<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 6 of 6
  • Item type:Publication,
    Effect of stearic acid treatment on the properties of aligned short hemp fibre mats and their potential use as reinforcement in polypropylene matrix composites
    2021, Springer
    The main objective of this study was to assess the effect of stearic acid vapour treatment on hemp fibre mats produced using dynamic sheet forming, and the potential use of these treated mats as reinforcement in polypropylene matrix composites. Stearic acid was successfully applied through vapour treatment, appearing to form a layer on fibre surfaces. It was found that the presence of stearic acid increased hydrophobicity and thermal stability of fibre mats. It was also found to increase thermal stability of polypropylene matrix composites as well as their strength.
  • Item type:Publication,
    Treatment of hemp fibres for use in rotational moulding
    2021, Springer
    The benefit of using alkali-treated hemp fibre as the reinforcement for rotationally moulded evaluated in this research. Untreated and alkali treated hemp fibre were characterised using different techniques such as scanning electron microscopy (SEM), thermal analysis, and Fourier transform infrared spectroscopy (FT-IR). These techniques showed that the alkali treatment removed non-cellulosic components from hemp fibres, which improved their separation and thermal resistance. Composites with alkali treated fibre resisted the exposure to elevated temperatures for prolonged periods (characteristic of the rotational moulding process) with no apparent signs of thermal degradation, unlike when untreated fibre was used. The effect of using maleic anhydride grafted polyethylene (MAPE) as a coupling agent was also investigated. The addition of 3 wt% MAPE improved the properties tensile strength and Young’s modulus of composites with treated hemp fibre, which was attributed to better fibre-matrix adhesion. Different fibre contents were assessed in this research to produce rotationally moulded composites; a poor fibre distribution was observed above 5 wt% fibre content, which resulted in low tensile strength and Young’s modulus.
  • Item type:Publication,
    Alkali treatment of hemp fibres for the production of aligned hemp fibre mats for composite reinforcement
    2020, Springer
    The main objective of this study was to produce aligned hemp fibre mats from high strength hemp fibres using dynamic sheet forming (DSF). Alkali treatment of hemp fibre was carried out at ambient and high temperature to separate fibres. Single fibre tensile testing was used to assess the tensile properties of the fibres. It was found that the highest tensile properties were exhibited by high temperature treated fibre, whereas the tensile properties exhibited by ambient temperature treated fibre were lower than for untreated fibre. It was also found that fibre granulated after high temperature treatment, was better separated than that granulated before high temperature treatment. This well-separated fibre could successfully be formed into mats using DSF. The orientation of the formed mat was analysed using ImageJ (NIH, USA) software by which the potential of DSF to produce aligned hemp fibre mat was supported. The tensile properties of composite reinforced by these aligned hemp fibre mats were assessed.
  • Item type:Publication,
    Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites
    2019, Springer
    In this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.
  • Item type:Publication,
    Manufacturing and characterization of sustainable hybrid composites using sisal and hemp fibres as reinforcement of poly (lactic acid) via injection moulding
    2019, Elsevier Science BV
    Natural polymers based composites offers significant advantages over synthetic fibre reinforced petroleum matrix based composites with regard to biodegradability, biocompatibility, design flexibility and sustainability. This work reports for the first time manufacturing of hybrid fibre reinforced biodegradable composites using sisal and hemp fibre with polylactic acid employing melt processing and injection moulding techniques. Granulated sisal and hemp fibres were blended and hybrid composites were manufactured using aliphatic polyester made up of lactic acid (PLA) through extrusion and injection moulding and their performance was evaluated. Experimental results revealed that density, elongation at break and water absorption capacity of hybrid composites were 1.14 ± 0.07 g/cm³, 0.93 ± 0.35% and 1.06 ± 0.18% respectively. The achieved mean tensile strength (46.25 ± 6.75 MPa), Young’s modulus (6.1 ± 0.58 GPa) and specific tensile strength (38.86 ± 5.0) of hybrid fibre reinforced PLA composites were improved compared to neat PLA. The flexural strength (94.83 ± 11.21 MPa), flexural modulus (6.04 ± 0.55 GPA) and specific flexural strength (79.76 ± 8.80) of hybrid fibre composites also showed better performance than those of neat PLA. Incorporation of sisal and hemp fibre with polylactide remarkably increased the impact strength of composites. Overall, the hybrid composites demonstrated good performance suggesting that they have great potential for use as an environmentally friendly alternative material in automotive, packaging, electronics, interiors and agricultural applications.
  • Item type:Publication,
    Analysis of mechanical properties of hemp fibre reinforced unsaturated polyester composites
    2013, Sage
    Different chemically treated hemp fibre reinforced unsaturated polyester composites were investigated over a range of fibre content (0–60 wt%). Although Young’s modulus of all the short fibre reinforced unsaturated polyester composites was found to be higher than that of unreinforced unsaturated polyester; however, tensile strength of the composites exceeded that of the unsaturated polyester matrix only for the combined alkali- and silane-treated fibre composites at 40 wt% fibre content. The decrease in tensile strength of the composites could be attributed to stress concentrations caused by the fibres in conjunction with the brittle matrix. Impact strength of all the treated fibre composites was higher than that of the untreated fibre composites at all fibre contents. KIc and GIc of the composites decreased initially and thenincreased as the fibre content increased because more and more fibres being available to pull-out. The mechanical properties of the composites were increased further due to the alignment of long fibres.