University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
6 results
Search Results
Item type:Publication, The effects of alkaline digestion, bleaching and ultrasonication treatment of fibre on 3D printed harakeke fibre reinforced polylactic acid composites2023-03, Elsevier BVThis paper documents an investigation of the effects of fibre treatment on New Zealand flax (harakeke) fibre reinforced polylactic acid (PLA) composites. The raw fibre was alkali digested, followed by bleaching and then modified with ultrasonication. Alkali treatment removed lignin and other non-cellulosic components and partially separated fibre bundles while bleaching further removed lignin and improved the separation of elementary fibres, resulting in microfibres with a cellulose content 92 wt%. With subsequent ultrasonication, microfibrils could be seen partially separated (defibrillation) at fibre surfaces. Treated fibres were compounded with PLA at a fibre loading of 30 wt% and extruded into composite filaments. Filaments from alkali, bleached and ultrasonication-treated fibres had smooth surfaces, which translated into high-quality printability along with good mechanical performance. The combination of chemically treated microfibres with selective surface defibrillation using ultrasonication and fibre alignment induced by the printing process resulted in 3D printed samples with a tensile strength of 79 MPa and Young’s modulus of 8.7 GPa, which are the highest values reported so far for 3D printed PLA-based composites reinforced with short fibres.Item type:Publication, Fibre orientation of novel dynamically sheet formed discontinuous natural fibre PLA composites2016, ElsevierThis paper describes work carried out to fabricate and to assess the fibre orientation in PLA reinforced by aligned discontinuous harakeke and hemp fibre mats produced using a dynamic sheet former (DSF). These mats were combined with PLA sheets to make composites with fibre contents of 5–40 wt% using a hot press. It was found that the fibre orientation factors (Kθ) for both harakeke and hemp fibre composites were higher than those values seen in the literature for composites prepared using injection moulding and hot pressed using randomly oriented fibre mats, but slightly lower than the highest values obtained with aligned fibre nonwoven preform composites utilising more processing stages. The highest Kθ values for harakeke and hemp fibres in this work were found to be 0.58 and 0.44 respectively. Kθ decreased, reflecting increased fibre misalignment as fibre content increased, believed to be due to fibre agglomeration and the higher pressure required during processing.Item type:Publication, Preparation and mechanical properties of novel bio-composite made of dynamically sheet formed discontinuous harakeke and hemp fibre mat reinforced PLA composites for structural applications2016-06-01, Elsevier Science BvThe objective of this study was to fabricate and assess the structure and mechanical performance of PLA reinforced by aligned discontinuous alkali treated natural fibre mats. The novel aspect of this work was in terms of composite processing, in particular, the use of fibre mats produced using a dynamic sheet former (DSF) wherein discontinuous treated fibres were aligned. Composites with different fibre weight contents were assessed using optical microscopy, scanning electron microscopy (SEM) and tensile testing. It was found that the fibres had a reasonable degree of alignment parallel to the DSF rotation direction together with good fibre dispersion. Tensile strengths of harakeke and hemp composites up to 101.6 MPa and to 87.3 MPa were achieved, approximately 90 and 60% higher respectively than PLA (53.9 MPa). It was also found that minimum and critical fibre volume fractions for harakeke and hemp fibre composites were lower than that found for injection moulded composites, due to better reinforcement efficiency obtained as a result of increased fibre alignment.Item type:Publication, Comparison of dynamic properties of magnetorheological elastomers with existing antivibration rubbers2015-12-15, ElsevierTan δ and energy dissipated during hysteresis testing of isotropic and anisotropic MREs containing silane modified iron sand particles in a natural rubber matrix were compared with existing antivibration rubbers. Tan δ was measured using dynamic mechanical analysis (DMA) over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100–50 °C). Energy dissipated was measured using a universal tester under cyclic tensile loading. The chosen antivibration rubbers for comparison contained different contents of carbon black filler (30, 50 and 70 phr) in a natural rubber matrix. It was found that energy absorption for comparative samples was generally higher than isotropic and anisotropic MREs over the range of frequency and strain amplitude explored, as well as in hysteresis testing and this was believed to be largely due the presence of carbon black in the formulation. Further assessment was carried out on materials that were the same as anisotropic MREs except they had additions of carbon black. The energy absorption was found higher than comparative samples with the same carbon black contents, supporting the use of iron sand to improve damping. However, trends for energy absorption at around Tg were found to reverse which is considered to be due to the segmental motion of rubber chains being by far the most significant influence on energy absorption in the glass transition zone.Item type:Publication, Mode I and Mode II interlaminar fracture toughness of composite laminates interleaved with electrospun nanofibre veils2015-05-01, ElsevierIn this study, the effects of interleaved nanofibre veils on the Mode I and Mode II interlaminar fracture toughness (ILFT) of autoclave cured unidirectional carbon/epoxy composite laminates were investigated. Various electrospun nanofibre veils consisting of a range of different polymer types, fibre diameters and veil architectures were placed in the laminate mid-planes, which were subsequently subjected to double cantilever beam and end-notch flexure tests. It was found that the polymer type and veil areal weight were the most important factors contributing to laminate performance. A 4.5 g/m2 PA66 veil provided the best all-round performance with fracture toughness improvements of 156% and 69% for Mode I and Mode II, respectively.Item type:Publication, Comparison of harakeke with hemp fibre as a potential reinforcement in composites2014-12-01, ElsevierThe objective of this study was to characterize the performance of untreated and chemically treated harakeke fibre (a leaf fibre from a plant native to New Zealand) and compare with hemp fibre to assess its use as potential reinforcement in composites. Alkali treatment is among the most popular treatments used to remove unwanted fibre constituents such as pectin, hemicellulose and waxes; it can enhance fibre properties, fibre separation, interfacial bonding and fibre dispersion within a composite. Physical and mechanical properties of untreated and alkali treated fibres were assessed using single fibre tensile testing, X-ray diffraction (XRD), scanning electron microscopy (SEM) and thermal analysis using thermogravimetric analysis (TGA). Untreated harakeke fibre was found to be lower in tensile strength compared to untreated hemp fibre. It was also found that the tensile strength of harakeke and hemp fibres treated with 5wt% NaOH/2wt% Na2SO3 and 5wt% NaOH was not significantly affected and these fibres had good fibre separation. However, alkali treatment was found to lead to higher crystallinity index (Ic) and better thermal stability for harakeke as well as hemp fibres.