    Tensile and flexural performance of FDM 3D printed Harakeke (NZ Flax) fiber -PLA composites for lightweight structural applications
    2026, Elsevier
    Current research on the shift toward sustainable materials has intensified interest in biodegradable alternatives polymers, with poly-lactic acid (PLA) emerging as a leading candidate. With various advantages, including biodegradability and processability, PLA's tensile and flexural strength can be further enhanced to increase its use in lightweight structural applications. This study introduces a novel integration of harakeke (New Zealand flax) fibers into PLA, a material pairing that has not been comprehensively investigated for additive manufacturing-based components. The research uniquely employs a Response Surface Methodology (RSM)-based optimization framework to systematically analyze and model the combined effects of fiber content (0-20 wt.%), raster angle (45-90°), and raster width (0.5-1.0 mm) on the composite’s tensile and flexural performance. The findings reveal that a raster width of 0.5 mm, raster angle of 45°, and a flax infill of 10% by weight provide the best synergy of stiffness and strength. The maximum values ​​of Young's modulus are 4453.85 MPa, and the flexural stress is 73.395 MPa. Increased fiber loadings above 20 wt.% reduce performance due to fiber agglomeration. Among orientations, the 45° raster is preferable to 90° due to increased load transfer and stress distribution, and narrower raster widths facilitate greater interlayer bonding and deposition density.
  • Item type:Publication,
    Combining Hydromorphic and Shape-Shifting Effects for Programmable Passive Actuation in 4D-Printed Biocomposites
    2025, Elsevier BV
    4D printing involves the fabrication of structures that respond dynamically to external stimuli. While various actuation mechanisms have been extensively studied, the integration of multiple actuation effects remains relatively unexplored. This study examines the combined influence of hydromorphic and shape-shifting effects in a biocomposite containing 40 wt% cellulose fibres. The biocomposite was combined with polylactide (PLA) and processed via 3D printing to produce bi-material strips, which were then comprehensively analysed for their material properties and shape-changing behaviour. Upon immersion in water, the biocomposite expanded by 3.2 % perpendicular to the printing direction and exhibited a marked decrease in Young’s modulus with increasing water content. Bi-material strips 1 mm thick displayed pronounced hydromorphic behaviour, achieving maximum curvatures of 0.036 - 0.052 mm-1 depending on the passive-to-active layer thickness ratio. Thicker strips (4 mm) reached 0.012 mm-1 under the same conditions. When both heat and water were applied as external stimuli, the biocomposite and neat PLA layers became simultaneously active, and curvatures of up to 0.057 mm⁻¹ were obtained for 4 mm strips. This curvature surpassed the hydromorphic-only and shape-shifting-only responses by factors of 4.77 and 1.82, respectively. The results demonstrate that integrating water- and heat-induced stimuli increases achievable curvature and accelerates the response, enabling high-curvature deformations even in relatively thick structures. The approach therefore holds promise for applications that demand significant shape transformations without compromising structural integrity.
  • Item type:Publication,
    Reactive compatibilization of harakeke fiber-reinforced poly(lactic) acid/polybutylene succinate blend
    2024, Wiley
    Different blends of poly(lactic acid) (PLA) and polybutylene succinate (PBS), and their harakeke fiber-reinforced composites were studied. Scanning electron microscopy showed that the PLA and PBS are incompatible and poorly miscible. Tensile strength and tensile modulus of the blends were found to reduce as the amount of PBS increased. Reinforcement alone was not able to significantly improve the mechanical performance of the blend, which is lower than that of neat PLA. Therefore, simultaneous reinforcement and reactive compatibilization were performed using harakeke fiber, and dicumyl peroxide as reinforcement and compatibilizer, respectively. This produced about 201% increase in the crystallinity of PLA. Compared with the PLA/PBS blend, the dual effect approach increased the tensile strength and tensile modulus by 31% and 148%, respectively. Likewise, dynamic mechanical analysis showed that the thermomechanical properties of the composite greatly improved.
  • Item type:Publication,
    Polylactide composites reinforced with pre-impregnated natural fibre and continuous cellulose yarns for 3D printing applications
    2024, MDPI AG
    Achieving high-performance 3D printing composite filaments requires addressing challenges related to fibre wetting and uniform fibre/polymer distribution. This study evaluates the effectiveness of solution (solvent-based) and emulsion (water-based) impregnation techniques to enhance fibre wetting in bleached flax yarns by polylactide (PLA). For the first time, continuous viscose yarn composites were also produced using both impregnation techniques. All the composites were carefully characterised throughout each stage of production. Initially, single yarns were impregnated and consolidated to optimise formulations and processing parameters. Solution impregnation resulted in the highest tensile strength (356 MPa) for PLA/bleached flax filaments, while emulsion impregnation yielded the highest tensile strength for PLA/viscose filaments (255 MPa) due to better fibre wetting and fibre distribution. Impregnated single yarns were then combined, with additional polymer added to produce filaments compatible with standard material extrusion 3D printers. Despite a reduction in the mechanical performance of the 3D-printed composites due to additional polymer impregnation, relatively high tensile and bending strengths were achieved, and the Charpy impact strength (&gt;127 kJ/m2) for the viscose-based composite exceeded the reported values for bio-derived fibre reinforced composites. The robust mechanical performance of these filaments offers new opportunities for the large-scale additive manufacturing of structural components from bio-derived and renewable resources.
  • Item type:Publication,
    Recyclable hemp hurd fibre-reinforced PLA composites for 3D printing
    2024, Elsevier
    In this study, 3D printing filaments were produced from hemp hurd fibre-reinforced polylactide (PLA) composites. Hemp hurd microfibres were obtained through alkaline digestion followed by a bleaching treatment and were used to produce PLA-based composites with 20–40 wt% fibre content for fused deposition modelling. Tensile testing of 3D printed composites revealed a gradual increase of Young's modulus with the addition of fibres, reaching a maximum of 7.1 GPa for the 40 wt% composite - a two-fold increase to neat PLA. However, tensile strength was only improved for the 20 wt% formulation, with an increase of 8% in comparison with neat PLA. Nevertheless, the thermo-mechanical properties of the composites were significantly enhanced with the addition of fibres. In addition, physical objects were printed from the recycled filaments to assess their recyclability and printability. It was found that the recycled filaments maintained comparable mechanical properties and printability after three recycling cycles.
  • Item type:Publication,
    Mechanenzymatic production of natural fibre from harakeke (New Zealand flax) and its characterization for potential use in composites for building and construction applications
    2024, Elsevier B.V.
    Mechanical processing of natural fibres can be used to produce large quantities of clean and refined fibres. However, this often results in fibre damage when used alone, thereby affecting the quality of fibres produced, and it generally makes them of insufficient quality for high-performance composite applications. In contrast, the use of biological agents such as enzymes have become a rapidly expanding area of research for producing high quality fibres, but this is still limited to pilot scales. This paper reports the effect of synergizing the salient features of mechanical processing (using a super masscolloider) and enzymatic treatment, on the structure and properties of harakeke (indigenous New Zealand flax) fibre. The cellulose fibres produced are characterized for their potential use as reinforcement in composites. Results show that the combination of mechanical processing with enzymatic treatment could help to overcome the limitations of both processes.
  • Item type:Publication,
    Combined digestion and bleaching of New Zealand flax /harakeke fibre and its effects on the mechanical, thermal, and dynamic mechanical properties of poly(lactic) acid matrix composites
    2023-01, Elsevier BV
    In this study, New Zealand flax (harakeke) fibre was initially modified through digestion in an alkali solution followed by bleaching with hydrogen peroxide and sodium silicate with the aim of improving thermal and mechanical performance of its composites, through increased interfacial bonding. X-ray diffraction analysis (XRD), Fourier transform infrared spectroscopy and lignin analysis showed that the combination of bleaching and alkali treatment resulted in a higher cellulose content than digestion alone. Fibre inclusion was found to increase the crystallinity of PLA, likely due to heterogeneous nucleation on the treated fibres, which in turn helped to improve the composite strength. The highest tensile strength, tensile modulus and thermal stability were achieved with the bleached fibre which is believed to be due to better fibre distribution and stronger interfacial interaction. This was supported by the adhesion factor and effectiveness coefficient calculated using the data obtained from dynamic mechanical analysis.