University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
5 results
Search Results
Item type:Publication, Tensile properties and fracture behaviour of an ultrafine grained Ti–47Al–2Cr (at.%) alloy at room and elevated temperatures2012, SpringerAn ultrafine grained (UFG) Ti–47Al–2Cr (at.%) alloy has been synthesized using a combination of high energy mechanical milling and hot isostatic pressing (HIP) of a Ti/Al/Cr composite powder compact. The material produced has been tensile tested at room temperature, 700 and 800 °C, respectively, and the microstructure of the as-HIPed material and the microstructure and fracture surfaces of the tensile tested specimens have been examined using X-ray diffractometry, optical microscopy, scanning electron microscopy and transmission electron microscopy. The alloy shows no ductility during tensile testing at room temperature and 700 °C, respectively, but very high ductility (elongation to fracture 70–100%) when tensile tested 800 °C, indicating that its brittle to ductile transition temperature (BDTT) falls within the temperature range of 700–800 °C. The retaining of ultrafine fine equiaxed grain morphology after the large amount of plastic deformation of the specimens tensile tested at 800 °C and the clear morphology of individual grains in the fractured surface indicate that grain boundary sliding is the predominant deformation mechanism of plastic deformation of the UFG TiAl based alloy at 800 °C. Cavitation occurs at locations fairly uniformly distributed throughout the gauge length sections of the specimens tensile tested at 800 °C, again supporting the postulation that grain boundary sliding is the dominant mechanism of the plastic deformation of the UFG TiAl alloys at temperatures above their BDTT. The high ductility of the UFG alloy at 800 °C and its fairly low BDTT indicates that the material a highly favourable precursor for secondary thermomechanical processing.Item type:Publication, High temperature mechanical properties of Ti-47Al-2Cr (at %) alloy produced using powder compact forging of a mechanically milled powder2009, IOP PublishingUltrafine grained (UFG) Ti-47Al-2Cr (at %) alloy was prepared using a combination of high energy ball milling of a mixture of elemental powders to produce a Ti/Al/Cr composite powder and forging of compacts of this composite powder. The microstucture of the powder forged alloy was found to be dependent on the initial condition of the powder. The alloy produced by this method has demonstrated good formability, both in tensile and compression testings at elevated temperatures. A ductility of 80–165% in tension has been observed, while in a compression plastic strain of ~ 50% was found to be easily achievable, without causing cracking. The deformation behaviour of the particular alloy in tension and compression at elevated temperature has been discussed in detail. The results from the present investigation indicate that UFG Ti-47Al-2Cr (at %) alloy produced using powder compact forging has good formability, and is suitable precursor for near-net shaping using thermomechanical processes such as forging and superplastic forming.Item type:Publication, Tribological properties of thermally sprayed TiAl-Al₂O₃ composite coating2009, IOP PublishingThe use of thermal spray coatings provides protection to the surfaces operating in severe environments. The main goal of the current work is to investigate the possibility of using a high velocity oxy fuel (HVOF) thermally sprayed wear resistant TiAl/Al2O3 coating on tool steel (H13) which is used for making dies for aluminium high pressure die casting. A feedstock of TiAl/Al2O3 composite powder was produced from a mixture of Al and TiO2 powders by high energy mechanical milling, followed by a thermal reaction process. The feedstock was then thermally sprayed using a high velocity oxy-fuel (HVOF) technique onto H13 steel substrates to produce a composite coating. The present study describes and compares the tribological properties such as friction and sliding wear rate of the coating both at room and high temperature (700°C). The results showed that the composite coating has lower wear rate at high temperature (700°C) than the uncoated H13 sample. At Room temperature without using lubricant there is no much significant difference between the wear rate of the coated and uncoated samples. The experimental results showed that the composite coating has great potential for high temperature application due to its lower wear rate at high temperature in comparison with the uncoated sample at the same temperature. The composite coating was characterized using scanning electron microscopy (SEM), optical microscopy and X-ray diffractometry (XRD). This paper reports the experimental observations and discusses the wear resistance performance of the coatings at room and high temperatures.Item type:Publication, Microstructure and thermal stability of nanostructured Cu-7.5vol.%Al₂O₃ composite powders produced by high energy mechanical milling2009, IOP ScienceNanostructured Cu-7.5vol.%Al₂O₃ composite powders were produced from a mixture of Cu powder and Al₂O₃ nanopowder using two routes of high energy mechanical milling. The milled composite powders were heat treated at 150, 300, 400 and 500°C for 1 hour, respectively, to determine the thermal stability of the microstructure and corresponding micohardness change of the powder particles as a function of the annealing temperature. For the nanocomposite powder produced with 12 hours of milling (Route 1), heat treatment at 150°C did not change the microstructure, increasing the annealing temperature from 150 to 500°C caused the Cu grain sizes to increase due to grain coarsening. For the composite powder produced with 24 hours milling (Route 2), the grain sizes of the Cu matrix also increased due to grain coarsening with increasing the annealing temperature from 150 to 500°C. Average microhardness decreased significantly for both the nanocomposite powders but the degree of grain size increase was smaller with increasing the annealing temperature from 400 to 500°C.Item type:Publication, Synthesis, Microstructure, and Mechanical Properties of a Novel Ti₂AlC/TiC/Al₂O₃In Situ Composite2006, Wiley-Blackwell Publishing, Inc.This paper describes a novel process for synthesizing a Ti₂AlC/TiC/Al₂O₃in situ composite. This route utilizes TiO₂, carbon, and Al powders as raw materials, and involves high-energy mechanical milling and powder sintering. The Ti₂AlC/TiC/Al₂O₃ bulk in situ composite produced has a phase composition of Ti₂AlC–20 vol% TiC–35 vol% Al₂O₃ with fine Al₂O₃ particles (size: 0.5–15 μm) embedded in a Ti₂AlC/TiC matrix. The Ti₂AlC grains exhibit a nanometer scale lamellar structure, and most of the Al₂O₃ grains contain fine cubic TiOmC1−m precipitates (size: 10–200 nm). The average hardness and bending strength of the composite are in the ranges of 11–12.5 GPa and 380–440 MPa, respectively. Here we have demonstrated that the mechanical performance (mainly hardness and bending strength) of the composite is directly correlated with the size of the Al2O3 particles present in the as-fabricated in situ composite.