University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, Fabrication, microstructure, mechanical, and electrochemical properties of NiMnFeCu high entropy alloy from elemental powders2022, MDPI AGTransition metal based high entropy alloys (HEAs) are often used in electrocatalytic (water electrolysis) applications due to the synergistic effect operating among its constituent elements and unpaired electrons in d orbitals of the concerned metal. In this study, a low cost NiMnFeCu high entropy alloy was successfully synthesised using the combined techniques of mechanical milling (MA) and vacuum sintering. X‐ray diffraction was used to analyse the phase composition, optical microscopy, and scanning electron microscopy were used to characterise the fabricated material’s microstructure and chemical homogeneity, thermal, and mechanical properties were tested using the differential scanning calorimetry method and a universal testing machine, respectively. Electrochemical workstation was used to carry out preliminary electrochemical studies such as linear sweep voltammetry (LSV), cyclic voltammetry (CV) and chronoamperometry. The results showed that the as‐ sintered NiMnFeCu HEA possessed a single‐ phase FCC structure. The HEA NiMnFeCu sintered at 1050 °C (S4) and 1000 °C (S2) with a holding time of 2 h showed a yield strength of 516.3 MPa and 389.8 MPa, respectively, and the micro‐hardness values were measured to be 233.45 ± 9 HV and 198.7 ± 8 HV, respectively. Preliminary electrochemical studies proved that the alloy sintered at 1000 °C (S2) with a holding time of 2 h exhibited excellent electrocatalytic properties with a measured overpotential of 322 mV at 10 mA cm⁻² at 100 cycles of CV and good stability for 10 h when compared to state‐of‐the‐art electrocatalytic materials IrO₂ and RuO₂ This suggested that the HEA NiMnFeCu fabricated under the condition S2 could potentially be used for industrial‐scale water electrolysis as it possesses permissible mechanical and good electrochemical properties.Item type:Publication, Heat treatment, impact properties, and fracture behaviour of Ti-6Al-4V alloy produced by powder compact extrusion.2019, MDPIThe mechanical properties of titanium and titanium alloys are very sensitive to processing, microstructure, and impurity levels. In this paper, a blended powder mixture of Ti-6Al-4V alloy was consolidated by powder compact extrusion that involved warm compaction, vacuum sintering, and hot extrusion. The as-processed material with an oxygen content of 0.34 wt.% was subjected to various annealing treatments. The impact toughness of heat-treated material was determined using Charpy V-notch impact testing at room temperature. An emphasis was placed on establishing a relationship among fracture behaviour, microstructure, and the resulting properties of tested material. From the results, it is apparent that the highest impact toughness value of 19.3 J was achieved after α/β annealing and is comparable with typical values given in the literature for wrought Ti-6Al-4V. In terms of fracture behaviour, it is quite apparent that the crack propagation behaviour of powder-produced material is rather complex compared with the limited amount of data reported for ingot counterparts.Item type:Publication, Effect of microwave sintering parameters on the physical and mechanical properties of pure Ti and blended elemental Ti alloys2018, Trans Tech PublicationsMicrowave sintering (MWS) was used to consolidate hydride de-hydride Ti powder and blended elemental Ti6Al4V, Ti5Fe and Ti5Al5Mo5V3Cr (Ti5553) powder mixtures. The amount of powders used to prepare the powder compacts was scaled up to 500g.The effect of the MWS conditions on the relative density, porosity distribution, microstructure and tensile properties were studied. Furthermore, uniformity in distribution of the alloying elements was checked. For most of the materials considered, a combinations of sintering temperature of 1200ºC and 1300ºC and holding time of 5 to 30 min resulted in significantly improved density. Nevertheless sintering temperature of at least 1300ºC was required for pore coalescence and high tensile properties.