University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, Manufacturing and characterization of sustainable hybrid composites using sisal and hemp fibres as reinforcement of poly (lactic acid) via injection moulding2019, Elsevier Science BVNatural polymers based composites offers significant advantages over synthetic fibre reinforced petroleum matrix based composites with regard to biodegradability, biocompatibility, design flexibility and sustainability. This work reports for the first time manufacturing of hybrid fibre reinforced biodegradable composites using sisal and hemp fibre with polylactic acid employing melt processing and injection moulding techniques. Granulated sisal and hemp fibres were blended and hybrid composites were manufactured using aliphatic polyester made up of lactic acid (PLA) through extrusion and injection moulding and their performance was evaluated. Experimental results revealed that density, elongation at break and water absorption capacity of hybrid composites were 1.14 ± 0.07 g/cm³, 0.93 ± 0.35% and 1.06 ± 0.18% respectively. The achieved mean tensile strength (46.25 ± 6.75 MPa), Young’s modulus (6.1 ± 0.58 GPa) and specific tensile strength (38.86 ± 5.0) of hybrid fibre reinforced PLA composites were improved compared to neat PLA. The flexural strength (94.83 ± 11.21 MPa), flexural modulus (6.04 ± 0.55 GPA) and specific flexural strength (79.76 ± 8.80) of hybrid fibre composites also showed better performance than those of neat PLA. Incorporation of sisal and hemp fibre with polylactide remarkably increased the impact strength of composites. Overall, the hybrid composites demonstrated good performance suggesting that they have great potential for use as an environmentally friendly alternative material in automotive, packaging, electronics, interiors and agricultural applications.Item type:Publication, Using synchrotron FTIR spectroscopy to determine secondary structure changes and distribution in thermoplastic protein2013, WileyBlood meal is a high protein, low value by-product of the meat processing industry that can be converted into a thermoplastic material by extrusion with a combination of a surfactant, urea, a reducing agent, water, and plasticiser. Changes in protein structure after each processing step (mixing with additives, extrusion, injection molding, and conditioning) were explored using synchrotron FTIR microspectroscopy. Blood meal particles were found to have higher β-sheet content around the perimeter with a randomly structured core. α-Helices were either located near the core or were evenly distributed throughout the particle. Structural rearrangement consistent with consolidation into a thermoplastic was seen after extrusion with processing additives, resulting in reduced α-helices and increased β-sheets. Including triethylene glycol as a plasticiser reduced α-helices and β-sheets in all processing steps. At all processing stages, regions with increased β-sheets could be identified suggesting blood meal-based thermoplastics should be considered as a semicrystalline polymer where clusters of crystalline regions are distributed throughout the disordered material.Item type:Publication, Preparation, microstructure and properties of Ti-6Al-4V rods by powder compact extrusion of powder mixture2012, Trans Tech PublicationsTi-6Al-4V (wt%) alloy rods were prepared successfully using a low-cost method that combines mixing elemental and master alloy powders and powder compact extrusion. The microstructure and mechanical properties of the rods and the effects of extrusion temperature on them were investigated. The results showed that the microstructure and mechanical properties of the extruded rods were strongly affected by the extrusion temperature. With increasing extrusion temperature from 1200°C to 1300°C and keeping the powder compact holding time unchanged at 2 minutes, the fraction of undissolved V rich particles in the microstructure of the extruded rod decreased substantially to zero, the level of composition homogenization increased dramatically to the highest level, and the UTS and elongation of the extruded rods increased significantly from 886MPa and 1.2% to 1300MPa and 7.1%, respectively. The tensile properties of the Ti-6Al-4V alloy rods produced by powder compact extrusion of the powder mixture are comparable to those of Ti-6Al-4V alloy produced by ingot metallurgy and thermomechanical processing.