<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 2 of 2
  • Item type:Publication,
    On microstructural evolution and mechanical properties of Ti-5Al-5V-5Mo-3Cr alloy synthesised from elemental powder mixtures
    2018, Elsevier
    In this paper, we explored to prepare a multi-compositional titanium alloy, Ti-5Al-5V-5Mo-3Cr (Ti-5553), by powder compact extrusion from elemental powder mixtures, and investigate the microstructure variation during the synthesising process and after post heat treatments and the changes of mechanical properties. XRD, OM and SEM were used to analyse the phase constitutions and microstructures of the Ti-5553 alloy at different processing conditions, and tensile tests were conducted to examine their mechanical properties. The results showed that a homogeneous Ti-5553 alloy was successfully produced by powder compact extrusion from the powder mixtures, β phase was mainly contained in the hot-pressed and 1200°C-extruded Ti-5553 alloy and had an equiaxed microstructure. Different types of α phase precipitated from the β matrix after heat treatment, and this significantly changed the microstructures and improved the mechanical properties of the extruded Ti-5553 alloy, with yield strength of 1250 MPa and ultimate strength of 1300 MPa for the alloy treated at 675 °C for 2 h, and the ductility of about 6.1% for the alloy treated at 780 °C for 2 h.
  • Item type:Publication,
    Preparation, microstructure and properties of Ti-6Al-4V rods by powder compact extrusion of powder mixture
    2012, Trans Tech Publications
    Ti-6Al-4V (wt%) alloy rods were prepared successfully using a low-cost method that combines mixing elemental and master alloy powders and powder compact extrusion. The microstructure and mechanical properties of the rods and the effects of extrusion temperature on them were investigated. The results showed that the microstructure and mechanical properties of the extruded rods were strongly affected by the extrusion temperature. With increasing extrusion temperature from 1200°C to 1300°C and keeping the powder compact holding time unchanged at 2 minutes, the fraction of undissolved V rich particles in the microstructure of the extruded rod decreased substantially to zero, the level of composition homogenization increased dramatically to the highest level, and the UTS and elongation of the extruded rods increased significantly from 886MPa and 1.2% to 1300MPa and 7.1%, respectively. The tensile properties of the Ti-6Al-4V alloy rods produced by powder compact extrusion of the powder mixture are comparable to those of Ti-6Al-4V alloy produced by ingot metallurgy and thermomechanical processing.