University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, Mechanical behaviour of ultrafine grained Cu and Cu-(2.5 and 5) vol.%Al₂O₃ composites produced by powder compact forging2011, Trans Tech PublicationsNanostructured Cu-(2.5 and 5) vol.%Al₂O₃ composite powders were produced from a mixture of Cu powder and Al₂O₃ nanopowder using high energy mechanical milling, and then compacted by hot pressing. The Cu and Cu- Al₂O₃ composite powder compacts were then forged into disks at temperatures in the range of 500-800°C to consolidate the Cu and Cu- Al₂O₃ composite powders. Tensile testing of the specimens cut from the forged disks showed that the Cu forged disk had a good ductility (plastic strain to fracture: ~15%) and high yield strength of 320 MPa, and the Cu-(2.5 and 5)vol.%Al₂O₃ composite forged disks had a high fracture strength in range of 530-600 MPa, but low ductility.Item type:Publication, Microstructure and mechanical behaviour of ultrafine grained Al-4wt%Cu-(2.5-10) Vol.% SiC metal matrix composites produced by powder compact forging2011, Trans Tech PublicationsUltrafine grained Al-4wt%Cu-(2.5-10) vol.% SiC metal matrix composite powders were produced from a mixture of Al, Cu and SiC powders using high energy mechanical milling (HEMM). The composite powders produced were first hot pressed at 300°C with a pressure of 240 MPa to produce cylindrical powder compacts with a relative density in the range of 80-94% which decreased with increasing the SiC volume fraction. Powder compact forging was utilized to consolidate the powder compacts into nearly fully dense forged disks. With increasing the volume fraction of SiC from 2.5% to 10%, the average microhardness of the forged disks increased from 73HV to 162HV. The fracture strength of the forged disks increased from 225 to 412 MPa with increasing the volume fraction of SiC particles from 2.5 to 10%. The Al-4wt%Cu-2.5vol.%SiC forged disk did not show any macroscopic plastic yielding, while the Al-4wt%Cu-(7.5 and 10)vol.% SiC forged disk showed macroscopic plastic yielding with a small plastic strain to fracture (~1%).Item type:Publication, Effect of processing condition and composition on the microhardness of Cu-(2.5-10)vol.%Al₂O₃ nanocomposite powder particles produced by high energy mechanical milling2010, World ScientificNanostructured Cu-(2.5-10vol.%)Al₂O₃ nanocomposites were produced using high energy mechanical milling. For the as-milled Cu- Al₂O₃ composite powder particles having Al₂O₃ volume fractions of 2.5% and 5%, the increase in average microhardness is significant with the increase of milling time from 12 hours to 24 hours. With the increase of the content of Al₂O₃ nanoparticles the microhardness increases and in the range of 255HV-270HV. The milled nanocomposite powders were heat treated at 150, 300, 400 and 500°C for 1 hour, respectively, to determine the thermal stability of the powder particles as a function of annealing temperature. The average microhardness increased/decreased for the Cu- Al₂O₃ composites after annealing at 150°C due to the dislocation density, while increasing the annealing temperature to 300°C and 400°C the average microhardness almost remained mostly unchanged. Further increasing the annealing temperature to 500°C causes significant decrease in average microhardness due to reduction in dislocation density and coarsening of Cu grains of the Cu- Al₂O₃ composite powders produced after 24 hours of milling. This paper is to report and discuss the changes of the microhardness of the material, caused by the compositions and processing conditions, used to fabricate the Cu-(2.5-10)vol.% Al₂O₃ nanocomposite powders.