    Relationship between manufacturing and properties of vacuum sintered Ti and Ti-6Al-7Nb
    2022, MDPI AG
    Titanium alloys are ideal for a great range of engineering applications; however, their high manufacturing costs hinder their widespread use. This study investigates the relationship between the processing and properties of representative Ti-based materials manufactured via powder metallurgy in order to reduce the manufacturing costs. This is possible as powder metallurgy techniques are near-net shape processes with high yield of material. It is found that the relative density increases with the sintering temperature, and it is slightly higher for longer processing times, reaching values in the 94–97% range. Moreover, homogeneous microstructures are obtained for all the conditions investigated, achieving an equiaxed microstructure for Ti and the typical lamellar structure for the Ti-6Al-7Nb alloy. However, the increment of the temperature also leads to a higher amount of interstitial pick-up, with a maximum increment of 0.21 wt.% and 0.028 wt.% for oxygen and nitrogen, respectively. The highest properties achieved for Ti and Ti-6Al-7Nb are 272 HV (hardness), 17.9 W/m·K (thermal conductivity), and 62.7 μohm·cm (electrical resistivity) and 336 HV, 6.9 W/m·K, and 180 μohm·cm, respectively.
  • Item type:Publication,
    Assessment of Plasma Deposition Parameters for DED Additive Manufacturing of AA2319
    2023, MDPI AG
    Arc-directed energy deposition using wire as feedstock is establishing itself as a 3D printing method capable of obtaining additively manufactured large structures. Contrasting results are reported in the literature about the effect of the deposition parameters on the quality of the deposited tracks, as it is highly dependent on the relationship and intercorrelations between the individual input parameters, which are generally deposition-technique-dependent. This study comprehensively analysed the effect of several deposition parameters and clarified their interactions in plasma metal deposition of Al alloys. It was found that, although no straightforward correlation between the individual input parameters investigated and the measured output deposition track’s quality aspects existed, the input current had the greatest effect, followed by the wire feed speed and its interaction with the input current. Moreover, the greatest effect of changing the shielding gas atmosphere, including the gas mixture, flow rate and plasma flow, was on the penetration depth, and fine-tuning the frequency/balance ratio and the preheating of the deposition substrates reduced the amount of porosity. This study demonstrates that well-deposited multi-layer walls made out of Al alloys can successfully be achieved via plasma metal deposition.
  • Item type:Publication,
    Joint effect of steel addition and press-and-sinter on the properties of low-cost PM Ti Alloys
    2018, Trans Tech Publications
    Cheap alloying elements and creative processing techniques are a way forward to open up more industrial opportunities for Ti in sectors where it is not extensively applied yet, rather than in aerospace and biomedical applications. This study focuses on understanding the joint effect of using a commercial steel powder to add Fe to pure Ti and its processing by press-and-sinter on the behaviour of low-cost PM Ti alloys. It is found that the calibrated addition of steel permits to develop new low-cost Fe-bearing Ti alloys that can satisfactorily be produced using the blending elemental PM approach. Densification of the samples and homogenization of the chemical composition are enhanced by the high diffusivity of Fe. The low-cost α+β alloys reach comparable physical and mechanical properties to those of wrought-equivalent PM Ti alloys, such as Ti-6Al-4V, and are therefore promising candidates for load-bearing lightweight products.
  • Item type:Publication,
    Low-Cost α+β PM Ti Alloys by Fe/Ni Addition to Pure Ti
    2016
    Ti and its alloys can deliver a very interesting combination of properties such as low density, high strength, corrosion resistance and biocompatibility and, therefore, are very flexible materials which can be adapted to various applications. Nonetheless, Ti and Ti alloys are only employed in critical applications (i.e. aeronautical and aerospace, nautical, medical, etc.) or in products for leisure. In both of these cases the higher fabrication costs of Ti in comparison to its competitors (i.e. steel and aluminium) is not the limiting factor as it is for many structural applications, especially for mass production (i.e. automotive sector). The use of creative techniques and the decrement of the starting price of Ti have been identified as the two main routes to follow to decrease the fabrication costs. In this study, the production of low-cost α+β Ti alloys has been assessed by combining the addition of cheap alloying elements (in particular a Fe/Ni powder) with the classical powder metallurgy route (pressing and sintering). Physical and mechanical properties as well as microstructural analysis of these low-cost alloys were measured and correlated to the processing parameters used to sinter them. It is found that the low-cost Ti alloys show similar behaviour to conventional α+β Ti alloys and, thus, have the potential to be used for non-critical applications.
  • Item type:Publication,
    Quantifying the properties of low-cost powder metallurgy titanium alloys
    2017-02
    The extensive industrial employment of titanium is hindered by its high production costs where reduction of these costs can be achieved using cheap alloying elements and appropriate alternative processing techniques. In this work the feasibility of the production of low-cost titanium alloys is addressed by adding steel to pure titanium and processing the alloys by powder metallurgy. In particular, a spherical 4140 LCH steel powder commonly used in metal injection moulding is blended with irregular hydride-dehydride Ti. The new low-cost alloys are cold uniaxially pressed and sintered under high vacuum and show comparable properties to other wrought-equivalent and powder metallurgy titanium alloys. Differential thermal analysis and X-ray diffraction analyses confirm that Ti can tolerate the employment of iron as primary alloying element without forming detrimental TiFe-based intermetallic phases. Thus, the newly designed α+β alloys could be used for cheaper non-critical components.
  • Item type:Publication,
    Evaluation of the mechanical properties of powder metallurgy Ti-6Al-7Nb alloy
    2017-03
    Titanium and its alloys are common biomedical materials owing to their combination of mechanical properties, corrosion resistance and biocompatibility. Powder metallurgy (PM) techniques can be used to fabricate biomaterials with tailored properties because changing the processing parameters, such as the sintering temperature, products with different level of porosity and mechanical performances can be obtained. This study addresses the production of the biomedical Ti-6Al-7Nb alloy by means of the master alloy addition variant of the PM blending elemental approach. The sintering parameters investigated guarantee that the complete diffusion of the alloying elements and the homogenization of the microstructure is achieved. The sintering of the Ti-6Al-7Nb alloy induces a total shrinkage between 7.4% and 10.7% and the level of porosity decreases from 6.2% to 4.7% with the increment of the sintering temperature. Vickers hardness (280–300 HV30) and tensile properties (different combination of strength and elongation around 900 MPa and 3%) are achieved.
  • Item type:Publication,
    Understanding the properties of low-cost iron-containing powder metallurgy titanium alloys
    2016-11-15
    The high production costs of titanium in comparison to other structural metals is the main limiting factor for the wide employment of titanium. Cost reduction can be addressed considering creative fabrication methods and/or formulating new chemical compositions. In this work the fabrication of low-cost iron-containing powder metallurgy titanium alloys is studied by using a spherical 85Fe/15Ni powder whose small particle size and spherical morphology favours both the densification of the material and the diffusion of the alloying elements. The designed composition are obtained by the blending elemental approach and processed by means of the conventional powder metallurgy route. The high vacuum sintered α + β alloys show homogeneous microstructure and the formation of brittle intermetallic phases is prevented as checked by XRD and DTA analysis. Similar physical and mechanical behaviour to wrought-equivalent structural titanium alloys is obtained for these new low-cost alloys which, therefore, are potential materials for cheaper structural titanium components.
  • Item type:Publication,
    Modification of sintered titanium alloys by hot isostatic pressing
    2012, Trans Tech Publications
    Powder metallurgy (PM) permits to obtain titanium alloys with properties and microstructures close to ingot metallurgy products. However, residual porosity is normally present in the products produced by the PM route of powder pressing and sintering (P&S)\, and this needs to be reduced by using post-sintering process step such as hot isostatic pressing (HIP) and forging. In this study, the microstructural and mechanical property changes caused by HIP of samples of two alloys, near-α Ti-3Al-2.5V alloy and α+β Ti-6Al-4V, produced by P&S route were investigated. Two types of powders were utilised: prealloyed powders and blend of elemental titanium powder and master alloy powder. Four conditions defined by HIP temperature, pressure and time were used to HIP the sintered samples with two geometries. The results show that, independent of the HIP conditions used, HIP increased the relative density of the samples to approximately 97.5% and their hardness by 30-50 HV depending on the HIP condition. However, HIP at 1000°C changes the fracture mode of the sintered samples from ductile to brittle.