University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
3 results
Search Results
Item type:Publication, High temperature deformation behavior of Ti–46Al–2Cr–4Nb–0.2Y alloy2012, ElsevierThe hot deformation characteristics of cast and hot isostatically pressed Ti-46Al-2Cr-4Nb-0.2Y (at%) alloy in the temperature range of 1100-1250°C and strain rate range of 0.01-1.0s -1 using hot compression tests were studied. The processing map of the alloy at true strain of 0.5 was also developed on the basis of the dynamic materials model (DMM). The experimental results show that the flow stress decreases significantly with increasing deformation temperature and decreasing strain rate. Using the kinetic rate equation the stress exponent n and the apparent activation energy of deformation Q were determined as 4.47 and 400.4kJmol -1, respectively. The efficiency values of power dissipation of the domain at strain rate below 0.4s -1 show that the dynamic recrystallization occurring of γ phase in the alloy is easier in the wide deformation temperature range (1100-1250°C) due to low stacking fault energy. The fraction of new recrystallized grains increased with increasing the hot deformation temperature at a given strain rate. With the increasing of strain rate, the uniformity of microstructure was decreased. The domain defined by the temperature range of 1200-1230°C and the strain rate range of 0.01-0.05s -1 which corresponds to a peak efficiency of about 60% is the optimal deformation condition of the alloy. Based on the optimal deformation conditions, a cylindrical sample was near isothermally forged. The microstructure and shape of pancake by forging was in good agreement with the prediction of processing map.Item type:Publication, Microstructure and mechanical properties of large size as-cast Ti-43Al-9V-0.2Y (at.%) alloy ingot from brim to centre2011, ElsevierA Ti-43Al-9V-0.2Y (at.%) alloy ingot with the size of Ф160×400mm was prepared by vacuum arc remelting (VAR). The microstructure of the as-cast Ti-43Al-9V-0.2Y alloy was composed of B2/α₂/γ lamellar colonies and massive B2 and γ phases which were distributed along the boundaries of these lamellar colonies in the form of equiaxed grains. Based on the grain size variation along the radius direction of the ingot, the ingot could be divided into four ring regions from brim to centre. It has been understood that the grain size variation between these four regions was due to the interplay of the effects of the cooling rate and the yttrium content on solidified microstructures in these regions. Mechanical testing of the samples cut from these four regions showed that there existed a clear correlation between the yield strength and the average grain sizes of the four ring regions, which approximately conformed to a Hall-Petch relationship.Item type:Publication, Interfacial microstructure and shear strength of Ti-6Al-4V/TiAl laminate composite sheet fabricated by hot packed rolling2011, ElsevierA two layer Ti-6Al-4V(wt%)/Ti-43Al-9V-Y(at%) laminate composite sheet with a uniform interfacial microstructure and no discernible defects at the interfaces has been prepared by hot-pack rolling, and its interfacial microstructure and shear strength were characterized. Characterization of the interfacial microstructure shows that there was an interfacial region of uniform thickness of about 250 μm which consisted of two layers: Layer I on the TiAl side which was 80 μm thick and Layer II on the Ti-6Al-4V side which was 170 μm thick. The microstructure of Layer I consisted of massive γ phases, needlelike γ phases and B2 phase matrix, while the microstructure of Layer II consisted of α₂ phase. The microstructure of the interfacial region is the result of the interdiffusion of Ti element from Ti-6Al-4V alloy layer into the TiAl alloy layer and Al element from the TiAl alloy layer into the Ti-6Al-4V alloy layer. The shear strength measurement demonstrated that the bonding strength between the TiAl alloy and Ti-6Al-4V alloy layers in the laminate composite sheet was very high. This means that the quality of the interfacial bonding between the two layers achieved by the multi-path rolling is high, and the interface between the layers is very effective in transferring loading, causing significantly improved toughness and plasticity of the TiAl/Ti-6Al-4V laminate composite sheet.