<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 4 of 4
  • Item type:Publication,
    Hemp fibre reinforced poly(lactic acid) composites
    2007, Trans Tech Publications
    The potential of hemp fibre as a reinforcing material for Poly(lactic acid) (PLA) was investigated. Good interaction between hemp fibre and PLA resulted in increases of 100% for Young’s modulus and 30% for tensile strength of composites containing 30 wt% fibre. Different predictive ‘rule of mixtures’ models (e.g. Parallel, Series and Hirsch) were assessed regarding the dependence of tensile properties on fibre loading. Limited agreement with models was observed. Differential scanning calorimetry (DSC) and x-ray diffraction (XRD) studies showed that hemp fibre increased the degree of crystallinity in PLA composites.
  • Item type:Publication,
    Analysis of mechanical properties of hemp fibre reinforced unsaturated polyester composites
    2013, Sage
    Different chemically treated hemp fibre reinforced unsaturated polyester composites were investigated over a range of fibre content (0–60 wt%). Although Young’s modulus of all the short fibre reinforced unsaturated polyester composites was found to be higher than that of unreinforced unsaturated polyester; however, tensile strength of the composites exceeded that of the unsaturated polyester matrix only for the combined alkali- and silane-treated fibre composites at 40 wt% fibre content. The decrease in tensile strength of the composites could be attributed to stress concentrations caused by the fibres in conjunction with the brittle matrix. Impact strength of all the treated fibre composites was higher than that of the untreated fibre composites at all fibre contents. KIc and GIc of the composites decreased initially and thenincreased as the fibre content increased because more and more fibres being available to pull-out. The mechanical properties of the composites were increased further due to the alignment of long fibres.
  • Item type:Publication,
    Flexural properties of hemp fibre reinforced polylactide and unsaturated polyester composites
    2011, Elsevier
    In this work, flexural strength and flexural modulus of chemically treated random short and aligned long hemp fibre reinforced polylactide and unsaturated polyester composites were investigated over a range of fibre content (0–50 wt%). Flexural strength of the composites was found to decrease with increased fibre content; however, flexural modulus increased with increased fibre content. The reason for this decrease in flexural strength was found to be due to fibre defects (i.e. kinks) which could induce stress concentration points in the composites during flexural test, accordingly flexural strength decreased. Alkali and silane fibre treatments were found to improve flexural strength and flexural modulus which could be due to enhanced fibre/matrix adhesion.
  • Item type:Publication,
    Improvement of mechanical performance of industrial hemp fibre reinforced polylactide biocomposites
    2011-03, Elsevier
    In this work, mechanical properties of chemically treated random short fibre and aligned long hemp fibre reinforced PLA composites were investigated over a range of fibre content (0–40 wt.%). It was found that tensile strength, Young’s modulus and impact strength of short hemp fibre reinforced PLA composites increased with increased fibre content. Alkali and silane fibre treatments were found to improve tensile and impact properties which appears to be due to good fibre/matrix adhesion and increased matrix crystallinity. A 30 wt.% alkali treated fibre reinforced PLA composite (PLA/ALK) with a tensile strength of 75.5 MPa, Young’s modulus of 8.18 GPa and impact strength of 2.64 kJ/m2 was found to be the best. However, plane-strain fracture toughness and strain energy release rate decreased with increased fibre content. The mechanical properties of the PLA/ALK composites were increased further due to alignment of long fibres.