University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
5 results
Search Results
Item type:Publication, Effect of Mn on the Properties of Powder Metallurgy Ti-2.5Al-xMn Alloys.2023-07-10, MDPITitanium alloys are the ideal material for a wide range of structural applications, but their high cost compared to other metals hinders their adoption. Powder metallurgy and cheap alloying elements can be used to create new Ti alloys. In this study, the simultaneous addition of Al and Mn is considered to manufacture and characterise ternary Ti-2.5Al-Mn alloys obtained via pressing and sintering by varying the Mn content (1-10 wt.%). It is found that the addition of the alloying elements reduces compressibility. Consequently, the amount of porosity increases (8.5 → 10.8%) with the amount of Mn as the alloys were processed under the same conditions. The progressive addition of Mn refines the classical lamellar microstructure and, eventually, transforms it into an equiaxed β-grain structure with acicular α grains. The microstructural changes lead to continuous increases in strength (ultimate tensile strength: 694 → 851 MPa) and hardness (225 → 325 HV30) with an associated loss of ductility (elongation to failure: 13.9 → 1.0%). However, the obtained ternary Ti-2.5Al-Mn alloys have similar or better overall mechanical behaviour than most of the binary Ti-Mn alloys obtained through a variety of manufacturing methods.Item type:Publication, Antibacterial Ti-Mn-Cu alloys for biomedical applications2020, Oxford University Press (OUP)Titanium alloys are common biomedical materials due to their biocompatibility and mechanical performance. However, titanium alloys are expensive and, unless surface treated, generally cannot prevent surgical infections related to bacteria which can damage the integrity of the implant. In this study, new titanium alloys were developed via powder metallurgy and the addition of manganese and copper, respectively, aiming to limit the manufacturing costs and induce new functionality on the materials including antibacterial response. The addition of manganese and copper to titanium significantly changes the behaviour of the Ti-Mn-Cu alloys leading to the successful stabilization of the beta titanium phase, great refinement of the typical lamellar structure, and achievement of materials with low level of porosity. Consequently, it is found that the mechanical performance and the antibacterial efficacy are enhanced by the addition of a higher amount of alloying elements. The manufactured Ti-Mn-Cu alloys fulfil the requirements for structural biomedical implants and have antibacterial response making them potential candidates for permanent medical implants.Item type:Publication, Biomedical Ti-Cu-Mn alloys with antibacterial capability2021, ElsevierThis study aims to develop Ti–Cu–Mn alloys with antibacterial capability for reducing the possibility of bacterial infection during biomedical implant surgeries. Ternary alloys were designed to be manufactured via powder metallurgy, which has intrinsic manufacturing, economic, and environmental benefits. The amount of each of the alloying elements was limited to prevent the formation of brittle phases. It is found that the selected compositions of Cu (0.5-5 wt.%) plus Mn (0.25-2.5 Mn wt.%) can successfully be manufactured achieving microstructures, tensile properties and antibacterial capability performance comparable to those of other biomedical Ti alloys. Specifically, homogeneous compositions are achieved with the selected sintering parameters (1300 °C/120 min). The strength and hardness of the material increase proportionally with the addition rate of Cu and Mn, and antibacterial capability values were found to be above the 90% threshold required for antibacterial certification.Item type:Publication, Thermomechanical processing of cost-affordable powder metallurgy Ti-5Fe alloys from the blended elemental approach: Microstructure, tensile deformation behavior, and failure2020, MDPIThe development of cost-affordable Ti alloys is key for the application of Ti in other industries like the automobile sector. Therefore, a combination of powder metallurgy (PM) and low-cost compositions is an interesting approach. In this article, a cost-affordable PM Ti-5Fe alloy is processed following the blended elemental route and extruded at high temperature to remove porosity. Different extrusion temperatures and heat treatments (i.e., solution treatment and aging, STA) are performed to obtain ultrafine microstructures, and their effect on the mechanical behavior is studied. For extrusions in the β phase, microstructures consist of coarse lamellar colonies, resulting in alloys with improved properties compared to the as-sintered alloy but still lacking toughness due to the failure happening just after necking onset. Extruding in the α + β phase results in a bimodal microstructure of fine elongated primary α and coarse lamellar colonies, and the alloy becomes tougher. STA with aging below the eutectoid temperature of 590 °C leads to a hard but brittle alloy, whereas STA with aging above it results in alloys with strength comparable to the as-extruded conditions and enhanced ductility.Item type:Publication, Effect of microwave sintering parameters on the physical and mechanical properties of pure Ti and blended elemental Ti alloys2018, Trans Tech PublicationsMicrowave sintering (MWS) was used to consolidate hydride de-hydride Ti powder and blended elemental Ti6Al4V, Ti5Fe and Ti5Al5Mo5V3Cr (Ti5553) powder mixtures. The amount of powders used to prepare the powder compacts was scaled up to 500g.The effect of the MWS conditions on the relative density, porosity distribution, microstructure and tensile properties were studied. Furthermore, uniformity in distribution of the alloying elements was checked. For most of the materials considered, a combinations of sintering temperature of 1200ºC and 1300ºC and holding time of 5 to 30 min resulted in significantly improved density. Nevertheless sintering temperature of at least 1300ºC was required for pore coalescence and high tensile properties.