    Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts
    2013, Elsevier
    Ti-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.
  • Item type:Publication,
    Microstructure and mechanical properties of large size Ti-43Al-9V-0.2Y alloy pancake produced by pack-forging
    2013, Elsevier
    A pancake of Ti-43Al-9V-0.2Y (at.%) alloy with dimensions of ϕ480 mm × 46 mm was fabricated by pack-forging with a thick reduction of 80%. The as-forged Ti-43Al-9V-0.2Y alloy pancake has a duplex (DP) microstructure, which is composed of B2/α₂/γ lamellar colonies and massive B2 and γ phase regions distributed along the boundaries between the lamellar colonies. Different microstructures were obtained by heat treatment of samples cut from the as-forged Ti-43Al-9V-0.2Y alloy pancake. A fully lamellar (FL) structure consisting of B2/α₂/γ lamellar colonies was obtained after the heat treatment of 1350 °C/8 h. Tensile test results exhibited that the yield strength (YS) and ultimate tensile strength (UTS) of the alloy with DP microstructure were decreased from 680.7 MPa to 834.3 MPa at room temperature to 589.5 MPa and 693.1 MPa at 700 °C, respectively, and the elongation (δ) of the alloy with DP microstructure was increased from 1.99% at room temperature to 12.12% at 700 °C; the elongation (δ) of the alloy with FL microstructure was increased from 1.52% at room temperature to 85.84% at 800 °C.