  • Item type:Publication,
    Strengthening mechanisms of Ti via Al addition
    2020, Elsevier
    Pure Ti is characterised by an interesting combination of performance from an engineering point of view. The addition of Al to Ti can be used to reduce the intrinsic cost of the material, decrease the density of the alloy, and increase the mechanical performance. This study is focused on evaluating the physical properties, microstructural evolution and mechanical behaviour of Ti-xAl alloys (where x = 1–6 wt%) in order to scientifically understand the strengthening mechanisms of the addition of Al to pure Ti manufactured via the conventional powder metallurgy route of cold uniaxial pressing plus solid state sintering. The addition of Al to Ti does not affect the compressibility of the alloy but changes the consolidation and densification of the alloy. The incremental addition of Al results in the progressive strengthening of Ti via the simultaneous contribution from substitutional solid solution and grain refinement strengthening which outdo the negative effect of the residual porosity.
  • Item type:Publication,
    Comparison of the Cracking Behavior of Powder Metallurgy and Ingot Metallurgy Ti-5Al-5Mo-5V-3Cr Alloys during Hot Deformation
    2019-02-01, MDPI
    The hot workability of metallic materials is significantly dependent on its ability to form plastic without cracking and fracturing. In this work, the cracking behavior of powder metallurgy (PM) Ti-5Al-5Mo-5V-3Cr (Ti-5553) alloy, consolidated from powder mixture, at a deformation temperature range of 600 ◦C–850 ◦C and strain rate of 0.1 s−1–10 s−1, was investigated through isothermal compression tests. The cracking behavior of the as-cast ingot metallurgy (IM) Ti-5553 alloy, at a deformation temperature of 700 ◦C was also investigated for comparison. Results suggested that the PM Ti-5553 alloy had a better hot workability, with a larger cracking-free processing window, and a lower deformation resistance than the IM counterpart. 45◦ shear fracture occurred in the PM alloy, compressed at the condition of 600 ◦C/10 s−1, and edge cracking was observed at the 700 ◦C/10 s−1. 45◦shear fracture was also significant in the IM alloy specimen tested at 700 ◦C/10 s−1, and all the other IM alloy specimens compressed at 700 ◦C displayed longitudinal cracking. Moreover, the microscopic cracking observation showed that ductile dimple cracking can be found in the IM alloy, but brittle cleavage fracture was dominant in the cracking surface of PM alloy with a relatively low cracking ductility
  • Item type:Publication,
    Thermomechanical processing of cost-affordable powder metallurgy Ti-5Fe alloys from the blended elemental approach: Microstructure, tensile deformation behavior, and failure
    2020, MDPI
    The development of cost-affordable Ti alloys is key for the application of Ti in other industries like the automobile sector. Therefore, a combination of powder metallurgy (PM) and low-cost compositions is an interesting approach. In this article, a cost-affordable PM Ti-5Fe alloy is processed following the blended elemental route and extruded at high temperature to remove porosity. Different extrusion temperatures and heat treatments (i.e., solution treatment and aging, STA) are performed to obtain ultrafine microstructures, and their effect on the mechanical behavior is studied. For extrusions in the β phase, microstructures consist of coarse lamellar colonies, resulting in alloys with improved properties compared to the as-sintered alloy but still lacking toughness due to the failure happening just after necking onset. Extruding in the α + β phase results in a bimodal microstructure of fine elongated primary α and coarse lamellar colonies, and the alloy becomes tougher. STA with aging below the eutectoid temperature of 590 °C leads to a hard but brittle alloy, whereas STA with aging above it results in alloys with strength comparable to the as-extruded conditions and enhanced ductility.
  • Item type:Publication,
    Advancement in the pressureless sintering of CP titanium using high-frequency induction heating
    2019, Springer
    High-frequency induction heating is applied as an alternative heating source for pressureless sintering of commercially pure Ti powders, aiming to intensify the sintering process. The effects of the process parameters on the properties of the sintered material are systematically studied. The initial powder compact density is the most influential parameter permitting sintered structures with highly porous to almost fully dense appearance. Short heating time combined with sintering to temperatures just above the β-transus resulted in a strong diffusion bonding between the Ti powder particles, and grain growth is observed at the former boundaries of the neighboring powder particles. The dimpled appearance of the fracture surface at those regions confirmed the strong metallic interparticle bonding. Tensile properties comparable to those of Ti-Grade 3 and Ti-Grade 4 are achieved, which also demonstrates the efficiency of the induction sintering process. A mechanism explaining the fast and efficient sintering is proposed. The process has the added advantage of minimizing the oxygen pickup.
  • Item type:Publication,
    On microstructural evolution and mechanical properties of Ti-5Al-5V-5Mo-3Cr alloy synthesised from elemental powder mixtures
    2018, Elsevier
    In this paper, we explored to prepare a multi-compositional titanium alloy, Ti-5Al-5V-5Mo-3Cr (Ti-5553), by powder compact extrusion from elemental powder mixtures, and investigate the microstructure variation during the synthesising process and after post heat treatments and the changes of mechanical properties. XRD, OM and SEM were used to analyse the phase constitutions and microstructures of the Ti-5553 alloy at different processing conditions, and tensile tests were conducted to examine their mechanical properties. The results showed that a homogeneous Ti-5553 alloy was successfully produced by powder compact extrusion from the powder mixtures, β phase was mainly contained in the hot-pressed and 1200°C-extruded Ti-5553 alloy and had an equiaxed microstructure. Different types of α phase precipitated from the β matrix after heat treatment, and this significantly changed the microstructures and improved the mechanical properties of the extruded Ti-5553 alloy, with yield strength of 1250 MPa and ultimate strength of 1300 MPa for the alloy treated at 675 °C for 2 h, and the ductility of about 6.1% for the alloy treated at 780 °C for 2 h.
  • Item type:Publication,
    Producing High-Quality Titanium Alloy by a Cost-Effective Route Combining Fast Heating and Hot Processing
    2018, Springer
    Powder metallurgy is a very attractive method for producing titanium alloys, which can be near-net-shape formed and have freedom in composition selection. However, applications are still limited due to product affordability. In this paper, we will discuss a possible cost-effective route, combining fast heating and hot processing, to produce titanium alloys with similar or even better mechanical properties than that of ingot metallurgy titanium alloys. Two titanium alloys, Ti-5Al-5V-5Mo-3Cr (Ti-5553) and Ti-5Fe, were successfully produced from HDH titanium powder and other master alloy powders using the proposed processing route. The effect of the processing route on microstructural variation and mechanical properties have been discussed.