<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 7 of 7
  • Item type:Publication,
    Discussions on grain refinement of magnesium alloys by carbon inoculation
    2005-03, Elsevier
    Carbon inoculation has no effect on magnesium alloys that do not contain aluminium. The hypothesis proposed in a recent article [Scripta Materialia 49 (2003) 1129] that segregation of carbon plays a major role in the grain refinement of magnesium alloys by carbon inoculation is inconsistent with many of the observed facts. The Al4C3 or Al–C–O hypothesis, which is supported by experimental observations, is still the most reasonable mechanism proposed to date for the grain refinement of magnesium alloys by carbon inoculation.
  • Item type:Publication,
    Effect of manganese on grain refinement of Mg–Al based alloys
    2006-06, Elsevier
    Manganese is a grain refiner for high purity Mg–3%Al, Mg–6%Al, Mg–9%Al, and commercial AZ31 (Mg–3%Al–1%Zn) alloys when introduced in the form of an Al–60%Mn master alloy splatter but the use of pure Mn flakes and ALTAB™ Mn75 tablets shows no grain refinement. Long time holding of the melt at 730 °C leads to an increase in grain size. The mechanism is attributed to the presence of an ε-AlMn phase (hexagonal close-packed) in the master alloy splatter.
  • Item type:Publication,
    Effect of iron on grain refinement of high-purity Mg–Al alloys
    2004-07, Elsevier Ltd
    The effect of iron on the grain refinement of high-purity Mg–3%Al and Mg–9%Al alloys has been investigated using anhydrous FeCl3 as an iron additive at 750 °C in carbon-free aluminium titanite crucibles. It was shown that grain refinement was readily achievable for both alloys. Fe- and Al-rich intermetallic particles were observed in many magnesium grains.
  • Item type:Publication,
    Grain coarsening of magnesium alloys by beryllium
    2004-10, Elsevier Ltd
    A trace of beryllium can lead to dramatic grain coarsening in Mg–Al alloys at normal cooling rates. It is, however, unclear whether this effect applies to aluminium-free magnesium alloys or not. This work shows that a trace of beryllium also causes considerable grain coarsening in Mg–Zn, Mg–Ca, Mg–Ce and Mg–Nd alloys and hinders grain refinement of magnesium alloys by zirconium as well.
  • Item type:Publication,
    Mechanism for grain refinement of magnesium alloys by superheating
    2007-04, Elsevier
    The mechanisms for grain refinement of magnesium alloys by superheating have remained ambiguous since 1931. A model has been proposed on the basis of the recent understanding of the grain refinement of both high purity and commercial purity Mg–Al alloys. The model explains most of the experimental observations about superheating. Analysis of the grain size data obtained from different Mg–Al alloys as a function of the growth restriction factor with and without superheating provides good support to the model.
  • Item type:Publication,
    Native grain refinement of magnesium alloys
    2005-10, Elsevier Ltd
    High purity Mg–Al type alloys have a naturally fine grain size compared to commercial purity alloys with the same basic composition. This is referred to as native grain refinement. It is shown that native grain refinement occurs only in magnesium alloys containing aluminium. The mechanism is attributed to the Al4C3 particles existing in these alloys.
  • Item type:Publication,
    Uptake of iron and its effect on grain refinement of pure magnesium by zirconium
    2004-05, Maney Publishing
    The uptake of iron by molten magnesium from uncoated new mild steel crucibles at temperatures 680°C, 730°C, and 780°C has been investigated. It was shown that the uptake of iron was sluggish at 680°C and the use of 0.05% zirconium addition could effectively suppress the increase in iron content within the first 2 h of holding at temperature. Rapid and severe uptake of iron was observed at 780°C. As a consequence, it was found that the grain refinement of pure magnesium achieved by 1% zirconium addition nearly vanished after 60 min hold at 780°C due to the depletion of soluble zirconium. The uptake of iron at 730°C was conspicuous but it was still controllable by use of 0.05% zirconium addition within the first 60 min of holding at temperature. The work conducted using an aluminium titanite crucible and a boron nitride coated mild steel crucible at 730°C further confirmed the highly detrimental influence of the uptake of iron on the grain refinement of pure magnesium by zirconium. The characteristic zirconium rich coring structures developed from circular to rosette like when the melt was held at 730°C in an uncoated mild steel crucible, while no such evolution was observed when held in an aluminium titanite crucible at the same temperature. Recommendations to minimise the consumption of zirconium by the uptake of iron were made based on the results obtained from this investigation. The mechanism of grain refinement of magnesium by a low concentration of zirconium is discussed.