Now showing 1 - 10 of 18
  • Item type:Publication,
    On the processing of a powder metallurgy low-cost Ti alloy via different induction sintering strategies
    2026, MDPI
    Reducing the cost of Ti alloys, both from a processing and compositional point of view, is a pathway forward for harnessing more extensively the industrial and environmental benefits associated with their uses, and it is an outstanding manufacturing challenge. Thus, this study investigated the manufacturing of a low-cost Ti alloy using different induction sintering strategies where both aspects are designed to reduce the final cost. The primary conclusion is that induction sintering of Ti alloys by cycling the temperature above and below the allotropic phase transformation (i.e., beta transus) suffices for the need for high green density values, which are commonly achieved using more expensive methods. This is due to faster densification kinetics. The fast uniform heating of the alloys leads to homogenous pore distribution in the entire volume and the dissolution of the alloying elements, especially during cycling sintering due to the fine particle size of the alloying elements. Consequently, despite the low homologous sintering temperatures used, the induction sintered low-cost Ti alloys do not fail catastrophically, although the ability to sustain plastic deformation is affected by the features of the residual porosity.
  • Item type:Publication,
    Strengthening mechanisms of Ti via Al addition
    2020, Elsevier
    Pure Ti is characterised by an interesting combination of performance from an engineering point of view. The addition of Al to Ti can be used to reduce the intrinsic cost of the material, decrease the density of the alloy, and increase the mechanical performance. This study is focused on evaluating the physical properties, microstructural evolution and mechanical behaviour of Ti-xAl alloys (where x = 1–6 wt%) in order to scientifically understand the strengthening mechanisms of the addition of Al to pure Ti manufactured via the conventional powder metallurgy route of cold uniaxial pressing plus solid state sintering. The addition of Al to Ti does not affect the compressibility of the alloy but changes the consolidation and densification of the alloy. The incremental addition of Al results in the progressive strengthening of Ti via the simultaneous contribution from substitutional solid solution and grain refinement strengthening which outdo the negative effect of the residual porosity.
  • Item type:Publication,
    Yield of cyclic vs heat-and-hold induction sintering on the mechanical behaviour of the low-cost Ti-5Fe alloy
    2025-06, Elsevier BV
    The high cost of Ti alloys is hindering their industrial implementation and, therefore, the quest for low-cost Ti alloys entails lowering the intrinsic cost using cheaper alloying elements and developing more efficient manufacturing methods. In this study, the yield of manufacturing the novel low-cost Ti-5Fe alloy via heat-and-hold and cyclic induction sintering around the allotropic α→β phase transformation was compared as the latter is expected to enhance densification. It is demonstrated that induction sintering is extremely efficient due to its characteristic high heating rates and simultaneously permits to obtain homogenous chemical compositions at low homologous sintering temperatures. Cyclic sintering yields faster sintering kinetics, which results in higher densification with respect to heat-and-hold, achieving uniform residual porosity distributions within the microstructure, comparable relative density, and on average smaller and more spherical pores. Consequently, higher strength but not necessarily higher ductility is obtained for the cyclic sintered Ti-5Fe alloy as the failure mode entails crack propagation through irregularly shaped pores.
  • Item type:Publication,
    Behavior of Different β Stabilizers on the Microstructure and Properties of Ternary Ti‐3Sn‐X Alloys
    2023, Wiley
    The manufacturing of Ti alloys via powder metallurgy and the development of novel compositions are two strategies to reduce the cost of Ti, which is still the primary factor deterring its wider use in engineering applications. In this study, new Ti alloys based on the combined addition of Sn with Nb, Mo, or Mn are manufactured via powder metallurgy to gain an understanding of the role of these β stabilizers on the performance achievable. It is found that the designed alloys have a fully homogeneous chemistry regardless of their actual composition and a lamellar or β‐type microstructure depending on the actual β stabilizer used. This study confirms that the β‐stabilizing power effect decreases from Mn to Mo and, eventually, Nb. The compressibility and sinterability of the alloys increase with the progressive addition of the selected powders, generally leading to stronger and more ductile materials. It is also found that the proposed Ti‐3Sn‐Mo alloys are characterized by the best strength/ductility pairs compared to a variety of sintered or cast binary/ternary Ti alloys bearing the alloying elements considered in this work.
  • Item type:Publication,
    Advancement in the pressureless sintering of CP titanium using high-frequency induction heating
    2019, Springer
    High-frequency induction heating is applied as an alternative heating source for pressureless sintering of commercially pure Ti powders, aiming to intensify the sintering process. The effects of the process parameters on the properties of the sintered material are systematically studied. The initial powder compact density is the most influential parameter permitting sintered structures with highly porous to almost fully dense appearance. Short heating time combined with sintering to temperatures just above the β-transus resulted in a strong diffusion bonding between the Ti powder particles, and grain growth is observed at the former boundaries of the neighboring powder particles. The dimpled appearance of the fracture surface at those regions confirmed the strong metallic interparticle bonding. Tensile properties comparable to those of Ti-Grade 3 and Ti-Grade 4 are achieved, which also demonstrates the efficiency of the induction sintering process. A mechanism explaining the fast and efficient sintering is proposed. The process has the added advantage of minimizing the oxygen pickup.
  • Item type:Publication,
    The effect of heat treatments on microstructure and mechanical properties of as-extruded Ti-6Al-4V alloy rod from blended elemental powders
    2018, Trans Tech Publications
    In this study, Ti-6Al-4V bars were first prepared by extrusion of powder compacts from blended powder mixtures in the beta phase region, then the as-extruded bars were heat-treated following four different conditions: beta quenching and aging (βQA), broken up structure (BUS) treatment, solution treatment and aging (STA) and recrystallization annealing (RA). The effect of the heat treatments on microstructure and mechanical properties was studied using optical microscopy, scanning electron microscopy, and mechanical test to determine which heat treatment condition has the greatest impact on the mechanical properties of the as-extruded Ti-6Al-4V alloy. The results show that the as-extruded condition has the best balance of strength (1120 MPa of UTS) and ductility (11% of elongation to failure). βQA and STA lead to a slight increase in strength but ductility decreases considerably. After BUS and RA treatments, both strength and ductility are reduced. The relationship between processing, microstructure and properties was studied, and their implications towards fatigue behaviour and fracture toughness discussed.
  • Item type:Publication,
    On microstructural evolution and mechanical properties of Ti-5Al-5V-5Mo-3Cr alloy synthesised from elemental powder mixtures
    2018, Elsevier
    In this paper, we explored to prepare a multi-compositional titanium alloy, Ti-5Al-5V-5Mo-3Cr (Ti-5553), by powder compact extrusion from elemental powder mixtures, and investigate the microstructure variation during the synthesising process and after post heat treatments and the changes of mechanical properties. XRD, OM and SEM were used to analyse the phase constitutions and microstructures of the Ti-5553 alloy at different processing conditions, and tensile tests were conducted to examine their mechanical properties. The results showed that a homogeneous Ti-5553 alloy was successfully produced by powder compact extrusion from the powder mixtures, β phase was mainly contained in the hot-pressed and 1200°C-extruded Ti-5553 alloy and had an equiaxed microstructure. Different types of α phase precipitated from the β matrix after heat treatment, and this significantly changed the microstructures and improved the mechanical properties of the extruded Ti-5553 alloy, with yield strength of 1250 MPa and ultimate strength of 1300 MPa for the alloy treated at 675 °C for 2 h, and the ductility of about 6.1% for the alloy treated at 780 °C for 2 h.
  • Item type:Publication,
    Producing High-Quality Titanium Alloy by a Cost-Effective Route Combining Fast Heating and Hot Processing
    2018, Springer
    Powder metallurgy is a very attractive method for producing titanium alloys, which can be near-net-shape formed and have freedom in composition selection. However, applications are still limited due to product affordability. In this paper, we will discuss a possible cost-effective route, combining fast heating and hot processing, to produce titanium alloys with similar or even better mechanical properties than that of ingot metallurgy titanium alloys. Two titanium alloys, Ti-5Al-5V-5Mo-3Cr (Ti-5553) and Ti-5Fe, were successfully produced from HDH titanium powder and other master alloy powders using the proposed processing route. The effect of the processing route on microstructural variation and mechanical properties have been discussed.
  • Item type:Publication,
    Effect of microwave sintering parameters on the physical and mechanical properties of pure Ti and blended elemental Ti alloys
    2018, Trans Tech Publications
    Microwave sintering (MWS) was used to consolidate hydride de-hydride Ti powder and blended elemental Ti6Al4V, Ti5Fe and Ti5Al5Mo5V3Cr (Ti5553) powder mixtures. The amount of powders used to prepare the powder compacts was scaled up to 500g.The effect of the MWS conditions on the relative density, porosity distribution, microstructure and tensile properties were studied. Furthermore, uniformity in distribution of the alloying elements was checked. For most of the materials considered, a combinations of sintering temperature of 1200ºC and 1300ºC and holding time of 5 to 30 min resulted in significantly improved density. Nevertheless sintering temperature of at least 1300ºC was required for pore coalescence and high tensile properties.
  • Item type:Publication,
    Development of low cost PM Ti alloys by thermomechanical processing of powder blends
    2016, Trans Tech Publications
    This research focuses on the development of low cost powder metallurgy (PM) Ti alloys suitable for application in PM thermomechanical processing with mechanical properties comparable to those of wrought Ti6Al4V alloy. The alloy systems studied are Ti3Al2V, Ti5Fe and Ti3.2Fe1Cr0.6Ni0.1Mo (Ti5SS). The alloy mixtures were produced by blending Ti HDH powders with Al40V, 316SS master alloy powders or elemental Fe powder. The blended powders were further consolidated using various methods: high vacuum sintering (HVS), induction sintering (IS), powder compact forging (PCF) and powder compact extrusion (PCE). It is found that, PM Ti3Al2V and Ti5Fe alloy processed by PCE or PCF followed by recrystallization annealing (RA) achieved tensile properties comparable with wrought Ti6Al4V alloy. Tensile properties such as yield strength (YS) of 910MPa, UTS of 1010MPa and 15% elongation to fracture for Ti3Al2V alloy are reported. Ti5Fe alloy gives YS and UTS of 870MPa and 968MPa respectively, combined with 20.3% elongation to fracture. The tensile results are related to the microstructure developed during the consolidation processes. The oxygen contamination as a result of the high temperature processing is also reported.