University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
15 results
Search Results
Item type:Publication, Collagen extraction from animal skin2022-06-13, MDPI AGCollagen is the most abundant structural protein in animals. It is the major component of skin. It finds uses in cosmetics, medicine, yarn production and packaging. This paper reviews the extraction of collagen from hides of most consumed animals for meat with the focus on literature published since 2000. The different pretreatment and extraction techniques that have been investigated for producing collagen from animal skins are reviewed. Pretreatment by enzymatic, acid or alkaline methods have been used. Extraction by chemical hydrolysis, salt solubilization, enzymatic hydrolysis, ultrasound assisted extraction and other methods are described. Post-extraction purification methods are also explained. This compilation will be useful for anyone wishing to use collagen as a resource and wanting to further improve the extraction and purification methods.Item type:Publication, Effect of stearic acid treatment on the properties of aligned short hemp fibre mats and their potential use as reinforcement in polypropylene matrix composites2021, SpringerThe main objective of this study was to assess the effect of stearic acid vapour treatment on hemp fibre mats produced using dynamic sheet forming, and the potential use of these treated mats as reinforcement in polypropylene matrix composites. Stearic acid was successfully applied through vapour treatment, appearing to form a layer on fibre surfaces. It was found that the presence of stearic acid increased hydrophobicity and thermal stability of fibre mats. It was also found to increase thermal stability of polypropylene matrix composites as well as their strength.Item type:Publication, Moisture sensitivity and compressive performance of 3D-printed cellulose-biopolyester foam lattices2021, ElsevierBiobased, foam-like polyester composite materials were 3D-printed from a thermoset paste formulation. This paste formulation was composed of sebacic acid, glycerol, citric acid, and cellulose nanocrystals in water and ethanol with potassium chloride as a salt porogen. Thin walls and lattices were 3D-printed with geometry selected to facilitate post-printing processes such as water removal during polyester curing and the post-curing removal of the salt porogen. The compressive performance of these moisture-sensitive lattice structures was investigated after conditioning at different humidity levels and by water immersion. Finite element analysis was used to simulate the compressive performance of these porous lattice structures using a crushable foam material model. Addition of plant triglyceride oils from sunflower and coconut were trialled to modify the compressive performance and moisture sensitivity. Addition of 5 wt% coconut oil to the formulation prior to 3D-printing was found to lower the cured material’s stiffness under dry conditions while increasing the compressive plateau strength of the lattice structures after water immersion.Item type:Publication, Alkali treatment of hemp fibres for the production of aligned hemp fibre mats for composite reinforcement2020, SpringerThe main objective of this study was to produce aligned hemp fibre mats from high strength hemp fibres using dynamic sheet forming (DSF). Alkali treatment of hemp fibre was carried out at ambient and high temperature to separate fibres. Single fibre tensile testing was used to assess the tensile properties of the fibres. It was found that the highest tensile properties were exhibited by high temperature treated fibre, whereas the tensile properties exhibited by ambient temperature treated fibre were lower than for untreated fibre. It was also found that fibre granulated after high temperature treatment, was better separated than that granulated before high temperature treatment. This well-separated fibre could successfully be formed into mats using DSF. The orientation of the formed mat was analysed using ImageJ (NIH, USA) software by which the potential of DSF to produce aligned hemp fibre mat was supported. The tensile properties of composite reinforced by these aligned hemp fibre mats were assessed.Item type:Publication, Comparison of strength and Young modulus of aligned discontinuous fibre PLA composites obtained experimentally and from theoretical prediction models2019, ElsevierThe present paper describes work carried out to compare the strength performance of PLA reinforced aligned discontinuous harakeke and hemp fibre mat composites evaluated experimentally and using various simple elastic mathematical prediction models. Fibre mats were produced by means of Dynamic Sheet Former (DSF), and stacked alternately with PLA sheets to produce composites with up to 40 wt% fibre content. The fibre content was increased from 5 wt% to 40 wt% using 5 wt% interval. In this work, both harakeke and hemp composites were manufactured using hot-press. It was found that, better agreement to the experiment was obtained for Young’s modulus compared to those composite strengths. The Modified Rule of Mixtures is found to give accuracy within 41% for strength, while the Cox model showing the best agreement (<10%) for Young’s modulus for fibre contents up to 25 wt%. Better agreement obtained for Young’s modulus is believed to due to less mechanism involved at where Young’s modulus is measured.Item type:Publication, Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites2019, SpringerIn this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.Item type:Publication, Manufacturing and characterization of sustainable hybrid composites using sisal and hemp fibres as reinforcement of poly (lactic acid) via injection moulding2019, Elsevier Science BVNatural polymers based composites offers significant advantages over synthetic fibre reinforced petroleum matrix based composites with regard to biodegradability, biocompatibility, design flexibility and sustainability. This work reports for the first time manufacturing of hybrid fibre reinforced biodegradable composites using sisal and hemp fibre with polylactic acid employing melt processing and injection moulding techniques. Granulated sisal and hemp fibres were blended and hybrid composites were manufactured using aliphatic polyester made up of lactic acid (PLA) through extrusion and injection moulding and their performance was evaluated. Experimental results revealed that density, elongation at break and water absorption capacity of hybrid composites were 1.14 ± 0.07 g/cm³, 0.93 ± 0.35% and 1.06 ± 0.18% respectively. The achieved mean tensile strength (46.25 ± 6.75 MPa), Young’s modulus (6.1 ± 0.58 GPa) and specific tensile strength (38.86 ± 5.0) of hybrid fibre reinforced PLA composites were improved compared to neat PLA. The flexural strength (94.83 ± 11.21 MPa), flexural modulus (6.04 ± 0.55 GPA) and specific flexural strength (79.76 ± 8.80) of hybrid fibre composites also showed better performance than those of neat PLA. Incorporation of sisal and hemp fibre with polylactide remarkably increased the impact strength of composites. Overall, the hybrid composites demonstrated good performance suggesting that they have great potential for use as an environmentally friendly alternative material in automotive, packaging, electronics, interiors and agricultural applications.Item type:Publication, A review on the use of Hydroxyapatite-carbonaceous structure composites in bone replacement materials for strengthening purposes2018, MDPIBiomedical materials constitute a vast scientific research field, which is devoted to producing medical devices which aid in enhancing human life. In this field, there is an enormous demand for long-lasting implants and bone substitutes that avoid rejection issues whilst providing favourable bioactivity, osteoconductivity and robust mechanical properties. Hydroxyapatite (HAp)-based biomaterials possess a close chemical resemblance to the mineral phase of bone, which give rise to their excellent biocompatibility, so allowing for them to serve the purpose of a bone-substituting and osteoconductive scaffold. The biodegradability of HAp is low (Ksp ≈ 6.62 × 10⁻¹²⁶) as compared to other calcium phosphates materials, however they are known for their ability to develop bone-like apatite coatings on their surface for enhanced bone bonding. Despite its favourable bone regeneration properties, restrictions on the use of pure HAp ceramics in high load-bearing applications exist due to its inherently low mechanical properties (including low strength and fracture toughness, and poor wear resistance). Recent innovations in the field of bio-composites and nanoscience have reignited the investigation of utilising different carbonaceous materials for enhancing the mechanical properties of composites, including HAp-based bio-composites. Researchers have preferred carbonaceous materials with hydroxyapatite due to their inherent biocompatibility and good structural properties. It has been demonstrated that different structures of carbonaceous material can be used to improve the fracture toughness of HAp, as they can easily serve the purpose of being a second phase reinforcement, with the resulting composite still being a biocompatible material. Nanostructured carbonaceous structures, especially those in the form of fibres and sheets, were found to be very effective in increasing the fracture toughness values of HAp. Minor addition of CNTs (3 wt.%) has resulted in a more than 200% increase in fracture toughness of hydroxyapatite-nanorods/CNTs made using spark plasma sintering. This paper presents a current review of the research field of using different carbonaceous materials composited with hydroxyapatite with the intent being to produce high performance biomedically targeted materials.Item type:Publication, Fibre orientation of novel dynamically sheet formed discontinuous natural fibre PLA composites2016, ElsevierThis paper describes work carried out to fabricate and to assess the fibre orientation in PLA reinforced by aligned discontinuous harakeke and hemp fibre mats produced using a dynamic sheet former (DSF). These mats were combined with PLA sheets to make composites with fibre contents of 5–40 wt% using a hot press. It was found that the fibre orientation factors (Kθ) for both harakeke and hemp fibre composites were higher than those values seen in the literature for composites prepared using injection moulding and hot pressed using randomly oriented fibre mats, but slightly lower than the highest values obtained with aligned fibre nonwoven preform composites utilising more processing stages. The highest Kθ values for harakeke and hemp fibres in this work were found to be 0.58 and 0.44 respectively. Kθ decreased, reflecting increased fibre misalignment as fibre content increased, believed to be due to fibre agglomeration and the higher pressure required during processing.Item type:Publication, Preparation and mechanical properties of novel bio-composite made of dynamically sheet formed discontinuous harakeke and hemp fibre mat reinforced PLA composites for structural applications2016-06-01, Elsevier Science BvThe objective of this study was to fabricate and assess the structure and mechanical performance of PLA reinforced by aligned discontinuous alkali treated natural fibre mats. The novel aspect of this work was in terms of composite processing, in particular, the use of fibre mats produced using a dynamic sheet former (DSF) wherein discontinuous treated fibres were aligned. Composites with different fibre weight contents were assessed using optical microscopy, scanning electron microscopy (SEM) and tensile testing. It was found that the fibres had a reasonable degree of alignment parallel to the DSF rotation direction together with good fibre dispersion. Tensile strengths of harakeke and hemp composites up to 101.6 MPa and to 87.3 MPa were achieved, approximately 90 and 60% higher respectively than PLA (53.9 MPa). It was also found that minimum and critical fibre volume fractions for harakeke and hemp fibre composites were lower than that found for injection moulded composites, due to better reinforcement efficiency obtained as a result of increased fibre alignment.