder was brittle, and fractured prematurely during tensile testing.Item type:Publication, Tensile properties of Ti-6Al-4V discs produced by open die powder compact forging of pre-alloyed HDH powders2012, Trans Tech PublicationsOpen die powder compact forging was employed for consolidation of Ti-6Al-4V(wt.%) powders which were produced by a hydride-dehydride (HDH) process. The powders were initially warm-compacted into cylindrical shapes. Induction heating was used for preheating the compacts prior to forging into plates. The effect of the forging parameters such as temperature and pre-sintering time on the microstructure and tensile properties of the forged plates were studied. Porosity and the alpha-beta phase distribution were investigated to enable a better understanding of their effect on the fracture behaviour of the tensile tested specimens. The fracture surfaces of the broken tensile specimens were analysed using Scanning Electron Microscopy (SEM) to find the correlation between microstructure, residual porosity and fracture behaviour. A combination of high ultimate tensile strength of over 1200MPa and a good ductility reflected by an elongation to fracture of around 10% was achieved in some of the forged discs.Item type:Publication, Effects of lubrication on the powder metallurgy processing of titanium2012, Trans Tech PublicationsThe role of lubrication on the consolidation behaviour of titanium powder, density increase and change in microstructure on subsequent sintering was investigated. HDH titanium powder mixed with 0-2wt% stearic acid or magnesium stearate was cold compacted. It was found that 0.3-0.6wt% of internal lubricant significantly improves the compressibility. However, more than 0.6wt% of lubricant aids the densification in the low-pressure region but limits the maximum density at high pressure. Moreover, 0.3-0.6wt% of lubricant offers a more uniform density distribution to the powder compact, while greater than 0.6wt% of lubricant leads to a segregation of lubricant in the surface region. The shape retention, ejection behaviour, de-lubrication behaviour and sintered properties were also studied in this work.