Now showing 1 - 3 of 3
  • Item type:Publication,
    Reactive compatibilization of harakeke fiber-reinforced poly(lactic) acid/polybutylene succinate blend
    2024, Wiley
    Different blends of poly(lactic acid) (PLA) and polybutylene succinate (PBS), and their harakeke fiber-reinforced composites were studied. Scanning electron microscopy showed that the PLA and PBS are incompatible and poorly miscible. Tensile strength and tensile modulus of the blends were found to reduce as the amount of PBS increased. Reinforcement alone was not able to significantly improve the mechanical performance of the blend, which is lower than that of neat PLA. Therefore, simultaneous reinforcement and reactive compatibilization were performed using harakeke fiber, and dicumyl peroxide as reinforcement and compatibilizer, respectively. This produced about 201% increase in the crystallinity of PLA. Compared with the PLA/PBS blend, the dual effect approach increased the tensile strength and tensile modulus by 31% and 148%, respectively. Likewise, dynamic mechanical analysis showed that the thermomechanical properties of the composite greatly improved.
  • Item type:Publication,
    Polylactide composites reinforced with pre-impregnated natural fibre and continuous cellulose yarns for 3D printing applications
    2024, MDPI AG
    Achieving high-performance 3D printing composite filaments requires addressing challenges related to fibre wetting and uniform fibre/polymer distribution. This study evaluates the effectiveness of solution (solvent-based) and emulsion (water-based) impregnation techniques to enhance fibre wetting in bleached flax yarns by polylactide (PLA). For the first time, continuous viscose yarn composites were also produced using both impregnation techniques. All the composites were carefully characterised throughout each stage of production. Initially, single yarns were impregnated and consolidated to optimise formulations and processing parameters. Solution impregnation resulted in the highest tensile strength (356 MPa) for PLA/bleached flax filaments, while emulsion impregnation yielded the highest tensile strength for PLA/viscose filaments (255 MPa) due to better fibre wetting and fibre distribution. Impregnated single yarns were then combined, with additional polymer added to produce filaments compatible with standard material extrusion 3D printers. Despite a reduction in the mechanical performance of the 3D-printed composites due to additional polymer impregnation, relatively high tensile and bending strengths were achieved, and the Charpy impact strength (&gt;127 kJ/m2) for the viscose-based composite exceeded the reported values for bio-derived fibre reinforced composites. The robust mechanical performance of these filaments offers new opportunities for the large-scale additive manufacturing of structural components from bio-derived and renewable resources.
  • Item type:Publication,
    Gelatin and collagen from sheepskin
    2024-05-31, MDPI AG
    Abattoirs dispose of sheepskins as solid waste due to low price and poor demand for sheepskin leather. In principle, as an alternative to being disposed of in landfill, sheepskins can serve as a source of the protein collagen or the hydrolysis product, gelatin. In this research, sheepskins collected from abattoirs were used as a source of collagen. Three extraction methods were compared: acid extraction, acid with enzymes, and alkali extraction. The extracted material was characterized using scanning electron microscopy (SEM) and Fourier-transform infrared spectroscopy (FTIR), small angle X-ray scattering (SAXS), and sodium dodecyl sulfate polyacrylamide gel electrophoresis (SDS-PAGE). The collagen and gelatin extraction yield ranged from 3.1% to 4.8% with the product purity determined by hydroxyproline, ranging from 7.8% for the alkali process to 59% and 68% for the acid and acid-enzyme processes. SDS PAGE showed that the acid process produced fragments with molecular weights in the range 100 to &gt;250 kDa, while acid–enzyme resulted in smaller fragments, below 30 kDa. The FTIR region of the amide I band at 1800–1550 cm−1, which was used as an indicator of the collagen and gelatin content, showed that the gelatin dominated in the acid extracts, and the alkaline extract contained a large portion of keratin. SAXS was found to be a sensitive method for showing the presence of intact collagen fibrils in materials from all of the extraction methods, albeit at low concentrations. Herein, sheepskin is shown to be a useful source for collagen–gelatin material of varying molecular weights.