<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 5 of 5
  • Item type:Publication,
    The effect of silane coupling agent on iron sand for use in magnetorheological elastomers Part 1: Surface chemical modification and characterization
    2015-01-01, Elsevier
    Bis-(3-triethoxysilylpropyl) tetrasulphane (TESPT) was employed for surface modification of iron sand for use in magnetorheological elastomers (MREs). The amount of TESPT was varied at five levels (2, 4, 6, 8 and 10 wt%) relative to iron sand content to assess the optimum amount of coupling agent for interfacial bonding and damping performance. Evidence that coupling had occurred between iron sand and TESPT was identified by Raman Spectroscopy and the grafting percentage was determined by thermogravimetric analysis. Subsequently, isotropic MREs containing unmodified and modified iron sand particles and natural rubber were prepared. Crosslink density assessment by swelling testing provided evidence that the tetrasulphane group of TESPT formed crosslinks with the rubber chains. The results exhibited the advantages of TESPT as a coupling agent between iron sand particles and rubber and also revealed that 6% TESPT content produced the highest crosslink density. The effects of the amount of TESPT on dynamic mechanical properties the morphological characteristics of the MREs were also investigated.
  • Item type:Publication,
    Damping properties and microstructure of magnetorheological composites based on iron sand and natural rubber
    2013, University of Auckland - Department of Chemical & Materials Engineering, 2013
    Material with high damping capability is desired from the viewpoint of vibration suppression in structures. Rubber is by far the most commonly used material for damping; here damping relies on the energy absorbed due to viscous flow that occurs during deformation in this viscoelastic materials. However, enhancement of damping through rubber modification or rubber selection to increase viscous flow, not surprisingly, generally results in a reduction in stiffness and strength [1]. More recently, a new class of damping materials, magnetorheological elastomers (MREs) have been developed such that inclusion of magnetic particles in rubber enables additional damping through magnetic particle interaction and interfacial friction. Furthermore, damping and stiffness can be varied by application of an applied magnetic field during fabrication or in service. MREs can be utilised for damping, either alone or within a composite structure such as those including steel plates.
  • Item type:Publication,
    Dynamic Properties of Magnetorheological Elastomers Based on Iron Sand and Natural Rubber
    2015-02-20, Wiley-Blackwell
    In this study, magnetorheological elastomers (MREs) based on iron sand and natural rubber were prepared. The Taguchi method was employed to investigate the effect of a number of factors, namely, the iron sand content, iron sand particle size, and applied magnetic field during curing on the loss tangent (tan δ) and energy dissipated during cyclic loading. Tan δ was measured through dynamic mechanical analysis over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100 to 50°C). The energy dissipated was measured with a universal tester under cyclic tensile loading. The data were then statistically analyzed to predict the optimal combination of factors, and finally, experiments were conducted for verification. It was found that the iron sand content had the greatest influence on tan δ when measured over a range of frequency, and the energy dissipated during hysteresis tests. However, none of the factors showed a significant influence on tan δ when measured over a range of strain amplitude. Furthermore, the iron sand content and magnetic field were also found to influence the width of the peak in tan δ as a function of the temperature. The morphological characteristics of the MREs were also examined with scanning electron microscopy.
  • Item type:Publication,
    Comparison of dynamic properties of magnetorheological elastomers with existing antivibration rubbers
    2015-12-15, Elsevier
    Tan δ and energy dissipated during hysteresis testing of isotropic and anisotropic MREs containing silane modified iron sand particles in a natural rubber matrix were compared with existing antivibration rubbers. Tan δ was measured using dynamic mechanical analysis (DMA) over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100–50 °C). Energy dissipated was measured using a universal tester under cyclic tensile loading. The chosen antivibration rubbers for comparison contained different contents of carbon black filler (30, 50 and 70 phr) in a natural rubber matrix. It was found that energy absorption for comparative samples was generally higher than isotropic and anisotropic MREs over the range of frequency and strain amplitude explored, as well as in hysteresis testing and this was believed to be largely due the presence of carbon black in the formulation. Further assessment was carried out on materials that were the same as anisotropic MREs except they had additions of carbon black. The energy absorption was found higher than comparative samples with the same carbon black contents, supporting the use of iron sand to improve damping. However, trends for energy absorption at around Tg were found to reverse which is considered to be due to the segmental motion of rubber chains being by far the most significant influence on energy absorption in the glass transition zone.
  • Item type:Publication,
    A new method to predict optimum cure time of rubber compound using dynamic mechanical analysis
    2013, Wiley
    The degree of vulcanization of a rubber compound has a big influence on the properties of the final product. Therefore, precisely defining the curing process including optimum cure time is important to ensure the production of final products having high performance. Typically, vulcanization is represented using vulcanization curves. The main types of equipment used for producing vulcanization curves are the oscillating disc rheometer (ODR) and the moving die rheometer (MDR). These can be used to plot graphs of torque versus time at a constant temperature to show how cure is proceeding. Based on the results obtained, optimum cure time (t₉₀) is calculated as the time required for the torque to reach 90% of the maximum achievable torque. In this study, the use of Dynamic Mechanical Analysis (DMA) for assessment of t₉₀ was assessed. DMA was carried out using shear mode isothermal tests to measure the changes in material properties caused by vulcanization. The results revealed that the shear storage modulus (G′), shear loss modulus (G′′), and tan δ all reflect the vulcanization process, however, tan δ gave the best representation of level of vulcanization. Indeed, the curve of tan δ was able to be used to derive the t₉₀ for rubber compounds and showed good agreement with the results from an MDR.