  • Item type:Publication,
    Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites
    2019, Springer
    In this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.
  • Item type:Publication,
    Hemp fibre reinforced poly(lactic acid) composites
    2007, Trans Tech Publications
    The potential of hemp fibre as a reinforcing material for Poly(lactic acid) (PLA) was investigated. Good interaction between hemp fibre and PLA resulted in increases of 100% for Young’s modulus and 30% for tensile strength of composites containing 30 wt% fibre. Different predictive ‘rule of mixtures’ models (e.g. Parallel, Series and Hirsch) were assessed regarding the dependence of tensile properties on fibre loading. Limited agreement with models was observed. Differential scanning calorimetry (DSC) and x-ray diffraction (XRD) studies showed that hemp fibre increased the degree of crystallinity in PLA composites.
  • Item type:Publication,
    Analysis of mechanical properties of hemp fibre reinforced unsaturated polyester composites
    2013, Sage
    Different chemically treated hemp fibre reinforced unsaturated polyester composites were investigated over a range of fibre content (0–60 wt%). Although Young’s modulus of all the short fibre reinforced unsaturated polyester composites was found to be higher than that of unreinforced unsaturated polyester; however, tensile strength of the composites exceeded that of the unsaturated polyester matrix only for the combined alkali- and silane-treated fibre composites at 40 wt% fibre content. The decrease in tensile strength of the composites could be attributed to stress concentrations caused by the fibres in conjunction with the brittle matrix. Impact strength of all the treated fibre composites was higher than that of the untreated fibre composites at all fibre contents. KIc and GIc of the composites decreased initially and thenincreased as the fibre content increased because more and more fibres being available to pull-out. The mechanical properties of the composites were increased further due to the alignment of long fibres.
  • Item type:Publication,
    Flexural properties of hemp fibre reinforced polylactide and unsaturated polyester composites
    2011, Elsevier
    In this work, flexural strength and flexural modulus of chemically treated random short and aligned long hemp fibre reinforced polylactide and unsaturated polyester composites were investigated over a range of fibre content (0–50 wt%). Flexural strength of the composites was found to decrease with increased fibre content; however, flexural modulus increased with increased fibre content. The reason for this decrease in flexural strength was found to be due to fibre defects (i.e. kinks) which could induce stress concentration points in the composites during flexural test, accordingly flexural strength decreased. Alkali and silane fibre treatments were found to improve flexural strength and flexural modulus which could be due to enhanced fibre/matrix adhesion.
  • Item type:Publication,
    Effect of fibre treatments on interfacial shear strength of hemp fibre reinforced polylactide and unsaturated polyester composites
    2011, Elsevier
    Surface treatment of hemp fibres was investigated as a means of improving interfacial shear strength (IFSS) of hemp fibre reinforced polylactide (PLA) and unsaturated polyester (UPE) composites. Fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane. A combined treatment using sodium hydroxide and silane was also carried out. IFSS of PLA/hemp fibre samples increased after treatment, except in the case of maleic anhydride treatment. Increased IFSS could be explained by better bonding of PLA with treated fibres and increased PLA transcrystallinity. The highest IFSS was 11.4 MPa which was obtained for the PLA/alkali treated fibre samples. IFSS of UPE/hemp fibre samples increased for all treated fibres. This is believed to be due to the improvement of chemical bonding between the treated fibres and the UPE as supported by FT-IR results. The highest IFSS (20.3 MPa) was found for the combined sodium hydroxide and silane treatment fibre/UPE samples.
  • Item type:Publication,
    Influence of loading rate, alkali fibre treatment and crystallinity on fracture toughness of random short hemp fibre reinforced polylactide bio-composites
    2011, Elsevier
    Plane-strain fracture toughness (KIc) of random short hemp fibre reinforced polylactide (PLA) bio-composites was investigated along with the effect of loading rate, fibre treatment and PLA crystallinity. Fracture toughness testing was carried out at loading rates varying from 0.5 to 20 mm/min using single-edge-notched bending specimens with 0 to 30 wt% fibre. KQ (trial KIc) of composites decreased as loading rate increased, until stabilising to give KIc values at a loading rate of 10 mm/min and higher. The reduction of crazing and stress whitening, as well as a more direct crack path observed in PLA samples combined with reduced plastic deformation observed in composites provided explanation for this reduction. KIc of composites was found to decrease with increased fibre content and fibre treatment with sodium hydroxide. Studies controlling the degree of PLA crystallinity by heat treatment or “annealing” showed that reduction of KIc can be attributed to increased crystallinity.
  • Item type:Publication,
    Effect of various chemical treatments on the fibre structure and tensile properties of industrial hemp fibres
    2011, ELSEVIER SCI LTD
    Industrial hemp fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane to investigate the influence of treatment on the fibre structure and tensile properties. It was observed that the average tensile strength of sodium hydroxide treated fibres slightly increased compared with that of untreated fibres, which was believed to be as a result of increased cellulose crystallinity. The average tensile strength of acetic anhydride, maleic anhydride, silane and combined sodium hydroxide and silane treated fibres slightly decreased compared with that of untreated fibres, which was believed to be as a result of decreased cellulose crystallinity. However, the average Young’s modulus of all treated fibres increased compared with untreated fibres. This was considered to be as a result of densification of fibre cell walls due to the removal of non-cellulosic components during treatment.
  • Item type:Publication,
    Improvement of mechanical performance of industrial hemp fibre reinforced polylactide biocomposites
    2011-03, Elsevier
    In this work, mechanical properties of chemically treated random short fibre and aligned long hemp fibre reinforced PLA composites were investigated over a range of fibre content (0–40 wt.%). It was found that tensile strength, Young’s modulus and impact strength of short hemp fibre reinforced PLA composites increased with increased fibre content. Alkali and silane fibre treatments were found to improve tensile and impact properties which appears to be due to good fibre/matrix adhesion and increased matrix crystallinity. A 30 wt.% alkali treated fibre reinforced PLA composite (PLA/ALK) with a tensile strength of 75.5 MPa, Young’s modulus of 8.18 GPa and impact strength of 2.64 kJ/m2 was found to be the best. However, plane-strain fracture toughness and strain energy release rate decreased with increased fibre content. The mechanical properties of the PLA/ALK composites were increased further due to alignment of long fibres.
  • Item type:Publication,
    Characterisation of hemp fibre reinforced Poly(Lactic Acid) composites
    2009, Inderscience Enterprises
    In this work, the mechanical properties including tensile strength, flexural strength, impact strength and fracture toughness of the PLA/hemp composites were investigated over a range of fibre content (0-30 wt.%). It was observed that, the tensile strength and Young's modulus of the composites increased with increased fibre content. The flexural strength did not increase with fibre reinforcement, however, the flexural modulus of the composites increased significantly. Impact strength of the composites increased up to 20 wt. % fibre loading, however, further increased fibre loading caused a reduction of impact strength. KIc and GIc values decreased with increased fibre content.