<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 3 of 3
  • Item type:Publication,
    Thermal shock properties of Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite coatings
    2011, Trans Tech Publications
    Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite coatings have a potential to reduce dissolution and aluminium soldering tendency of H13 tool steel used in the aluminium processing industry. The thermal shock resistance of H13 tool steel coated with Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite powders sprayed using a high velocity oxygen fuel (HVOF) technique was studied. The thermal shock behaviour of the composite coatings was investigated by subjecting the coated coupons to a number of cycles, each cycle consisting of a holding time of 30 seconds in molten aluminium at 700 ± 10 °C followed by quenching into water. The surfaces of the coupons were examined for Al soldering and an evaluation of surface spallation. Any cracks found in the coatings were studied to explain their thermal shock behaviour. The results of this study showed that both Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite coatings on H13 tool steel have good thermal shock resistance with a thermal shock life between 300 to 400 cycles. The composite coatings and fracture surfaces were analyzed using scanning electron microscopy.
  • Item type:Publication,
    The performance of thermally sprayed titanium based composite coatings in molten aluminium
    2011, Elsevier
    The service life of die and tool steels in contact with molten aluminium is important in the aluminium processing industry. This article describes an investigation of the efficiency of thermally sprayed Ti(Al,O)/Al₂O₃ and TiAl(O)/Al₂O₃ composite coatings in resisting aluminium soldering on H13 tool steel. The powder feedstocks for making the composite coatings were produced by high energy mechanical milling of a mixture of Al and TiO₂ powders using different molar ratios followed by a thermal reaction process. The feedstocks were then thermally sprayed using a high velocity oxygen fuel (HVOF) technique onto an H13 steel substrate to produce composite coatings. The performance of the coatings was assessed in terms of Al soldering and liquid metal corrosion resistance after immersing in molten aluminium at a temperature of 700 ± 10 °C. The results of this study showed that composite coatings have a potential to act as a physical barrier to prevent aluminium attack on H13 tool steel. The nature of Al attack on H13 tool steel changed from generalised to more localised attack with the thermally sprayed coating. A Ti(Al,O)/Al₂O₃ composite coating was not attacked by molten aluminium, however localised attack on a H13 tool steel substrate was found to be caused by molten metal penetration through defects in the coating. Composite coating TiAl(O)/Al₂O₃ was attacked by molten aluminium resulting in dissolution of the coating. Composite coatings showed significantly lower dissolution in molten aluminium compared with the uncoated H13 steel. A Ti(Al,O)/Al₂O₃ composite coating was found to be a more effective protective coating than a TiAl(O)/Al₂O₃ composite coating due its greater resistance to molten aluminium attack.
  • Item type:Publication,
    Tribological properties of thermally sprayed TiAl-Al₂O₃ composite coating
    2009, IOP Publishing
    The use of thermal spray coatings provides protection to the surfaces operating in severe environments. The main goal of the current work is to investigate the possibility of using a high velocity oxy fuel (HVOF) thermally sprayed wear resistant TiAl/Al2O3 coating on tool steel (H13) which is used for making dies for aluminium high pressure die casting. A feedstock of TiAl/Al2O3 composite powder was produced from a mixture of Al and TiO2 powders by high energy mechanical milling, followed by a thermal reaction process. The feedstock was then thermally sprayed using a high velocity oxy-fuel (HVOF) technique onto H13 steel substrates to produce a composite coating. The present study describes and compares the tribological properties such as friction and sliding wear rate of the coating both at room and high temperature (700°C). The results showed that the composite coating has lower wear rate at high temperature (700°C) than the uncoated H13 sample. At Room temperature without using lubricant there is no much significant difference between the wear rate of the coated and uncoated samples. The experimental results showed that the composite coating has great potential for high temperature application due to its lower wear rate at high temperature in comparison with the uncoated sample at the same temperature. The composite coating was characterized using scanning electron microscopy (SEM), optical microscopy and X-ray diffractometry (XRD). This paper reports the experimental observations and discusses the wear resistance performance of the coatings at room and high temperatures.