University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
5 results
Search Results
Item type:Publication, Mechanical properties of thermoplastic protein from bloodmeal and polyester blends2014, WileyBlends of bloodmeal-based thermoplastic (NTP) and polybutylene succinate (PBS) were prepared to study the effect of compatibilization on mechanical properties. The Taguchi method was used for experimental design and the results were analysed in terms of signal-to-noise (S/N) ratios using analysis of variance (ANOVA). Between 5 and 10 wt.-% of either poly-2-ethyl-2-oxazoline (PEOX) and poly [(phenyl isocyanate)-co-formaldehyde] (pMDI) were used as compatibilizers in blends of 20–100% NTP. The tensile strength of the blends depended on the type of compatibilizer used while for elongation at break and modulus, NTP content had the largest influence. Compatibilizing efficiency was more pronounced at higher NTP content. The blend's morphology showed a smaller particle size for blends at optimal tensile properties while plastic deformation was observed for samples where elongation at break was optimal.Item type:Publication, Treating Bloodmeal with Peracetic Acid to Produce a Bioplastic Feedstock2013, WileyPeracetic acid is used to remove the color and odor from bloodmeal to produce a new bioplastic feedstock. The effects on bloodmeal molecular mass, crystallinity, thermal stability, solubility, product color and smell is investigated. 3 wt% PAA is the lowest concentration to sufficiently remove the odor from bloodmeal. Protein molecular mass is unaffected by PAA concentration. The crystallinity decreases from 35 to 31–27% when treated with 1–5 wt% PAA. Treating bloodmeal with 1–5 wt% PAA also reduces the protein's thermal stability, glass transition temperature (from 225 down to 50 °C) and increases its solubility in PBS, SDS, and sodium sulfite.Item type:Publication, Biodegradation of bloodmeal-based thermoplastics in green-waste composting2011, SpringerPolymers that are compostable and manufactured from renewable resources have gained significant importance in recent years. The objective of this work was to assess the biodegradability of bloodmeal-based thermoplastics in a commercial green-waste composting situation. Materials plasticised with tri-ethylene–glycol lost about 45% of their original mass after 12 weeks composting while unplasticised samples lost 35%. Degradation appeared to have been in two phases; an initial loss of soluble, low molecular compounds in the mesophilic phase followed by degradation of high molecular compounds as the temperature exceeded about 40 °C in the thermophilic phase. It was found that as degradation proceeded materials became more soluble. In addition, plasticised and unplasticized samples contained about 60 wt% moisture after 4 weeks of composting conditioning at 50% relative humidity resulted in approximately 8–10 wt% moisture, unaffected by the extent of degradation. FTIR revealed that proteins underwent hydrolytic cleavage resulting in the formation of primary amines. A significant reduction in combustion temperature was observed, indicative of a reduction in covalent bonding, likely due to shorter chains lengths or less cross-linking.Item type:Publication, Mechanical properties and water absorption of thermoplastic bloodmeal2011, Wiley Online LibraryBloodmeal mixtures containing SS, water, SDS and urea were extruded and injection-molded. Increased chain mobility with sufficient plasticization during processing increased the amount of available amino acids for strong water/protein interactions. Materials containing low water and increased SS had reduced tensile strength and elongation, compared to higher water at the same SS content. Materials containing three parts SS per hundred parts bloodmeal (pphbm), 60 pphbm water and 20 pphbm urea, were the only ductile materials after conditioning. Changing any one of these factors to a lower level will result in a brittle material. This mixture in combination with 3 pphbm SDS resulted in optimal mechanical properties (tensile strength of 9.6 MPa and Young's modulus of 534.9 MPa).Item type:Publication, Degradation as a result of UV radiation of bloodmeal-based thermoplastics2011, ElsevierPolymers are known for their susceptibility to degradation as a result of ultra-violet (UV) radiation. In this study, the UV stability of bloodmeal-based thermoplastics (BMT) was evaluated over a period of 12 weeks. Formulations with and without plasticiser were tested and moisture was excluded during accelerated weathering to isolate the effect of UV because of the material’s known sensitivity to moisture. It was found that embrittlement due to loss of water overshadowed the effect of UV degradation. Embrittlement caused the material’s toughness to be reduced by an order of magnitude after only two weeks of exposure, for either plasticised or unplasticised samples. An initial increase in tensile strength was observed after two weeks followed by a steady decline in strength. The elastic modulus reached a plateau after about two weeks of exposure. FTIR did not confirm any chemical changes after 12 weeks exposure and TGA suggested that low molecular mass species were quickly lost during the course of the test. The absence of chemical changes does not suggest resistance to environmental degradation, although the dark pigmentation of bloodmeal may have contributed to the lack of UV degradation. Embrittlement remains a greater concern and requires further attention.