    Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites
    2019, Springer
    In this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.
  • Item type:Publication,
    Analysis of mechanical properties of hemp fibre reinforced unsaturated polyester composites
    2013, Sage
    Different chemically treated hemp fibre reinforced unsaturated polyester composites were investigated over a range of fibre content (0–60 wt%). Although Young’s modulus of all the short fibre reinforced unsaturated polyester composites was found to be higher than that of unreinforced unsaturated polyester; however, tensile strength of the composites exceeded that of the unsaturated polyester matrix only for the combined alkali- and silane-treated fibre composites at 40 wt% fibre content. The decrease in tensile strength of the composites could be attributed to stress concentrations caused by the fibres in conjunction with the brittle matrix. Impact strength of all the treated fibre composites was higher than that of the untreated fibre composites at all fibre contents. KIc and GIc of the composites decreased initially and thenincreased as the fibre content increased because more and more fibres being available to pull-out. The mechanical properties of the composites were increased further due to the alignment of long fibres.