University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
8 results
Search Results
Item type:Publication, Investigation of a discus-milling process using a powder mixture of Al and TiO₂2006, SpringerIn this study, a powder mixture of Al and TiO₂ was employed to investigate the milling process in a discus mill. In this first report on this novel mechanical mill, several variables, including the milling time and powder charge and their effects on the microstructural evolution of powder particles, are monitored and studied. The study reveals that the dominant parameters of the milling process are the milling time and the starting powder charge, similar to the other high-energy ball-milling processes. The longer the milling time and the smaller the starting powder charge, the more homogeneous the mixing and the finer the microstructure of the powder particles. The reaction between Al and TiO₂ was not observed with a milling period as long as 6 hours, for the present materials. However, the reaction between Al and TiO₂, during the subsequent heat treatment, is influenced by the milling condition. The powders with the longer milling times and finer mixing microstructures also form a finer microstructure, after the reaction between Al and TiO₂ during heat treatment. The methods for achieving an optimal milling efficiency for the Al- TiO₂ system are discussed.Item type:Publication, Tensile properties of Ti-6Al-4V discs produced by open die powder compact forging of pre-alloyed HDH powders2012, Trans Tech PublicationsOpen die powder compact forging was employed for consolidation of Ti-6Al-4V(wt.%) powders which were produced by a hydride-dehydride (HDH) process. The powders were initially warm-compacted into cylindrical shapes. Induction heating was used for preheating the compacts prior to forging into plates. The effect of the forging parameters such as temperature and pre-sintering time on the microstructure and tensile properties of the forged plates were studied. Porosity and the alpha-beta phase distribution were investigated to enable a better understanding of their effect on the fracture behaviour of the tensile tested specimens. The fracture surfaces of the broken tensile specimens were analysed using Scanning Electron Microscopy (SEM) to find the correlation between microstructure, residual porosity and fracture behaviour. A combination of high ultimate tensile strength of over 1200MPa and a good ductility reflected by an elongation to fracture of around 10% was achieved in some of the forged discs.Item type:Publication, A study of polyvinyl butyryl based binder system in titanium based metal injection moulding2012, Trans Tech PublicationsMetal injection moulding (MIM) is an innovative injection moulding technique widely used to produce complex shaped components from feedstock composed of metal powders and thermosetting or thermoplastic binders. In MIM, binder selection and formulation are considered as critical processes since binder characteristics dictate the success of MIM. The purpose of this study is to determine the feasibility of polyvinyl butyryl (PVB) based binder system in Ti-6Al-4V(wt.%)/binder feedstock, as well as to understand the effects of key parameters, such as powder loading and mixing conditions on the rheological properties of a feedstock. In this study, PVB, polyethylene glycol (PEG), and stearic acid (SA) were chosen to formulate a multi-component binder system to prepare Ti-6Al-4V based feedstock with the aid of three types of mixers: a compounder, a modified mechanical mixer and a twin screw extruder. Further, morphological analysis was performed using optical microscopy and scanning electron microscopy. Thermal analysis was performed using simultaneous differential thermal analysis and thermogravimetric analysis. Results showed that binder formulation was reasonably successful with the aid of both mechanical mixer and a twin screw extruder under certain mixing conditions, and the critical powder loading was 68 vol.%, resulting in an optimum powder loading of 63 vol.%.Item type:Publication, Microstructural evolution during mechanical milling of Ti/Al powder mixture and production of intermetallic TiAl cathode target2011, SpringerTitanium aluminides are of great technological interest because of their attractive mechanical properties. Mechanical milling/alloying is a promising powder metallurgical technique, which can achieve ultrafine, uniform and manipulable microstructures. In this study, we employed a recently revisited discus mill to produce a composite Ti– (50–57) at.%Al powder feedstock, which is suitable for hot consolidation to produce bulk cathode targets for physical vapour deposition (PVD) coatings. The effects of milling time, quantity of process control agent (PCA) and discus-topowder weight ratio (DPR) on the microstructure evolution of the attendant Ti/Al composite powder were investigated in detail. It was found that to produce Ti/Al composite powders with a fine particle size and a uniform microstructure, the practicable processing parameters should be 2 or 3% isopropanol addition as PCA, 12 h of milling time and at least 13:1 DPR weight ratio. Cathode targets were produced by hot isostatic pressing (HIPing) the as-milled powders. The targets were then used to produce a PVD TiAlN coating which had an average microhardness of 2400 HV.Item type:Publication, Tensile Properties and Fracture Behaviour of Induction Sintered Ti and Ti-6Al-4V (wt %) Powder Compacts2011, Trans Tech PublicationsInduction heating of powder compacts could be a very effective method for metal powder consolidation to get the final product or as an intermediate consolidation step to produce feedstock for metal powder forging or extrusion. Our study has proven that only a few minutes of induction heating, of Ti and Ti-6Al-4V (wt %) powder compacts, increases their density dramatically and causes a significant sintering effect, as evidenced by the formation of interparticle diffusion bonding and reflected by the tensile properties of the induction sintered powder compacts. This paper presents and discusses the results of a study on the tensile properties and fracture behaviour of the Ti and Ti-6Al-4V powder compacts sintered under a variety of induction heating conditions. Keywords: Titanium alloys, powder consolidation, powder compact sintering, induction heating.Item type:Publication, Mechanical behaviour of Titanium, Ti-6Al-4V (wt %) alloy and Ti-47Al-2Cr (at %) alloy produced using powder compact forging2011, Trans Tech PublicationsPowder compact forging was used to produce bulk consolidated titanium and Ti-6Al-4V (wt %) and Ti-47Al-2Cr (at%) alloy disks from hydrogenated and dehydrogenated (HDH) and gas atomised powders (GA) powders (in the case of titanium and Ti-6Al-4V) and a mechanically milled powder (in the case of Ti-47Al-2Cr alloy). The bulk titanium and Ti-6Al-4V (wt %) alloy have been produced by forging of the powder compacts. The Ti-47Al-2Cr (at %) alloy was produced using canned powder compact forging of a Ti/Al/Cr composite powder. The purpose of the present study is to investigate the deformation and fracture behaviour of the bulk consolidated as-forged materials, by conducting tensile testing at room temperature (RT) and examination of the fractured specimens which had near-α, α + β and γ phase structures, respectively. It was found that as-forged bulk titanium disk produced using HDH powder showed a yield point with a yield strength of ~700 MPa and with a considerable amount of ductility. While the as-forged Ti-6Al-4V (wt %) alloy produced using HDH powder, fractured prematurely without any yielding. On the other hand yielding was observed in the as-forged Ti-6Al-4V (wt %) alloy produced using GA powder, showing a yield strength of ~970 MPa and a considerable amount of plastic strain to fracture. The bulk consolidated Ti-47Al-2Cr (at %) alloy also fractured prematurely with fracture strength of ~125 MPa. The mechanical behaviour of the as-forged bulk materials was found to be dependent on several factors such as initial powders used, green density of the powder compact, forging parameters used during forging. It was expected that the entrapped gas in green compacts, absorbed oxygen, porosity and inter-particle bonding play an important role on the quality of the as-forged material, which in turn affected the mechanical behaviour of the bulk material.Item type:Publication, Effect of milling parameters on microstructure of Ti/Al composite powder produced by discus milling2006, World Scientific Publishing CoThe motivation of this research is to develop a process for producing Ti/Al composite powders that enable synthesis of a single-phase TiAl intermetallic bulk material, which is then used as a target for physical vapour deposition (PVD) coating. This study reports the effects of milling time, amount of process control agent (PCA) added as well as the powder-to-medium ratio on the microstructure of the Ti/Al composite powder. Optical microscopy and scanning electron microscopy (SEM) were used to evaluate the level of mixing and the resulting powder particle size. X-ray diffraction analysis and differential thermal analysis were used for determining the phase constituents and the solid state reaction temperature of the as-milled powders.Item type:Publication, Fabrication of TiAl target by mechanical alloying and applications in physical vapour deposition coating2007, Trans Tech Publications LtdThe research involves the development of a powder metallurgical route for producing good quality TiAl targets for making physical vapour deposition (PVD) coatings. Mixtures of elemental titanium and aluminium powders were mechanically milled using a novel discus milling technique under various conditions. Hot isostatic pressing (HIP) was then employed for consolidation of the mechanically alloyed powders. A cathodic arc vapour deposition process was applied to produce a TiAIN coating. A microstructural examination was conducted on the target material and PVD coatings, using X-ray diffractometry (XRD), X-ray photoelectron spectrometry (XPS) and scanning electron microscopy (SEM). It has been found that combining mechanical alloying and HIP enable us to produce a fairly good quality of TiAl based target. The PVD coatings obtained from the TiAl target showed very high microhardness values.