University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
4 results
Search Results
Item type:Publication, The role of peracetic acid in bloodmeal decoloring2013, SpringerHydrogen peroxide (HP) can degrade soluble heme, forming yellow or colorless degradation products. Thermal treatment during bloodmeal production changes the conformation of oxyhemoglobin trapping heme in hydrophobic protein regions or forms methemoglobin (metHb) heme which catalytically removes HP. As a result, HP can only degrade a portion of the heme present in bloodmeal leading to poor decoloring. Equilibrium peracetic acid (PAA) solutions can effectively decolor bloodmeal. This work assessed the ability of PAA to decolor bloodmeal and the mechanism by which it occurs. The inability of HP to decolor bloodmeal is determined by the fact that it is unable to permanently degrade metHb heme, or hydrophobically trapped heme. Addition of organic acids to HP led to significant swelling of the protein chains but also to poorer decoloring and lower HP consumption compared to PAA. This suggested that in the case of PAA solutions, where bleaching was facile, the reason PAA solutions are capable of decoloring bloodmeal was due to the action of the PAA molecule against heme, whereas HP and acetic (ethanoic) acid played only minor roles in total bleaching. The decolored protein powder has reduced odor and whiter color, and is suitable for applications such as bioplastics.Item type:Publication, Biodegradation of bloodmeal-based thermoplastics in green-waste composting2011, SpringerPolymers that are compostable and manufactured from renewable resources have gained significant importance in recent years. The objective of this work was to assess the biodegradability of bloodmeal-based thermoplastics in a commercial green-waste composting situation. Materials plasticised with tri-ethylene–glycol lost about 45% of their original mass after 12 weeks composting while unplasticised samples lost 35%. Degradation appeared to have been in two phases; an initial loss of soluble, low molecular compounds in the mesophilic phase followed by degradation of high molecular compounds as the temperature exceeded about 40 °C in the thermophilic phase. It was found that as degradation proceeded materials became more soluble. In addition, plasticised and unplasticized samples contained about 60 wt% moisture after 4 weeks of composting conditioning at 50% relative humidity resulted in approximately 8–10 wt% moisture, unaffected by the extent of degradation. FTIR revealed that proteins underwent hydrolytic cleavage resulting in the formation of primary amines. A significant reduction in combustion temperature was observed, indicative of a reduction in covalent bonding, likely due to shorter chains lengths or less cross-linking.Item type:Publication, Odorous compounds in bioplastics derived from bloodmeal2011, SpringerDuring the processing of bloodmeal-based thermoplastics (BMT), volatile compounds are released which are odorous and unpleasant. Literature searches revealed that blood components are thermally unstable under oxidising conditions and the presence of iron in bloodmeal (BM) may catalyse the formation of various odorous compounds. The objective of this work was to establish an odour profile for BM as well as BMT prior to extrusion and to determine the effect of oxidative treatment on the resulting odour profile. A comparison of the volatile compounds arising from using BM with those arising from using red blood cells (RB) was carried out using headspace-solid phase micro-extraction–gas chromatography–mass spectrometry (HS-SPME–GC/MS). A total of 23 compounds were identified, 4 of which were products of putrefaction also identified in RB subjected to putrefactive degradation; these were phenol, 4-methyl phenol, indole and methyl indole. In addition, several aldehydes and ketones were identified in BM and RB and may result from thermal, microbiological or auto-oxidative deterioration of the lipids and proteins present in blood during BM manufacture. Oxidative treatment of BM removed some of the compounds that were generated by putrefaction and thermal degradation. Treatment led to an improvement in the perceived odour type and intensity of BM, however, upon conversion to BMT the perceived odour became significantly worse. This malodour was able to be mitigated by the addition of 10–20 wt% activated carbon or greater than 20 wt% natural zeolite, however some malodour reoccurred after storage.Item type:Publication, Degradation as a result of UV radiation of bloodmeal-based thermoplastics2011, ElsevierPolymers are known for their susceptibility to degradation as a result of ultra-violet (UV) radiation. In this study, the UV stability of bloodmeal-based thermoplastics (BMT) was evaluated over a period of 12 weeks. Formulations with and without plasticiser were tested and moisture was excluded during accelerated weathering to isolate the effect of UV because of the material’s known sensitivity to moisture. It was found that embrittlement due to loss of water overshadowed the effect of UV degradation. Embrittlement caused the material’s toughness to be reduced by an order of magnitude after only two weeks of exposure, for either plasticised or unplasticised samples. An initial increase in tensile strength was observed after two weeks followed by a steady decline in strength. The elastic modulus reached a plateau after about two weeks of exposure. FTIR did not confirm any chemical changes after 12 weeks exposure and TGA suggested that low molecular mass species were quickly lost during the course of the test. The absence of chemical changes does not suggest resistance to environmental degradation, although the dark pigmentation of bloodmeal may have contributed to the lack of UV degradation. Embrittlement remains a greater concern and requires further attention.