University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
9 results
Search Results
Item type:Publication, Impact Modification and Fracture Mechanisms of Core-Shell Particle Reinforced Thermoplastic Protein2016-08-01, WILEY-V C H VERLAG GMBHMechanical properties and fracture mechanisms of Novatein thermoplastic protein and blends with core–shell particles (CSPs) have been examined. Novatein is brittle with low impact strength and energy-to-break. Epoxy-modifi ed CSPs increase notched and unnotched impact strength, tensile strain-at-break, and energy-to-break, while tensile strength and modulus decrease as CSP content increases. Tg increases slightly with increasing CSP content attributed to physical crosslinking. Changes to mechanical properties are related to the critical matrix ligament thickness and rate of loading. Novatein control samples display brittle fracture characterized by large-scale crazing. At high CSP content a large plastic zone and a slow crack propagation zone in unnotched and tensile samples are observed suggesting increased energy absorption. Notched impact samples reach critical craze stresses easily regardless of CSP content reducing impact strength. It is concluded that the impact strength of thermoplastic protein can be modifi ed in a similar manner to traditional thermoplastics.Item type:Publication, Manipulating morphology in thermoplastic protein/polyester blends for improved impact strength2018-10-01, WILEYNovatein thermoplastic protein was blended with 10 wt% poly(butylene adipate- co- terephthalate) (PBAT) compatibilized with Joncryl ADR- 4368 and 2- methylimidazole (2MI). Morphology was tailored for favorable impact strength through changing vis-cosity ratio (λ) and interfacial tension (γ12). For uncompatibilized blends, λ decreased and γ12 increased with increasing Novatein water content, whereas compatibilizers caused a decrease in both λ and γ12. PBAT continuity was high when uncompatibi-lized, but dispersion improved with decreasing λ and increasing γ12. The dispersed domain size decreased in all compatibilized blends; PBAT continuity was lowest in samples with the smallest λ. Compatibilized blends had higher impact strength than Novatein and uncompatibilized blends through improved interfacial adhesion, smaller domain size, and increased dispersion. By altering λ and γ12, and with ap-propriate chemical interaction, a morphology can be created for improved impact strength. Increasing PBAT content showed further increases in impact strength; however, a cocontinuous morphology formed, demonstrating that composition can override the effect of λ and γ12.Item type:Publication, Effect of stearic acid treatment on the properties of aligned short hemp fibre mats and their potential use as reinforcement in polypropylene matrix composites2021, SpringerThe main objective of this study was to assess the effect of stearic acid vapour treatment on hemp fibre mats produced using dynamic sheet forming, and the potential use of these treated mats as reinforcement in polypropylene matrix composites. Stearic acid was successfully applied through vapour treatment, appearing to form a layer on fibre surfaces. It was found that the presence of stearic acid increased hydrophobicity and thermal stability of fibre mats. It was also found to increase thermal stability of polypropylene matrix composites as well as their strength.Item type:Publication, Chitosan: A review of sources and preparation methods2021, ElsevierThis review aims to explore different sources of chitin and methods of chitosan production with industrial consideration. This article first discussed different sources of chitin for industrial scale production, with considerations given to both their environmental impacts and commercialization potential. Secondly, this article reviews the two categories of chitosan preparation – chemical methods and biological methods - based on existing publications which used lobster by-products as a feedstock source. The mechanisms of the chemical methods are firstly summarized, and then the different chemical agents and reaction parameters used are discussed. Next, both enzymatic and fermentation-based approaches are reviewed under biological methods and compared with chemical methodologies, with lactic fermentation methods as the major focus. This article concludes that lobster cephalothorax could be an ideal source for chitosan preparation on an industrial scale; and chemical methods involve simpler processing overall, while produce chitosan with stronger bioactivities because of lower molecular weight (MW) and higher degree of deacetylation (DD) achieved by the products. Moreover, due to biological methods inevitably necessitating further chemical processing, an approach involving some unconventional chemical methods has been regarded as a more suitable strategy for industrial scale chitosan production.Item type:Publication, Alkali treatment of hemp fibres for the production of aligned hemp fibre mats for composite reinforcement2020, SpringerThe main objective of this study was to produce aligned hemp fibre mats from high strength hemp fibres using dynamic sheet forming (DSF). Alkali treatment of hemp fibre was carried out at ambient and high temperature to separate fibres. Single fibre tensile testing was used to assess the tensile properties of the fibres. It was found that the highest tensile properties were exhibited by high temperature treated fibre, whereas the tensile properties exhibited by ambient temperature treated fibre were lower than for untreated fibre. It was also found that fibre granulated after high temperature treatment, was better separated than that granulated before high temperature treatment. This well-separated fibre could successfully be formed into mats using DSF. The orientation of the formed mat was analysed using ImageJ (NIH, USA) software by which the potential of DSF to produce aligned hemp fibre mat was supported. The tensile properties of composite reinforced by these aligned hemp fibre mats were assessed.Item type:Publication, Effect of accelerated weathering on physico-mechanical properties of polylactide bio-composites2019, SpringerIn this work, injection moulded hemp fibre reinforced polylactide bio-composites of different fibre contents (0, 10, 20 and 30 wt%) were subjected to accelerated weathering of 12 h cyclic exposures of UV-light at 60 °C, water spray and condensation at 50 °C for 8, 16, 32, 48 and 64 cycles to study the changes in properties such as crystallinity, tensile, flexural, plane-strain fracture toughness (KIc) and strain energy release rate (GIc). The crystallinity of neat polylactide (PLA) was found to increase up to 50.6% after 64 cycles, whereas the crystallinity of composites of different fibre contents was found to increase in the range of 30.6 to 34.5% for 8 to 64 cycles. The overall mechanical properties (tensile, flexural, KIc and GIc) of the composites decreased as the number of cycles increased from 8 to 64. The crystallinity and the residual tensile strength, tensile modulus, tensile strain, KIc and GIc of the composites of 20 wt% fibres were found to be the highest after 64 cycles. In contrast, the residual flexural strength and flexural modulus of the composites of 30 wt% fibres were found to be the maximum after 64 cycles. Absorption of water, destruction of fibre integrity, degradation of PLA matrix, formation of cracks and pores were found to be the main causes of reduction in the mechanical properties of PLA bio-composites.Item type:Publication, Protein-Intercalated Bentonite as Nano-Reinforcement in Bloodmeal-Based Bioplastics2015, Prints PublicationsNovatein Thermoplastic Protein (NTP) is a biopolymer produced by modifying bloodmeal to a thermoplastic material, but requires reinforcement to improve mechanical properties. Proteinintercalated calcium (CaBt) and sodium bentonite (NaBt) were investigated as nano-scale reinforcements in NTP. These were prepared by recovering proteins from meat processing wastewater called stickwater, thereby reducing treatment cost and intercalating protein into clay layers in a single step. Using stickwater-modified NaBt improved the composite’s tensile strength by 23% (at 0.5 parts per hundred bloodmeal, pphBM) and Young’s modulus by 17% compared to standard NTP. Stickwater treatment greatly improved the compatibility of bentonite with NTP compared to gelatin-treated bentonite whose resulting composites only had similar or slightly improved mechanical properties. The improved mechanical properties are parallel with other improvements observed in thermal, crystallinity and filler distribution. Potential applications include plant pots and seedling trays for plant nursery and agricultural disposable tools such as weasand clips, nails and barbs.Item type:Publication, Foaming behavior of novatein and blends with polyethylene compatibilised by maleic anhydride2017, American Institute of Physics (AIP)Novatein® thermoplastic protein (NTP), a bloodmeal based thermoplastic, was successfully foamed without blowing agent or blending with other polymers using a BOY-35A injection moulder in free expansion mode. Previously, only soy protein has been successfully continuously foamed and zein and gluten batch foamed without blending or rheological modification. The greatest expansion ratio for NTP was 4.4 at 165°C. Blending NTP with compatibilised LLDPE and LDPE and adding blowing agent reduced expansion ratios. The foams exhibited a fibrous nature, with cell structures similar to those reported in literature for extrusion foamed thermoplastic soy protein isolate. SEM pictures suggested a possible role of either sodium sulphite, sodium dodecyl sulphate or sodium sulphate as a nucleating agent as particulates were found on the cell surfaces. Triethylene glycol and urea were thought to contribute to NTP foaming, along with water present in NTP, with two or more acting as the blowing agent.Item type:Publication, Dynamic Properties of Magnetorheological Elastomers Based on Iron Sand and Natural Rubber2015-02-20, Wiley-BlackwellIn this study, magnetorheological elastomers (MREs) based on iron sand and natural rubber were prepared. The Taguchi method was employed to investigate the effect of a number of factors, namely, the iron sand content, iron sand particle size, and applied magnetic field during curing on the loss tangent (tan δ) and energy dissipated during cyclic loading. Tan δ was measured through dynamic mechanical analysis over a range of frequency (0.01–130 Hz), strain amplitude (0.1–4.5%), and temperature (−100 to 50°C). The energy dissipated was measured with a universal tester under cyclic tensile loading. The data were then statistically analyzed to predict the optimal combination of factors, and finally, experiments were conducted for verification. It was found that the iron sand content had the greatest influence on tan δ when measured over a range of frequency, and the energy dissipated during hysteresis tests. However, none of the factors showed a significant influence on tan δ when measured over a range of strain amplitude. Furthermore, the iron sand content and magnetic field were also found to influence the width of the peak in tan δ as a function of the temperature. The morphological characteristics of the MREs were also examined with scanning electron microscopy.