  • Item type:Publication,
    On microstructural evolution and mechanical properties of Ti-5Al-5V-5Mo-3Cr alloy synthesised from elemental powder mixtures
    2018, Elsevier
    In this paper, we explored to prepare a multi-compositional titanium alloy, Ti-5Al-5V-5Mo-3Cr (Ti-5553), by powder compact extrusion from elemental powder mixtures, and investigate the microstructure variation during the synthesising process and after post heat treatments and the changes of mechanical properties. XRD, OM and SEM were used to analyse the phase constitutions and microstructures of the Ti-5553 alloy at different processing conditions, and tensile tests were conducted to examine their mechanical properties. The results showed that a homogeneous Ti-5553 alloy was successfully produced by powder compact extrusion from the powder mixtures, β phase was mainly contained in the hot-pressed and 1200°C-extruded Ti-5553 alloy and had an equiaxed microstructure. Different types of α phase precipitated from the β matrix after heat treatment, and this significantly changed the microstructures and improved the mechanical properties of the extruded Ti-5553 alloy, with yield strength of 1250 MPa and ultimate strength of 1300 MPa for the alloy treated at 675 °C for 2 h, and the ductility of about 6.1% for the alloy treated at 780 °C for 2 h.
  • Item type:Publication,
    Mechanical behaviour of Titanium, Ti-6Al-4V (wt %) alloy and Ti-47Al-2Cr (at %) alloy produced using powder compact forging
    2011, Trans Tech Publications
    Powder compact forging was used to produce bulk consolidated titanium and Ti-6Al-4V (wt %) and Ti-47Al-2Cr (at%) alloy disks from hydrogenated and dehydrogenated (HDH) and gas atomised powders (GA) powders (in the case of titanium and Ti-6Al-4V) and a mechanically milled powder (in the case of Ti-47Al-2Cr alloy). The bulk titanium and Ti-6Al-4V (wt %) alloy have been produced by forging of the powder compacts. The Ti-47Al-2Cr (at %) alloy was produced using canned powder compact forging of a Ti/Al/Cr composite powder. The purpose of the present study is to investigate the deformation and fracture behaviour of the bulk consolidated as-forged materials, by conducting tensile testing at room temperature (RT) and examination of the fractured specimens which had near-α, α + β and γ phase structures, respectively. It was found that as-forged bulk titanium disk produced using HDH powder showed a yield point with a yield strength of ~700 MPa and with a considerable amount of ductility. While the as-forged Ti-6Al-4V (wt %) alloy produced using HDH powder, fractured prematurely without any yielding. On the other hand yielding was observed in the as-forged Ti-6Al-4V (wt %) alloy produced using GA powder, showing a yield strength of ~970 MPa and a considerable amount of plastic strain to fracture. The bulk consolidated Ti-47Al-2Cr (at %) alloy also fractured prematurely with fracture strength of ~125 MPa. The mechanical behaviour of the as-forged bulk materials was found to be dependent on several factors such as initial powders used, green density of the powder compact, forging parameters used during forging. It was expected that the entrapped gas in green compacts, absorbed oxygen, porosity and inter-particle bonding play an important role on the quality of the as-forged material, which in turn affected the mechanical behaviour of the bulk material.