University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, Flexural properties of hemp fibre reinforced polylactide and unsaturated polyester composites2011, ElsevierIn this work, flexural strength and flexural modulus of chemically treated random short and aligned long hemp fibre reinforced polylactide and unsaturated polyester composites were investigated over a range of fibre content (0–50 wt%). Flexural strength of the composites was found to decrease with increased fibre content; however, flexural modulus increased with increased fibre content. The reason for this decrease in flexural strength was found to be due to fibre defects (i.e. kinks) which could induce stress concentration points in the composites during flexural test, accordingly flexural strength decreased. Alkali and silane fibre treatments were found to improve flexural strength and flexural modulus which could be due to enhanced fibre/matrix adhesion.Item type:Publication, Effect of fibre treatments on interfacial shear strength of hemp fibre reinforced polylactide and unsaturated polyester composites2011, ElsevierSurface treatment of hemp fibres was investigated as a means of improving interfacial shear strength (IFSS) of hemp fibre reinforced polylactide (PLA) and unsaturated polyester (UPE) composites. Fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane. A combined treatment using sodium hydroxide and silane was also carried out. IFSS of PLA/hemp fibre samples increased after treatment, except in the case of maleic anhydride treatment. Increased IFSS could be explained by better bonding of PLA with treated fibres and increased PLA transcrystallinity. The highest IFSS was 11.4 MPa which was obtained for the PLA/alkali treated fibre samples. IFSS of UPE/hemp fibre samples increased for all treated fibres. This is believed to be due to the improvement of chemical bonding between the treated fibres and the UPE as supported by FT-IR results. The highest IFSS (20.3 MPa) was found for the combined sodium hydroxide and silane treatment fibre/UPE samples.Item type:Publication, Effect of various chemical treatments on the fibre structure and tensile properties of industrial hemp fibres2011, ELSEVIER SCI LTDIndustrial hemp fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane to investigate the influence of treatment on the fibre structure and tensile properties. It was observed that the average tensile strength of sodium hydroxide treated fibres slightly increased compared with that of untreated fibres, which was believed to be as a result of increased cellulose crystallinity. The average tensile strength of acetic anhydride, maleic anhydride, silane and combined sodium hydroxide and silane treated fibres slightly decreased compared with that of untreated fibres, which was believed to be as a result of decreased cellulose crystallinity. However, the average Young’s modulus of all treated fibres increased compared with untreated fibres. This was considered to be as a result of densification of fibre cell walls due to the removal of non-cellulosic components during treatment.