    Manufacturing and characterization of sustainable hybrid composites using sisal and hemp fibres as reinforcement of poly (lactic acid) via injection moulding
    2019, Elsevier Science BV
    Natural polymers based composites offers significant advantages over synthetic fibre reinforced petroleum matrix based composites with regard to biodegradability, biocompatibility, design flexibility and sustainability. This work reports for the first time manufacturing of hybrid fibre reinforced biodegradable composites using sisal and hemp fibre with polylactic acid employing melt processing and injection moulding techniques. Granulated sisal and hemp fibres were blended and hybrid composites were manufactured using aliphatic polyester made up of lactic acid (PLA) through extrusion and injection moulding and their performance was evaluated. Experimental results revealed that density, elongation at break and water absorption capacity of hybrid composites were 1.14 ± 0.07 g/cm³, 0.93 ± 0.35% and 1.06 ± 0.18% respectively. The achieved mean tensile strength (46.25 ± 6.75 MPa), Young’s modulus (6.1 ± 0.58 GPa) and specific tensile strength (38.86 ± 5.0) of hybrid fibre reinforced PLA composites were improved compared to neat PLA. The flexural strength (94.83 ± 11.21 MPa), flexural modulus (6.04 ± 0.55 GPA) and specific flexural strength (79.76 ± 8.80) of hybrid fibre composites also showed better performance than those of neat PLA. Incorporation of sisal and hemp fibre with polylactide remarkably increased the impact strength of composites. Overall, the hybrid composites demonstrated good performance suggesting that they have great potential for use as an environmentally friendly alternative material in automotive, packaging, electronics, interiors and agricultural applications.
  • Item type:Publication,
    Dynamic Properties of Magnetorheological Elastomers Based on Iron Sand and Natural Rubber
    2015-02-20, Wiley-Blackwell
    In this study, magnetorheological elastomers (MREs) based on iron sand and natural rubber were prepared. The Taguchi method was employed to investigate the effect of a number of factors, namely, the iron sand content, iron sand particle size, and applied magnetic field during curing on the loss tangent (tan δ) and energy dissipated during cyclic loading. Tan δ was measured through dynamic mechanical analysis over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100 to 50°C). The energy dissipated was measured with a universal tester under cyclic tensile loading. The data were then statistically analyzed to predict the optimal combination of factors, and finally, experiments were conducted for verification. It was found that the iron sand content had the greatest influence on tan δ when measured over a range of frequency, and the energy dissipated during hysteresis tests. However, none of the factors showed a significant influence on tan δ when measured over a range of strain amplitude. Furthermore, the iron sand content and magnetic field were also found to influence the width of the peak in tan δ as a function of the temperature. The morphological characteristics of the MREs were also examined with scanning electron microscopy.
  • Item type:Publication,
    Comparison of dynamic properties of magnetorheological elastomers with existing antivibration rubbers
    2015-12-15, Elsevier
    Tan δ and energy dissipated during hysteresis testing of isotropic and anisotropic MREs containing silane modified iron sand particles in a natural rubber matrix were compared with existing antivibration rubbers. Tan δ was measured using dynamic mechanical analysis (DMA) over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100–50 °C). Energy dissipated was measured using a universal tester under cyclic tensile loading. The chosen antivibration rubbers for comparison contained different contents of carbon black filler (30, 50 and 70 phr) in a natural rubber matrix. It was found that energy absorption for comparative samples was generally higher than isotropic and anisotropic MREs over the range of frequency and strain amplitude explored, as well as in hysteresis testing and this was believed to be largely due the presence of carbon black in the formulation. Further assessment was carried out on materials that were the same as anisotropic MREs except they had additions of carbon black. The energy absorption was found higher than comparative samples with the same carbon black contents, supporting the use of iron sand to improve damping. However, trends for energy absorption at around Tg were found to reverse which is considered to be due to the segmental motion of rubber chains being by far the most significant influence on energy absorption in the glass transition zone.