    Influence of feeding level after drying off on incidence of mastitis and keratin plug formation in dairy cows
    2004
    Two groups of 70 cows, including 51 identical twin sets, were grazed at either an unrestricted (14 kg dry matter intake/day; DMI/d) or restricted (6 kg DMI/d) daily pasture allowance for two weeks after drying off (DO). Incidence of new intramammary infection (IMI) and teat open/closed status was assessed at 7, 14 and 21 days after DO. Keratin plug formation was determined on a subset of 40 cows at 7 and 14 days after DO. Number of clinical mastitis (CM) cases and total new IMI did not differ between cows maintained on unrestricted or restricted DMI. However Streptococcus uberis was isolated from more new IMI in unrestricted animals than restricted animals (11.7% vs. 4.6 % of quarters respectively; P <0.01). At 7 and 14 days after DO, more teats were classified as open in the unrestricted group compared to the restricted animals (57% vs. 43% of quarters respectively; P <0.01). However weight of keratin collected from teat canals did not differ between nutritional treatments. Results suggest that unrestricted nutrition after DO did not increase risk of CM but does increase risk of S. uberis infection.
  • Item type:Publication,
    Biofibre production from chicken feather
    2011
    The global poultry industry generates at least 2 million tonnes of chicken feather every year. Feather fibre has potential as reinforcement for polymer composites with light-weight, thermal insulation and acoustic dampening properties. This study aimed to develop a process to produce clean fibre recovered from chicken feather. Raw feather was decontaminated by 0.15% sodium hypochlorite in 25 L water at pH 10.0 for two 30 min stages and cleaned by 0.15% hydrogen peroxide in 25 L water for three 30 min stages. Cleaned feather was comminuted in 300 L water using a centrifugal pump at 30 Hz impeller speed on full recycle for 4 h. Rachis and partially cut feather were removed using a 5 mm filter and fibre was recovered using a 1 mm filter. Wet fibre was dried in an air-forced oven at 70°C. Morphological studies revealed fibre surface remained intact after the treatment process.