University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
11 results
Search Results
Item type:Publication, Effect of stearic acid treatment on the properties of aligned short hemp fibre mats and their potential use as reinforcement in polypropylene matrix composites2021, SpringerThe main objective of this study was to assess the effect of stearic acid vapour treatment on hemp fibre mats produced using dynamic sheet forming, and the potential use of these treated mats as reinforcement in polypropylene matrix composites. Stearic acid was successfully applied through vapour treatment, appearing to form a layer on fibre surfaces. It was found that the presence of stearic acid increased hydrophobicity and thermal stability of fibre mats. It was also found to increase thermal stability of polypropylene matrix composites as well as their strength.Item type:Publication, Moisture sensitivity and compressive performance of 3D-printed cellulose-biopolyester foam lattices2021, ElsevierBiobased, foam-like polyester composite materials were 3D-printed from a thermoset paste formulation. This paste formulation was composed of sebacic acid, glycerol, citric acid, and cellulose nanocrystals in water and ethanol with potassium chloride as a salt porogen. Thin walls and lattices were 3D-printed with geometry selected to facilitate post-printing processes such as water removal during polyester curing and the post-curing removal of the salt porogen. The compressive performance of these moisture-sensitive lattice structures was investigated after conditioning at different humidity levels and by water immersion. Finite element analysis was used to simulate the compressive performance of these porous lattice structures using a crushable foam material model. Addition of plant triglyceride oils from sunflower and coconut were trialled to modify the compressive performance and moisture sensitivity. Addition of 5 wt% coconut oil to the formulation prior to 3D-printing was found to lower the cured material’s stiffness under dry conditions while increasing the compressive plateau strength of the lattice structures after water immersion.Item type:Publication, Alkali treatment of hemp fibres for the production of aligned hemp fibre mats for composite reinforcement2020, SpringerThe main objective of this study was to produce aligned hemp fibre mats from high strength hemp fibres using dynamic sheet forming (DSF). Alkali treatment of hemp fibre was carried out at ambient and high temperature to separate fibres. Single fibre tensile testing was used to assess the tensile properties of the fibres. It was found that the highest tensile properties were exhibited by high temperature treated fibre, whereas the tensile properties exhibited by ambient temperature treated fibre were lower than for untreated fibre. It was also found that fibre granulated after high temperature treatment, was better separated than that granulated before high temperature treatment. This well-separated fibre could successfully be formed into mats using DSF. The orientation of the formed mat was analysed using ImageJ (NIH, USA) software by which the potential of DSF to produce aligned hemp fibre mat was supported. The tensile properties of composite reinforced by these aligned hemp fibre mats were assessed.Item type:Publication, Comparison of strength and Young modulus of aligned discontinuous fibre PLA composites obtained experimentally and from theoretical prediction models2019, ElsevierThe present paper describes work carried out to compare the strength performance of PLA reinforced aligned discontinuous harakeke and hemp fibre mat composites evaluated experimentally and using various simple elastic mathematical prediction models. Fibre mats were produced by means of Dynamic Sheet Former (DSF), and stacked alternately with PLA sheets to produce composites with up to 40 wt% fibre content. The fibre content was increased from 5 wt% to 40 wt% using 5 wt% interval. In this work, both harakeke and hemp composites were manufactured using hot-press. It was found that, better agreement to the experiment was obtained for Young’s modulus compared to those composite strengths. The Modified Rule of Mixtures is found to give accuracy within 41% for strength, while the Cox model showing the best agreement (<10%) for Young’s modulus for fibre contents up to 25 wt%. Better agreement obtained for Young’s modulus is believed to due to less mechanism involved at where Young’s modulus is measured.Item type:Publication, Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites2019, SpringerIn this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.Item type:Publication, A review on the use of Hydroxyapatite-carbonaceous structure composites in bone replacement materials for strengthening purposes2018, MDPIBiomedical materials constitute a vast scientific research field, which is devoted to producing medical devices which aid in enhancing human life. In this field, there is an enormous demand for long-lasting implants and bone substitutes that avoid rejection issues whilst providing favourable bioactivity, osteoconductivity and robust mechanical properties. Hydroxyapatite (HAp)-based biomaterials possess a close chemical resemblance to the mineral phase of bone, which give rise to their excellent biocompatibility, so allowing for them to serve the purpose of a bone-substituting and osteoconductive scaffold. The biodegradability of HAp is low (Ksp ≈ 6.62 × 10⁻¹²⁶) as compared to other calcium phosphates materials, however they are known for their ability to develop bone-like apatite coatings on their surface for enhanced bone bonding. Despite its favourable bone regeneration properties, restrictions on the use of pure HAp ceramics in high load-bearing applications exist due to its inherently low mechanical properties (including low strength and fracture toughness, and poor wear resistance). Recent innovations in the field of bio-composites and nanoscience have reignited the investigation of utilising different carbonaceous materials for enhancing the mechanical properties of composites, including HAp-based bio-composites. Researchers have preferred carbonaceous materials with hydroxyapatite due to their inherent biocompatibility and good structural properties. It has been demonstrated that different structures of carbonaceous material can be used to improve the fracture toughness of HAp, as they can easily serve the purpose of being a second phase reinforcement, with the resulting composite still being a biocompatible material. Nanostructured carbonaceous structures, especially those in the form of fibres and sheets, were found to be very effective in increasing the fracture toughness values of HAp. Minor addition of CNTs (3 wt.%) has resulted in a more than 200% increase in fracture toughness of hydroxyapatite-nanorods/CNTs made using spark plasma sintering. This paper presents a current review of the research field of using different carbonaceous materials composited with hydroxyapatite with the intent being to produce high performance biomedically targeted materials.Item type:Publication, Fibre orientation of novel dynamically sheet formed discontinuous natural fibre PLA composites2016, ElsevierThis paper describes work carried out to fabricate and to assess the fibre orientation in PLA reinforced by aligned discontinuous harakeke and hemp fibre mats produced using a dynamic sheet former (DSF). These mats were combined with PLA sheets to make composites with fibre contents of 5–40 wt% using a hot press. It was found that the fibre orientation factors (Kθ) for both harakeke and hemp fibre composites were higher than those values seen in the literature for composites prepared using injection moulding and hot pressed using randomly oriented fibre mats, but slightly lower than the highest values obtained with aligned fibre nonwoven preform composites utilising more processing stages. The highest Kθ values for harakeke and hemp fibres in this work were found to be 0.58 and 0.44 respectively. Kθ decreased, reflecting increased fibre misalignment as fibre content increased, believed to be due to fibre agglomeration and the higher pressure required during processing.Item type:Publication, The effect of silane coupling agent on iron sand for use in magnetorheological elastomers Part 1: Surface chemical modification and characterization2015-01-01, ElsevierBis-(3-triethoxysilylpropyl) tetrasulphane (TESPT) was employed for surface modification of iron sand for use in magnetorheological elastomers (MREs). The amount of TESPT was varied at five levels (2, 4, 6, 8 and 10 wt%) relative to iron sand content to assess the optimum amount of coupling agent for interfacial bonding and damping performance. Evidence that coupling had occurred between iron sand and TESPT was identified by Raman Spectroscopy and the grafting percentage was determined by thermogravimetric analysis. Subsequently, isotropic MREs containing unmodified and modified iron sand particles and natural rubber were prepared. Crosslink density assessment by swelling testing provided evidence that the tetrasulphane group of TESPT formed crosslinks with the rubber chains. The results exhibited the advantages of TESPT as a coupling agent between iron sand particles and rubber and also revealed that 6% TESPT content produced the highest crosslink density. The effects of the amount of TESPT on dynamic mechanical properties the morphological characteristics of the MREs were also investigated.Item type:Publication, Comparison of dynamic properties of magnetorheological elastomers with existing antivibration rubbers2015-12-15, ElsevierTan δ and energy dissipated during hysteresis testing of isotropic and anisotropic MREs containing silane modified iron sand particles in a natural rubber matrix were compared with existing antivibration rubbers. Tan δ was measured using dynamic mechanical analysis (DMA) over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100–50 °C). Energy dissipated was measured using a universal tester under cyclic tensile loading. The chosen antivibration rubbers for comparison contained different contents of carbon black filler (30, 50 and 70 phr) in a natural rubber matrix. It was found that energy absorption for comparative samples was generally higher than isotropic and anisotropic MREs over the range of frequency and strain amplitude explored, as well as in hysteresis testing and this was believed to be largely due the presence of carbon black in the formulation. Further assessment was carried out on materials that were the same as anisotropic MREs except they had additions of carbon black. The energy absorption was found higher than comparative samples with the same carbon black contents, supporting the use of iron sand to improve damping. However, trends for energy absorption at around Tg were found to reverse which is considered to be due to the segmental motion of rubber chains being by far the most significant influence on energy absorption in the glass transition zone.Item type:Publication, Mode I and Mode II interlaminar fracture toughness of composite laminates interleaved with electrospun nanofibre veils2015-05-01, ElsevierIn this study, the effects of interleaved nanofibre veils on the Mode I and Mode II interlaminar fracture toughness (ILFT) of autoclave cured unidirectional carbon/epoxy composite laminates were investigated. Various electrospun nanofibre veils consisting of a range of different polymer types, fibre diameters and veil architectures were placed in the laminate mid-planes, which were subsequently subjected to double cantilever beam and end-notch flexure tests. It was found that the polymer type and veil areal weight were the most important factors contributing to laminate performance. A 4.5 g/m2 PA66 veil provided the best all-round performance with fracture toughness improvements of 156% and 69% for Mode I and Mode II, respectively.